ALLOY WHEEL // HOW TO WELD CRACKS// TIG welding ALUMINIUM
ฝัง
- เผยแพร่เมื่อ 5 ส.ค. 2021
- #BMW #CLASSICCAR #PANELBEATING #TIG #FABRICATION #WELDING #ALLOY #WHEEL #PLANISHING #RTECH #SNAPON #HOWTO #REPAIR
Join Tom Wilkes in this detailed guide on how to professionally repair a cracked alloy wheel.
(Music © Andrew Moors 2021) - ยานยนต์และพาหนะ
EXCELENTE VIDEO¡¡... Y MUY FACIL DE ENTENDER¡¡...SALUDOS DESDE MEXICO¡¡
A lot of the crap that came up would have been from what was trapped in the remnants of the crack. I always run a slitting disc down through the crack to try clear it out, and then do a pass just to burn any left over crud out before i start adding filler, that bit of extra prep makes life so much easier and neater. Other than that, fantastic vid bud 👍👍
What a clean Finish !!!!!!! 10/10
Thank you 👍
Brilliant vid. Thanks for this
Nice Job !
Nice work! Ric
Good explaining thank you 👍
Great video man
very good video smart wayof doingit mate
Brilliant
Good work bro
Thanks for the video.
Cheers Doug 👨🏭
Another good video instruction adding in the machine settings was a nice touch thanks
Thanks 👍👨🏭
The best repair iv ever seen
This guy takes pride in his work and definitely went above and beyond to make the rim appear that it was never repaired at all and it exactly appears that way. Thank you sir for taking time to show us your work
Thanks for the kind words 👍
But if you take the all weld off chances are it will break again very easily .
@@yasarramzan4796 Where in the hell did you see him 'taking off welds'?
I think he was referring to the Cap weld,in any case, he said with this process, he’s never had one returned so awesome job!!!
Good job there Crusty Tom!
😂 th-cam.com/video/ILjX9xQVQso/w-d-xo.html
Very nice work, fantastic repair.
Thank you 👨🏭
Ur the best
Nice looking repair 👍👏👏
Thanks mark 👨🏭
I've had some wheels done recently but they look nothing like that! Fantastic job!! 👌
Thank you Norman 👍
Thanks
Best finish I've seen , I prefer the drill and cut method but each to their own , looks super nice and I doubt it would affect the balance if at all
Thanks . I’ve done it that way too and had great results 👍
Hi Tom!
thanks for an amazing video! Very helpful and knowledgeable!
What did you use to put the groove in the wheel? With the wax? I couldn’t make out the name of the grinder, sorry this is my first rodeo.
Oh is it better to put a point on the tungsten or not? Thanks
Hi 👋 we use a tungsten carbide burr and a wax called trendi wax and that stops them clogging up. The grinder is a die grinder. Don’t put a sharp point on when welding Ali you only sharpen it for steel 👍 hope this helps
@@Metal_shaper_tom Thank you so much!
Nice job.
You should really wear a dust mask and use tig gloves though.
You only get one set of lungs.
great job looks like new...what would a repair like this cost ..?..
Hi probably in the region of £60/80
Hi Tom - I've just found your channel and I'm binge watching. What wax do you use to stop the tungsten burr clogging?
Hi Peter . We use trendiwax for this 👍
You would be better off using alcohol. Stops the clog and doesn’t leave a residue which can contaminate the weld
Nice work! Tell me, please, what is the name of this grinder? 5:27
@@Veganf00tS0ldier thnx!
Solid video but definitely consider using alcohol as a lubricant and de-clogger on your die grinder. We used to use wax and always had problems with impurities but now we are using alcohol we have found the problem drastically reduced
Thank you for the advice 👍
Great job,what area do you guys cover?
I’m in Cheltenham
What kind of welding stick u used to melt into the wheel?
5% silicone
what filler wire do you use
95%ali 5% silicone sure it’s called 1050
How is it holding? Did it leak any air after the weld?
Held really well. No issues with it
Wow,fantastic job.
Well done my man
Thank you 👍
Hi, can we use MIG to do the same work. Thx
I personally wouldn’t but that’s just me
I have the same problem on speedline wheel. I like the factory finish after repair !!! Its line never happened.
But is this repair strong enough or it will crack again to the same spot?
Hi 👋 I personally think this repair is strong enough to last. It hasn’t cracked again and it’s been at lest 6 months since I repaired it. Thanks 👨🏭
Can you build up for curb rash
Yeah I’d say so 👍
You in Texas? I need my rim fix asap
Yeah just down the road . Drop it off I’ll have it done in a hour.
with how many amps do you weld that rim
I think it was around 130 🤔