Do you really need to dry your filament?

แชร์
ฝัง
  • เผยแพร่เมื่อ 18 พ.ย. 2021
  • Can you leave your PLA spools out in the open and do you really need to dry PETG before every use?
    Thanks to OpenBuilds for sponsoring this video! Get your parts at openbuildspartstore.com/
    Products shown:
    Prusa MK3 go.toms3d.org/MK3Ass
    Prusament go.toms3d.org/Prusament
    Eibos filament dryer:
    on Amazon go.toms3d.org/EiDry
    on Aliexpress go.toms3d.org/EiDryAli
    Read the article to this video here: toms3d.org/2021/11/23/how-bad...
    Product links are affiliate links - I may earn a commission on qualifying purchases (at no extra cost to you)
    🎥 All my video gear toms3d.org/my-gear
    I use Epidemic Sound, sign up for a 30-day free trial here share.epidemicsound.com/MadeWi...
    🎧 Check out the Meltzone Podcast (with CNC Kitchen)! / @themeltzone
    👐 Enjoying the videos? Support my work on Patreon! / toms3dp
  • วิทยาศาสตร์และเทคโนโลยี

ความคิดเห็น • 599

  • @nipunagunarathne4882
    @nipunagunarathne4882 2 ปีที่แล้ว +105

    I can see his teleprompter reflected on the PSU lol. Was wondering for way too long wtf that movement was

    • @linkpuppyandzeldakitty
      @linkpuppyandzeldakitty 3 หลายเดือนก่อน +5

      You helped me see one of the secrets to making content Xd

  • @Milazzone
    @Milazzone 2 ปีที่แล้ว +614

    I would be curious to see the same test, but this time add in "after drying" categories via dry box or oven/dehydrator. Just to see how well it actually removes the moisture vs just keeping the filament bagged away in the first place.

    • @Akegata42
      @Akegata42 2 ปีที่แล้ว +38

      I was going to write this as well. Except I'd be more interested in the actual printing quality after drying rather than just how much moisture is removed. That is, I'd be interested in seeing if removing the moisture makes the filament print as well as if it was never wet in the first place.

    • @crazytexasgypsy
      @crazytexasgypsy 2 ปีที่แล้ว +20

      Just from my personal experience printing in high humidity environment, If you dry at most commonly recommended temps and times it brings it right back to just as good as new.

    • @wturber
      @wturber 2 ปีที่แล้ว +6

      Some PETG I buy reliably comes with substantial moisture in the filament even though the filament is vacuum packed with a silica gel pack. Some day I might just weigh a reel before and after drying. Anyway, depending on brand, "fresh out of the bag" may or may not be particularly dry. I always store my PETG, ASA, and ABS with substantial amounts of silica gel after I dry them. I printed little mesh-like cannisters that fit into the reel's center holes. FWIW, I live in a generally low humidity area (Phx, AZ metro).

    • @pizzablender
      @pizzablender 2 ปีที่แล้ว +1

      I dry my filament (PETG) by storing it with silica gel in a metal container. Takes a while to dry, but keeps it dry pretty well.

    • @truantray
      @truantray 2 ปีที่แล้ว

      No one ever mentions this, but filaments have volatile plasticizers. If you dry too hot, the plastic becomes brittle. I don't need to dry often, but I do it at no more than 30C.
      It's a bad habit to leave the spool on the printer between prints.

  • @WilliamWallace14051
    @WilliamWallace14051 2 ปีที่แล้ว +233

    More than one of the old time welders I knew had an old refrigerator with the compressor disabled and a 100 watt incandescent light bulb on in it to store the "sticks" in. The working refrigerator had the beer.

    • @advancedinventions1822
      @advancedinventions1822 2 ปีที่แล้ว +31

      Yes that’s because some welding electrodes can’t let the Coating get moisture in it or it can’t properly shield the weld and the quality and strength of the weld will be ruined.

    • @jeanmanuel6182
      @jeanmanuel6182 2 ปีที่แล้ว +9

      Those old tradesmen have some cool tricks up their sleeves

    • @cosmicraysshotsintothelight
      @cosmicraysshotsintothelight 2 ปีที่แล้ว +20

      You spelled "lunch beverage" wrong.

    • @jonahek2651
      @jonahek2651 2 ปีที่แล้ว +20

      @@cosmicraysshotsintothelight you spelled breakfast beverage wrong

    • @codyhoche8888
      @codyhoche8888 ปีที่แล้ว +1

      Lo hydrogen raids a filler metal meet to be stored at temp to prevent build up of hydrogen in the flux coating for example 7018 family of welding electrode

  • @edumaker-alexgibson
    @edumaker-alexgibson 2 ปีที่แล้ว +47

    Steam bubbles breaking the polymer chains - first time I've heard that explanation and it makes a lot of sense, thanks!
    Recently noted on a challenging ABS print (major buildup of internal stress) that I was getting delamination despite excellent print quality and printing very slowly at 260C.
    Just switching to a newly bought reel of ABS and no delamination at all!

  • @bkpickell
    @bkpickell ปีที่แล้ว +10

    A couple years ago I had a hotend collision with my bed and damaged my build surface. Long story short, it took me two years to get around to fixing it. So I have a two year old roll of pla that is still on the printer. I started printing parts again yesterday and the prints are flawless.

  • @BenjaminVaterlaus
    @BenjaminVaterlaus 2 ปีที่แล้ว +8

    After drying I only see a difference in layer adhesion and in stringing. I am glad that you did this, and it confirms that my process of keeping filaments in their bags with desiccant is likely enough for the casual prints.

  • @tomsmith3045
    @tomsmith3045 2 ปีที่แล้ว +4

    Loved that you put this up and included all of the background data. I read it as both the weight gain and potential strength loss are within the noise margins of your tests, and that's OK. That there are clear functional and appearance differences in printing, even with PLA, was great to learn. I live in the northeastern US, where it's very humid in the spring and fall, when the temperatures are mild. So we may see an indoor relative humidity of 45% or more. I've wondered if I'm being overly cautious in keeping all of my PLA in bags with desiccant, and it turns out I haven't! Thanks for this.

  • @carpenecopinum1665
    @carpenecopinum1665 2 ปีที่แล้ว +131

    Recently, I have gained the impression that manufacturer-specific additives to the filament matter much more than the actual base polymer (or to a similar degree).
    I have printed a bunch of PLA, ABS, HIPS and PETG. PETG appears to pick up moisture pretty quickly from every manufacturer, on the other side of the spectrum, none of the HIPS-filaments I tried appear to care much about it.
    But with both PLA and ABS, I have spools that have been out in my printer room for months and they still print like on the first day, but also spools that will start bubbling significantly just after a few weeks without drying.

    • @elvinhaak
      @elvinhaak 2 ปีที่แล้ว +12

      Yes, same results here. Some filaments (colors, brands) have much more problems with 'beeing wet' then others so it is even harder to compare.
      And then: I have had many filaments (of cheaper venders) that already came in wet in the new boxes: printing not soooo well, drying straight out of the new box made them a bit lighter (PETG a couple of % sometimes) after a couple of days in the food-dryer and printed much much better. But other venders: well, no problem printing fresh, no differences with a couple of days in the dryer and no visible printing-differences after weeks in the open.
      And moisture inside this year: mostly between 80 and 90 degrees in room, inside printcases between 60 and 75%. Other years it was much dryer so less problems.

    • @victortitov1740
      @victortitov1740 2 ปีที่แล้ว +4

      i agree, for example i had two rolls of abs, one white and one black, from the same manufacturer. The white one was very sensitive to moisture, the black one - not at all.

    • @MrKhay82
      @MrKhay82 2 ปีที่แล้ว +6

      @@victortitov1740 to get filament white, you need to add much more color pigments, than to get it black. so i would assume, the pigment is the sensitive part there.

    • @beauregardslim1914
      @beauregardslim1914 2 ปีที่แล้ว +1

      I've seen the same thing. I have some amazing "PETG Plus" which prints as easily as PLA and doesn't seem to need drying. But it smells so odd when I print with it that I wonder about breathing whatever they added.

    • @Aberusugi
      @Aberusugi 2 ปีที่แล้ว +2

      Pla and abs aren't very hygroscopic at all. Now try the same thing with nylon. It will be a nightmare to print with if you don't dry it.

  • @davidboston7943
    @davidboston7943 2 ปีที่แล้ว +71

    Hey Thomas, thanks for covering this. It's really great to see folks like you and Stefan over at CNC Kitchen trying to approach these questions in at least a relatively scientific way (including recognizing when your results just don't show enough significance to draw a conclusion). This is an area that's of great interest to my university lab, since we do a lot of prototyping with 3D printers. One subject that we've begun to explore, and there really doesn't seem to be a lot of readily available information on, is the effect on mechanical properties of moisture absorption post-printing. We did a brief (unpublished) study of a carbon-reinforced nylon where we printed a group of samples at once and tested groups of them at varying time intervals. It showed that the elastic modulus dropped by almost half within a week of printing. We haven't repeated the study for any other common materials, but it's certainly a result that warrants some further investigation if you're looking for subjects for future videos. Again, it's not an area that we're *particularly* interested in publishing results, since we focus on the structures we make with 3D printing, rather than the process itself, but there may be some potential for collaboration or sharing results if you're ever interested.

    • @tralfazy
      @tralfazy ปีที่แล้ว +1

      That somewhat confirms for me that my belief is correct that my PETg parts are degrading once printed. A handle or lifting arm might be just fine for several months, then suddenly one day it snaps or cracks without any changes in the external forces that are putting pressure on it.

    • @davidboston7943
      @davidboston7943 ปีที่แล้ว +8

      @@tralfazy Not to suggest that you're incorrect, because PETg certainly has a reputation for moisture absorption and is another material I want to look at when I have time (or a helpful undergrad I can enlist to do some work for me, haha); however, I suspect the situation you're describing has more to do with cyclical fatigue (possibly compounded with degradation). The time scale we've seen as we've conducted our tests is generally on the order of a week or less, with the most significant effect within the first 48 hours. The sudden failure of a part that previously appeared fine to me signals some kind of embrittlement (possibly from something like UV exposure?) or, again, repeated loading causing small defects to propagate and eventually compromise the part. Hard to say for sure without a more thorough investigation, but I do think this is something we need to be more aware of in the community 👍

  • @thebob94547
    @thebob94547 ปีที่แล้ว

    Hi Thomas, I always appreciate the way you are looking at those things - that level of detail is really mind blowing. Thanks for your work!!!

  • @FilamentStories
    @FilamentStories 2 ปีที่แล้ว +57

    Love this video. The panic that seems to surround "wet filament" is pretty extreme. I get regular comments about my filament being opened. I even get comments that I shouldn't open the bags, which makes it rather hard to print with the filament.

    • @reeces.pieces3
      @reeces.pieces3 2 ปีที่แล้ว +4

      how are you supposed to print the filament while it's still in the bag??

    • @pr0xZen
      @pr0xZen 2 ปีที่แล้ว +10

      @@reeces.pieces3 Easy. Just gotta stick with abstract art, 750g or 1kg prints with 100% infill. Use oven or high wattage bed heater for... "printing".
      The embedded spool is a feature, not a bug.

    • @TrueThanny
      @TrueThanny 2 ปีที่แล้ว +2

      I'm going to guess that the comments about not opening the bags were comedic hyperbole.

    • @frankb5728
      @frankb5728 2 ปีที่แล้ว +1

      I don't think it's extreme.. even PLA has issues and there are people who still don't believe so. I guess everyone's standards of quality are different.. I want perfect prints, that's what I aim for and I have definitely noticed difference

    • @frankb5728
      @frankb5728 2 ปีที่แล้ว +2

      ​@@yeoj_ Yes that is absolutely the reason, People rarely take that into account. I'm up north and we have very low RH in the winter and high in the summer, I've had to deal with 80+% humidity and I had print breaking issues even with PLA. I definitely needed a dry box

  • @e.a.steutel7874
    @e.a.steutel7874 ปีที่แล้ว

    Thank you for all the time you took showing this test. I’ve been having major problems printing petg after it being my favourite filament for months. It went from perfect prints to not usable in a few months. Even drying it for 20 hours does not give the same strong layer bonds anymore.

  • @extectic
    @extectic 2 ปีที่แล้ว +2

    Great effort, thanks. I do print a lot of PETG, so I think I'll start running it through my dehydrator if I'm planning on any major printing sessions.

  • @WhereNerdyisCool
    @WhereNerdyisCool 2 ปีที่แล้ว +57

    I'm glad you are covering this. I had a spool of Ultimaker PLA filament out in the open for 8 years. I decided to print with it and wow, stringy! I invested in a Print Dry Pro filament dryer and after 6 hours of drying, it printed very well! At work (home of the world's largest 3D printer), we dry the pellets for several hours before use, then they are loaded into the printer. That got me thinking about the weird print issues I would see on my home printers. I now dry all my filaments before use, no matter how amazing the vacuum packing looked. The results are way better! Also, active drying is the way to go. Sitting in a tub of desiccant wont do a thing, you need to actively heat it up to get the moisture out.

    • @Japie196401
      @Japie196401 2 ปีที่แล้ว +3

      Hi WNIC. Thx for your addition. Can you elaborate somewhat on "how long" and "how hot" your drying process is? Do you measure humidity? Or just time and temp.
      Thx for the effort.
      Regards Wouter

    • @jofagoma
      @jofagoma 2 ปีที่แล้ว +1

      @@Japie196401 I'd also really love to know more about this

    • @natalieisagirlnow
      @natalieisagirlnow 2 ปีที่แล้ว

      probably more to do with age than dryness

    • @someguy2741
      @someguy2741 2 ปีที่แล้ว +5

      @@Japie196401 I just experimented with dessicang pellets like this. Relative humidity here is 29%. The filament picked up all of that in a few days.
      I dried the dessicant for 2 hours at 210F/100C in a toaster oven. Then put the dessicant in a filament bag. The dessicant alone in the bag saw 19%. This might be the practical limit of the little white bags of random dessicant.
      When I put the now two day old filament in a bag it said 29%. When I added the dessicant it was pulled down to 19% in two days.
      It certainly seems that even in a couple days the filament is at ambient humidity. As for drying I bought a cheap toaster oven. The only caution is to preheat the oven first since as it is trying to reach temp it runs hot and will melt spools.

    • @pr0xZen
      @pr0xZen 2 ปีที่แล้ว +4

      Quite a lot of moisture can permeate a vacuum bag before it starts to show. A couple of small bags of silica gel can only do so much. They can't actually hold that much moisture, and silica gel don't really absorb much of anything below 35-40% humidity. If you have a sealed drybox and you need to bring it lower than that, you need to A) get rid of any cardboard packaging inside the box, and B) use Calcium Chloride based dessicants. You *must* have those dessicants in a container or bowl though - they get goopy and liquid'y as heck when they start to near their saturation point. They don't really "just absorb" moisture, they convert it to an unsaturated saline liquid (it won't vaporize again from there easily, but can make a mess if spilled). Keep that in mind when moving the drybox around, so you don't spill that mess around inside.
      As a peace offering for this goopyness, calcium chloride dessicant can absorb and convert 7 times its own weight in moisture, while silica gel start struggling at 30% its own weight.

  • @amarissimus29
    @amarissimus29 2 ปีที่แล้ว +18

    I remember when I got my first spool of nylon. Instantly turned my hot end into a steam engine, and that was right out of the vac-pack. Such a pain, but worth the work if you need awesome parts.

    • @gwapo9846
      @gwapo9846 ปีที่แล้ว

      English bro

    • @DatHondaBoi223
      @DatHondaBoi223 17 วันที่ผ่านมา

      @@gwapo9846wtf do you mean English, I understood his comment just fine

  • @3DMusketeers
    @3DMusketeers 2 ปีที่แล้ว +5

    Great video Tom! Love your dedication to the research and testing!
    Octolapse can be picky with print settings. We find when we do time lapses we have to cut temps by around 10C or more to keep that oozing down.
    Interesting about the smell of the ASA, I wonder if my old ASA and ABS will smell worse than new!
    Great video as always Tom! Love the detail here!

  • @war4peace1979
    @war4peace1979 2 ปีที่แล้ว

    This is the first video in MANY years which has a sponsor I did NOT skip.
    Thank you!

  • @HuntersOA
    @HuntersOA 2 ปีที่แล้ว

    I also have an eibos dryer and I love the heck out of it. 2 years ago I bought a prusament PETG and was never able to print it properly. After drying it it magically started working completely fine. Ever since I have it I print directly out of it and dry my filaments during printing.

  • @taantricks
    @taantricks 2 ปีที่แล้ว

    that opening shot.. just another level.. awesome.

  • @soggynode
    @soggynode 2 ปีที่แล้ว +16

    Good info as always. I'm also curious why the 300mm or so of PLA left inside a Bowden tube seems more brittle than the material coming off the spool.

  • @LT72884
    @LT72884 2 ปีที่แล้ว +3

    Glad to see this. Im actually a medical and aerospace engineer doing a full punlished study on the food safety qnd sanitation of 3d printing. I get to use a SEM scope often and some of the most dangerous bacteria. Ill be posting some youtube videos soon, discussing my findings since its for an internship.

  • @VincentVeak
    @VincentVeak 2 ปีที่แล้ว +3

    This was a perfect collab opportunity with CNC Kitchen!

  • @realcrys
    @realcrys 2 ปีที่แล้ว +3

    Interesting results! Inconclusive is better than I expected. I have an old roll of PETG I'm trying to use up, I'm really struggling with layer adhesion and warping compared to the same material from a fresh roll, even after drying it for almost a day

  • @Abrikosmanden
    @Abrikosmanden 2 ปีที่แล้ว

    What a great test setup! Well done!
    That shirt looks SO comfy, btw.

  • @janikhen7736
    @janikhen7736 2 ปีที่แล้ว +49

    as you mentioned drying, I‘d be interested in seeing how effective putting the filament on the hot buildplate and covering it is with that

    • @jofagoma
      @jofagoma 2 ปีที่แล้ว +2

      That's a nice idea. We could even develop a cover that seals sufficiently and with a temp and humidity sensor. Like that you'd avoid to spend more and it allows to keep things small. Thanks for the suggestion BTW

    • @RubixB0y
      @RubixB0y 2 ปีที่แล้ว +9

      Interesting idea, probably not worth pursuing it based on fundamental issues and the easy alternative of a food dehydrator.
      You mention a cover, I assume to keep the heat in, the problem is that also traps the moisture in. The airflow necessary to remove the moisture would take the heat away at a rate the surface area and wattage of the hot plate would struggle with. Consider, the bed heater is radiating from the bottom as well unless it's insulated.

    • @TechieSewing
      @TechieSewing 2 ปีที่แล้ว +3

      There is a video where a person dries Nylon this way, just covers it with a cardboard box. Said it was pretty effective.

    • @wturber
      @wturber 2 ปีที่แล้ว +2

      There are some TH-cam videos that show how to print a fixture for just that purpose. My problem with that is that it ties up your printer for hours. But that doesn't mean it isn't a nice option to have available.

    • @jofagoma
      @jofagoma 2 ปีที่แล้ว

      @@RubixB0y thanks for the information. Perhaps I should just search for a nice dehydrator.

  • @jordananderson1594
    @jordananderson1594 2 ปีที่แล้ว +2

    Great video, thanks as always for the informative and interesting content. I did want to say, though, to not fall in the trap that many scientists do that a lack of difference is a lack of results. Failing to reject a null hypothesis doesn't mean an experiment failed, it just means you didn't see what you expected. That is still extremely valuable information and it should be published! Thanks for publishing your unexpected results, they provided some really informative data.

  • @mokdumoknonsharrall1868
    @mokdumoknonsharrall1868 2 ปีที่แล้ว

    @Thomas Sanladerer: Thanks for doing this research. Hope to see more in the future. Glad you're acknowledging your biases and experimental flaws, that's important in science!

  • @jtrmal
    @jtrmal 2 ปีที่แล้ว +6

    One more thing to consider is that the mechanical properties of the printed thingy can actually improve after absorbing the moisture. For example nylon to have the expected "nylon" properties, it needs to be allowed to absorb at least some moisture. So the moisture might not be good for the print, but is part of the operating properties.

  • @MisterMakerNL
    @MisterMakerNL 2 ปีที่แล้ว +1

    Before I started I already said to myself, I don't care what he is going to say I have absolutely no issues with how I do it now. Just open in the air nothing special. Glad you had the same conclusion.

  • @olafschermann1592
    @olafschermann1592 2 ปีที่แล้ว +1

    Great content. Thank you for putting in that high effort to give us this helpful conclusion.

  • @hobo66
    @hobo66 ปีที่แล้ว

    Thanks for including ASA! It's my favorite filament and what I use the most, and it's rare to see it included

  • @jl8096
    @jl8096 11 หลายเดือนก่อน

    Thanks for great video! I was always wondering how humidity of filament affects the print quality and now I got the point.

  • @CDRaff
    @CDRaff 2 ปีที่แล้ว +2

    One thing that this video taught me is that the community as a whole is saying "You filament is wet" far too often. Apparently your filament can be very wet and still print fairly normally.

    • @someguy2741
      @someguy2741 2 ปีที่แล้ว +1

      What he didnt show is the other symptoms and things that are exaggerated by wet filament. First layer adhesion is greatly effect. Brittleness of fliament (i had PLA that broke into 1cm regular segments in a bowden tube and it wasnt even tight radius). Stringing and other things are a nuisance too. No amount of tuning could remove these issue but drying the filament makes a big difference. Of course he is using a fancy machine with a fancy buildplate. If you print on other media like glass you will notice these more.
      If you have trouble with first layer and the machine settings are good (height, temp, speed) try drying the filament. It makes the window of all other tuning much bigger. Surface finish is also better and part accuracy too.
      If you are consuming a 30 dollar roll of plastic it makes sense to make the best product you can. Of course that depends on your goals.

    • @CDRaff
      @CDRaff 2 ปีที่แล้ว

      @@someguy2741 I never said that it wasn't a problem at all for filament to be wet. What I did say is that "Your filament is wet, dry it out." is and has been an easy way for the community to brush off problems beginners are having because we don't want to take the time to actually figure out what the actual issue is.

  • @antilogism
    @antilogism 7 หลายเดือนก่อน

    I've had bubble issues in clear TPU that made it translucent. I didn't know that it was that sensitive. Printing dry looked great.

  • @hugoandre96
    @hugoandre96 2 ปีที่แล้ว

    from my experience with pla, I have left the same spool of filament in my garage unprotected from the elements in the florida humid weather for 5 months. Used it without any changes to the spool and it printed the same as a new roll

  • @WildChinoise
    @WildChinoise 2 ปีที่แล้ว

    Super informative. Thanks for performing the testing!

  • @TJCampie
    @TJCampie 2 ปีที่แล้ว +2

    man I freaking love your sweat shirts.

  • @GruesomeJeans
    @GruesomeJeans ปีที่แล้ว +3

    Pretty interesting stuff, I'm new to printing and have only had my printer for about 2 weeks or so. I've gone through almost 1kg of PLA so far that has just been sitting on the machines spool holder. I don't think the humidity is very high and the only issues I've had with print quality seem to be from my inexperience. I've been having a lot of fun printing random things and little tools, I've also been enjoying the process of learning new things!

  • @bruceyoung1343
    @bruceyoung1343 2 ปีที่แล้ว +1

    Thank you. I was blaming my failed prints on “moist” filament. That is until I made a filament dry box. Inside the dryBox down to 17% humidity and my prints weren’t any much better. I found my problem was due to heat creep up the heat break and messing up the end of the Bowden tube. So I ordered new style Capricorn YS (I think) Bowden tube to try. And steel nozzles

  • @beauregardslim1914
    @beauregardslim1914 2 ปีที่แล้ว +1

    Excellent to see some testing. Never assume factory "fresh" PETG isn't wet. I've had filament that came sealed with dessicant from a number of vendors that needed many hours of drying to stop seeing bubbles in the nozzle stream. Transparent and semitransparent seems to be worse than solid colours for some reason.

  • @Rcschim
    @Rcschim ปีที่แล้ว

    Great vid! and nice presentation. I like your humble approach and you "not totally scientific" tests. I do similar tests with drones and antenna reception ;)
    I'm new to 3D printing and love how much this has improved over the years - so it's very easy to start now!

  • @audi80flo
    @audi80flo ปีที่แล้ว +1

    More testing to be done. I've done quite some moisture related tests at my workplace while using professional hardware. The variations in moist levels can be quite significant and can be checked with a good scale.
    I've recently had an old spool of tpu dried (~500g) and checked pre and after: more than 15g of water!
    Some materials don't "moist" very fast, we usually saturate test samples in heated water in climate chambers. Cold water does take too long 😄
    Outside test: you can freeze-dry clothes, so maybe its even better stored outside?

  • @JT-Works
    @JT-Works 2 ปีที่แล้ว +1

    As someone that prints in a garage in Florida, I appreciate this video...

  • @artiem5262
    @artiem5262 2 ปีที่แล้ว

    thank you for a fascinating study!

  • @herrtrojanischespferd1063
    @herrtrojanischespferd1063 ปีที่แล้ว

    Thanks Thomas! Very informative.

  • @mysteriouspikachuman
    @mysteriouspikachuman 2 ปีที่แล้ว +1

    That intro sequence is so awkward yet brilliant

  • @yatyas72
    @yatyas72 2 ปีที่แล้ว +1

    Download the datasheet for each plastic. It will give you optimal temperature for molding as well as what temperature and for how long you need to dry them. I've been doing injection molding for 20 years and we dry all plastic before use it there are a ton of problems/defects that can result.

  • @thesledgehammerblog
    @thesledgehammerblog 2 ปีที่แล้ว +10

    In my case, the biggest issue I seem to have with filament that's been left sitting out isn't necessarily print quality (although I have some stuff that's got a lot of stringing) but brittleness. Hard to get a good print when the filament keeps breaking before it reaches the extruder.

    • @truantray
      @truantray 2 ปีที่แล้ว

      Filament has volatile plasticizers that go away with age and increase brittleness.

    • @Kalvinjj
      @Kalvinjj 2 ปีที่แล้ว +1

      @@truantray Interesting, this adds to the reasons why my older PLA roll is such a horrible nightmare to use. The thing breaks inside the extruder even, it can't unroll from the spool, heck last time I used it I just cut the appropriate length and let it as a little roll dangling on the extruder.

  • @scharkalvin
    @scharkalvin 2 ปีที่แล้ว +7

    Storing filament outdoors also exposes it to UV light, which could have its own bad effects.
    I usually store my filament in a closed zip lock bag with a packet of moisture absorber that usually comes with the filament. I haven't done a very good examination, but stored this way filament that has been opened seems as good as brand new. But then again the stuff I print isn't critical.

  • @martyb3783
    @martyb3783 หลายเดือนก่อน

    Very informative. Thanks for making this video!

  • @choschiba
    @choschiba 2 ปีที่แล้ว

    Thank you very much for the interesting video! My printer room is fairly dry, but to be on the safe side I will dry the spools lying around tomorrow and store them away properly.

  • @richmagda553
    @richmagda553 2 ปีที่แล้ว

    Like the thumbnail picture. A play on Dali's Atomica photograph. Excellent!

  • @rcmaniac25
    @rcmaniac25 2 ปีที่แล้ว +7

    My practice has been:
    - open bag
    - remove tiny desiccant
    - dry filament
    - put back in a sealed bag with larger (colored indicator) desiccant
    - move on with life
    I usually go for visual quality, so I know from printing out color swatches (that have a lot of retractions), dry filament is leagues better then straight out of bag (let alone wet) filament. But once that's done, I'm content.
    An interesting one for me was I was told by one filament manufacturer that there is a limit to how much you can dry filament before it starts to degrade and they recommended no more then 3-4 drying sessions (couple hours each time) for the entire spools lifespan. They use Natureworks PLA (don't remember the exact number).

  • @roysigurdkarlsbakk3842
    @roysigurdkarlsbakk3842 2 ปีที่แล้ว

    Thanks for this one. I'm looking forward to you testing the new Prusa XL ;)

  • @Golgafrincham
    @Golgafrincham 2 ปีที่แล้ว

    I'm living in a badly ventilated apartment. Currently we don't have any tumble-dryer (or any other enclosed area for drying) and during the winter we have to dry clothes after washing in-doors. To that, add heat and humidity from cooking etc. It is not uncommon for us to have a relative humidity sometimes in the upper 50%. As I was a beginner with 3D-printing I didn't think/know about the problem with water absorption, but I can tell you that keeping my Prusament PETG lying on a shelf without any bag or humidity protection made it unprintable.
    Details less than 5mm broke off very easy (sometimes couldn't even remove supports without breaking it), the surface was extremely rough, a lot of stringing. It was also clear that any kind of retraction gave a lot of artifacts and weak areas. Printing continuous parts ended up semi-ok.
    I bought a drybox, dried the PETG over night and every print come out beautifully now when storing it properly. Barely any stringing, smooth surface and parts are generally much stronger.
    I think if you really want to see wet filament, store it in upper 20s with 50% RH for a month. This is not that uncommon climate in badly ventilated apartments during the winter when there is limited possibilities for opening windows etc.

  • @jong2359
    @jong2359 2 ปีที่แล้ว

    I just pulled out some filament that had been stored out in the open in a storage unit for 1 year, in an unused backroom of my first house for 3 years, and then in my basement of my second house for another 3 years. It printed fine.

  • @darkdrewmo
    @darkdrewmo ปีที่แล้ว

    Hmm glad you did this test. I'm half way through an ASA spool in the winter and it has started to pop and bubble coming out of the nozzle and I assumed it was saturated with moisture. I can't even get the first layer to adhere at this point since the plastic barely bubbles out the nozzle. Probably time to order another spool unless I can use a dehumidifier or something to recover it.

  • @Damien_Clarke
    @Damien_Clarke 2 ปีที่แล้ว +2

    As usual, AWESOME Video! Your testing controls were well thought out, based upon your available tools and measurement limitations. There is one aspect that I don't think I hear you mention, did you have your dehumidifier running during testing? If so, would there not be a tendency that at all the samples would try to 'normalize' to the environment; i.e. get drier? That is, the longer that remained in the room environment, the samples would all eventually establish the same humidy level - time being the variable factor? Your thoughts?

  • @user-mz6qu3hz6m
    @user-mz6qu3hz6m 2 ปีที่แล้ว

    The main thing I noticed was that certain PLAs would just jam in my Prusa Mini when they used to print fine. An overnight stay in the dehydrator will make unprintable silk PLA print just fine. As some others have noted, it really seems to vary depending on the source and color. And I live in a semi-arid climate where indoor humidity is typically 20-40%.

  • @JamieHarveyJr
    @JamieHarveyJr 2 ปีที่แล้ว

    Waiting for your Eibos Cyclopes test. ‘My Tech Fun’ did an excellent dryer test that convinced me to buy one myself. Very happy with it too.

    • @danielkrah5129
      @danielkrah5129 2 ปีที่แล้ว

      I am using it since January now. Works relatively great. For EU customers it is bad that they only ship with US cables and then add adapters. (ok i got 1 of the better adapters but still meh ...) 1 feet is shorter so it wiggles (used a washer -> fixed) the weld of the lid on the backside is not that strong. (Used a little bit of superglue so fixed) When using without ptfe tubes the outlet in the front could be placed a little lower. But in general it works great. But i have to mention that i have an earliest bird unit so maybe some things are better in the current production and i only paid 52€ shipped for it. So i can't really complain for that price.

  • @therealharleybutler
    @therealharleybutler ปีที่แล้ว +1

    with a 0.6 nozzle or bigger having dry filament is essential if you don't want the most obscene amount of stringing known to man. I had some PETG and I couldn't even make any functional parts with it with my 0.6 nozzle because it would ooze too much. And then when I dried it out it worked absolutely perfectly. I was even able to lower my retraction quite a bit.

  • @JohnAldred
    @JohnAldred 2 ปีที่แล้ว +1

    I'd like to see these same tests with longer term exposure to the elements. I've got rolls here that have been open for months because they're a colour/material combo I don't print with often, can't get anymore so don't want to waste. And I definitely notice the difference in rolls that have been out for a few months. I've even seen it come straight from the manufacturer that way, too - either because they have a crappy packaging process and left the spools out in the warehouse for weeks before they bagged and shipped them out or the bag got burst on the way over. It's just my normal practice now to assume all spools are moist and throw them in the food dehydrator overnight the day before I want to print with it.

  • @alexhenry7942
    @alexhenry7942 2 ปีที่แล้ว

    Thanks for putting this together. Great video.
    Ive always been a little curious if letting a filament get wet, then drying, is any worse than just using it dry out of the box.

  • @JesusFreke
    @JesusFreke 2 ปีที่แล้ว +1

    A couple of things I've noticed: If you use a very large nozzle (e.g. 1.2mm) to just extrude some non-opaque PETG into air, it's incredibly easy to see steam bubbles in the extruded filament, unless the filament is nearly perfectly dry. And also, some/most PETG I've tried (although I haven't tried prusament) isn't dry enough to not show any bubbles even when taken out of a new, sealed bag and immediately used. I have to dry even new filament first, to get a no-bubble extrusion.

  • @memejeff
    @memejeff 2 ปีที่แล้ว

    Great video! I thought that it wasn't that important after some filament I have had out for 4 years works pretty well. To be fair, the humidity here is often 40-55% rel.

  • @ThantiK
    @ThantiK 2 ปีที่แล้ว

    THANK YOU FOR THIS VIDEO!

  • @johnkarobonik2017
    @johnkarobonik2017 2 ปีที่แล้ว +1

    Great video. Please do a best way to dry filament

  • @dalerbsr.5061
    @dalerbsr.5061 2 ปีที่แล้ว

    Thanks Tom, great video well done

  • @LudwigRuderstaller
    @LudwigRuderstaller 2 ปีที่แล้ว

    The LED Studio Light reflection (led pulse) in the prusas powersupply is very relaxing :)

  • @ZakLeek
    @ZakLeek 2 ปีที่แล้ว

    Super interesting video Tom, thank you so much! 🧡💜

  • @belladonnaRoot
    @belladonnaRoot 2 ปีที่แล้ว

    To me, the only significant data points are the quality, and the potential outlier of PETG being outdoors; which indicates cold may be a factor more than humidity. But the last one is...one point of data. Very good high-level analysis of the effects of humidity; thank you.

  • @delsydsoftware
    @delsydsoftware 2 ปีที่แล้ว +1

    I managed to accidentally do the same experiment. I had most of my filament and printers in storage in an unheated garage in Oregon for a year. During the time this filament was in storage, the humidity meter fluctuated between 75-95% humidity, with temps anywhere from 35F-75F. I had Hatchbox and Taclink PLA stored in the open, along with some eSun PETG and some generic TPU. Every roll of Hatchbox PLA ended up being just fine, and I was able to print high quality parts with all of it. Taclink's PLA would print fine, but the filament became super brittle. It would often break in the bowden tube during a print. Dehydrating it didn't fix the issue, so I ended up having to throw out the entire lot. Both the PETG and TPU printed terribly without dehydration, with a ton of bubbling and popping. Putting them in the dehydrator for a couple hours brought them back to normal, however.
    The Taclink issue is puzzling, because I remember getting super-reliable prints from it before it was stored. I'm assuming that there is a subtle formulation difference between it and Hatchbox. To be honest, Hatchbox black PLA is my usual workhorse filament, so I'm not surprised that it did better.

  • @medyk3D
    @medyk3D 2 ปีที่แล้ว

    For ASA and PETG I always dry them before printing. Even though I store them in vaccum bags with silica gel. The surface finish is just so much better.

  • @markusjacobi-piepenbrink9795
    @markusjacobi-piepenbrink9795 ปีที่แล้ว

    Well done!

  • @Techknowdude
    @Techknowdude 2 ปีที่แล้ว

    Excellent content. Did you notice the hydration altered how well the materials stuck to the build plate? I haven't done any specific testing, but historically I've had serious issues with PLA, Nylon, PETG, and PC sticking when they absorbed water.

  • @ianbertenshaw4350
    @ianbertenshaw4350 2 ปีที่แล้ว

    I never worried too much about moisture , I keep my filament (Usually PLA) in a vac bag and inside a cupboard to keep it clean and away from UV light . The same goes for the printer itself - it lives on a bench and has a Creality enclosure that has had the bottom cut out over it to keep the dust away from it and it also allows me to use a small fan fitted to the enclosure to suck out the fumes and pump them outside via a flexible pipe while printing .

  • @foamysking
    @foamysking 2 ปีที่แล้ว

    For the weighing aspect try getting a scale for firearms reloading those have to be extremely precise and could possibly end up showing a measurable difference

  • @stephennaylor4457
    @stephennaylor4457 2 ปีที่แล้ว

    That intro is amazing!

  • @Elephantine999
    @Elephantine999 2 ปีที่แล้ว

    Really interesting. Thanks!

  • @lakshithks5975
    @lakshithks5975 8 หลายเดือนก่อน

    Hey Tom great video,
    Wanted to know where is that jacket from, seems pretty nice

  • @PTEC3D
    @PTEC3D 2 ปีที่แล้ว

    I live on the Aussie Bass Coast and we regularly get days of > 70%RH and it definitely messes up PETG prints and sometimes even PLA. I made a rudimentary dry cabinet with a small-room dehumidifier that keeps 25C - 32C temp and < 35%RH (more when I remember to change the silicagel : ) and I still have to dry PETG regularly, and even PLA sometimes when I've left some out for a few weeks. I think the length of exposure is important, my theory is that even though the MSD says PETG will absorb moisture in just a few days it takes a week or two for moisture to penetrate deep enough to start pitting and spitting.

  • @SilvioMaranoSMH17
    @SilvioMaranoSMH17 8 หลายเดือนก่อน

    Most effect observed in this test are on printing accuracy but not mechanical because the time window wasn't long enough, it is needed much more time to see deep effects of moisture and how increase polymer chain degradation affecting specific material. E.g., PLA is less hygroscopic than PETG so it absorbs less water, but at same time it is more affected by hydrolysis than PETG (that is the most water resistant among the tested materials), this means that on long run moisture damages more PLA (that would become more brittle).

  • @PontusWelin
    @PontusWelin ปีที่แล้ว

    I have that scale. I hade to calibrate mine. But now it works fine.

  • @Steve211Ucdhihifvshi
    @Steve211Ucdhihifvshi ปีที่แล้ว

    Heres the thing too, its also about atmospheric humidity as well. So for example, I live in tropical Queensland Australia where its never lower than say 70% humidity and most often than not its 80% minimum. I discovered, that if the surrounding environment is humid the moisture boils off differently. Meaning i dont dry my nylon petg and asa/abs and petg. I keep it in a sealed container but the humidity never gets below about 35% in the box. You just adjust your settings to a point where you get good results. I did actually dry one filament once without changing a preset and it was overall good, but by the end of the day the humidity would have absorbed from the 88% air.
    Another thing I found is, quality manufacturers will have comprehensive manufacturer data sets sheets that you can pull all of this information from, you just need to know how to read the tech sheet.

  • @lupofroi
    @lupofroi 2 ปีที่แล้ว

    Great video, awesome to see your efforts. I just had a thought. You may see more accuracy with the filament weight measurements if you increase your sample size. For example, use a whole spool as a single sample. This is more expensive to conduct, as these tests are lossy. But, it would give a rough idea.
    What do you think about moisture causing filament to become more brittle over time?

  • @ethansdad3d
    @ethansdad3d 2 ปีที่แล้ว

    Thanks for the update on this hot topic. Maybe get a scale recommendation from Stefan. ;)

  • @dodgyaz
    @dodgyaz ปีที่แล้ว

    I've had PLA that was left out in the open for a few weeks pop holes in the outer wall of the print. You could hear it popping while printing. Stick it in a dryer overnight and the problem was resolved. The moisture in the filament was being turned into steam in the hotend and popping holes.
    I live in a dry part of Australia.

  • @XGerqusX
    @XGerqusX 7 หลายเดือนก่อน

    I know it's an old video, but figured you may need to know this. About the scale - there are two parameters on every scale. Resolution and accuracy. Resolution is what you ware referring to - 10mg. Accuracy on the other hand is connected to how much is weighted at a time, because accuracy is for example 0.5% of total weight. So if you put a heavy storage box on top of the scale, tare it and weight filament afterwards, you get accuracy of 0.5% of mass of the box + filament, not 0.5% of just filament, which can be all over the place. Cheers!

  • @Jobobn1998
    @Jobobn1998 2 ปีที่แล้ว +3

    For whatever it's worth, I notice an extremely significant difference in surface quality and stringing when printing with eSun PLA Pro that has absorbed water--especially when I'm printing minis with a 0.25mm nozzle. So much so that I dehydrate all my filament first and feed it from a drybox to get the absolute best minis I can. And the difference is really noticeable.

    • @crytocc
      @crytocc ปีที่แล้ว

      eSun seems to be particularly sensitive to moisture; my eSun PLA fared so poorly being stored in a normal room that after just a few weeks of being out in the open, the filament just straight-up _snapped,_ despite the printer not even being turned on at that time. I've never had those issues with my roll of Creality PLA, and my GST3D PLA+ seems to not care about being stored in room conditions either.

  • @corporaal1
    @corporaal1 2 ปีที่แล้ว

    Wow! A actual interesting sponsor message I didn’t get annoyed with and skip!

  • @rshort4296
    @rshort4296 2 ปีที่แล้ว

    Thanks for putting in the time for this video, I'll definitely stop leaving my filament out. One totally unrelated question though, where did you get that jumper?!

  • @DeusAequus
    @DeusAequus 2 หลายเดือนก่อน

    I keep my open filament in a box with silica desicant and it does a good job, I only actually dry intentionally if I notice signs of moisture on the results. Like egregious stringing or bubbling and popping. Can only really speak to PLA and PETG but I think my system works well. Just gotta do a small test print every time you put an open roll that could have absorbed some moisture on to know quickly.

  • @Uranday
    @Uranday 2 ปีที่แล้ว

    I would have liked to see what drying method is best to restore the filament. Good Video about the influence. Thx

  • @sierralarars
    @sierralarars 2 ปีที่แล้ว

    Might have already been suggested but you could try using one of the humidity monitors that woodworkers use for the before and after?

  • @licensetodrive9930
    @licensetodrive9930 2 ปีที่แล้ว

    I rarely dry PLA, but do dry PETG & TPU, especially the TPU, which I keep in the food dehydrator whilst its printing because wet TPU looks and performs bad.
    I've got a TPU reel in there right now waiting for me to print something, got distracted by a visitor but now back to the printing :)

  • @fortheregm1249
    @fortheregm1249 2 ปีที่แล้ว

    Thank you for including ABS. But what stands out most to me is the dimensional accuracy, Specially if you make stuff that need to fit or slide together.
    Any chance you could take a caliper to the chimneys ?

  • @tomjones2860
    @tomjones2860 2 ปีที่แล้ว

    Nice work Thomas... I would love to see a video investigating the mystery about "brittle" PLA. Almost everyone I know has had a PLA spool just start to shatter and break off brittle chunks. Some are convinced this is also a moisture problem, but for me this happens equally with PLA's stored in vacuum bags and with open PLA just left on a shelf... Also interesting I have never experienced PLA get brittle after it has been printed. and I have PLA brackets and holders at my work that are over 5 years old and they still look and work great.

    • @truantray
      @truantray 2 ปีที่แล้ว

      Plastic compounds have plasticizer additives to make the plastic flexible and flow better. These plasticizers are volatile and dry off as soon as you open the sealed bag. Brittle PLA has nothing to do with moisture, it's just age.

    • @dodgyaz
      @dodgyaz ปีที่แล้ว

      @@truantray Why do the rolls of brittle pla suddenly stop being brittle after they have been dried then?

  • @Rwnkl
    @Rwnkl 2 ปีที่แล้ว

    hi, great video! Any change in future you will do a review of eibos dryer (and maybe some others?).

  • @Badg0r
    @Badg0r 9 หลายเดือนก่อน

    Good video! I have build a printing corner in our shed that tent to get cold in the winter. I'm isolating it with a central heating system now, but it gets moist here. How about a test in a moist envoirnment and how long it will take if you print 1kg a week from a spool to see what the quality will do in that week?

  • @MeKnownAsI
    @MeKnownAsI 2 ปีที่แล้ว

    There is a lot of fear of "wet" filament, much of which I think is unfounded. I have comments regularly about my filament being out. I've not seen dramatic problems, or really problems at all with filament stored out in the open. Great video.

    • @ProtonOne11
      @ProtonOne11 2 ปีที่แล้ว

      I guess that is pretty easy to prove or disprove. It's not like a getting some large dessicant bags for a few $ and store your filament in a very dry environment for a week to see if it improves the result is hard or difficult or overly expensive.