G10 - The best print surface you've never heard of.

แชร์
ฝัง
  • เผยแพร่เมื่อ 26 เม.ย. 2024
  • Even if you only print PLA I highly recommend giving G10, otherwise known as FR4 or Garolite a go. I've been testing this cheap print surface on a range of materials and it's quite impressive indeed!
    Join the Maker's Muse Community - www.makersmuse.com/maker-s-mu...
    Where to find G10 (regularly updated, send through your suggestions for reputable suppliers!).
    //International//
    au.banggood.com/custlink/v33Y...
    //US//
    ePlastics - www.eplastics.com/G10NAT-060X...
    McMaster - www.mcmaster.com/garolite/mul...
    MatterHackers- www.matterhackers.com/store/c...
    Amazon - www.amazon.com/gp/search/ref=... SHEET 1/16 (search terms, direct links go out of stock too fast.)
    //UK//
    www.aiplastics.com/epoxy-4w-e...
    //Australia//
    www.artisansupplies.com.au/pr...
    50 3D Printing Tips and Tricks - gumroad.com/l/QWAh
    3D Printing Essentials - www.amazon.com/shop/makersmuse
  • วิทยาศาสตร์และเทคโนโลยี

ความคิดเห็น • 1.7K

  • @mozkitolife5437
    @mozkitolife5437 2 ปีที่แล้ว +617

    Alternative title: "The print surface _they_ don't want you to know about."

    • @MakersMuse
      @MakersMuse  2 ปีที่แล้ว +237

      Print bed companies hate him!

    • @jimurrata6785
      @jimurrata6785 2 ปีที่แล้ว +37

      This one little trick they use for perfect print results...

    • @backgammonbacon
      @backgammonbacon 2 ปีที่แล้ว +17

      It deforms if used incorrectly so clearly not beginner friendly. Companies don't want their products returned because the bed melted....no rocket science why its not used widely. Outside of nylon this seems to perform no better then pei which has none of the warping downsides.

    • @WhenDoesTheVideoActuallyStart
      @WhenDoesTheVideoActuallyStart 2 ปีที่แล้ว +4

      @@backgammonbacon There's FR4 made for high heat, only difference is the polymer. I'd recommend that instead of G10

    • @arbitrary_username
      @arbitrary_username 2 ปีที่แล้ว +5

      @@MakersMuse Thanks a lot for not being like that!

  • @AndrewWorkshop
    @AndrewWorkshop 2 ปีที่แล้ว +520

    Used G10 for custom drone frames. Recently as a transom for a boat. Awesome i can use the left overs for a print surface now, thanks!. Super useful material.

    • @franteryda4730
      @franteryda4730 2 ปีที่แล้ว +3

      Hi Andrew!! What a surprise to find you here

    • @NACAM42
      @NACAM42 2 ปีที่แล้ว +7

      It's really popular for handgun grips too.

    • @xymaryai8283
      @xymaryai8283 2 ปีที่แล้ว +2

      what kind of drones, have you had luck with smaller 5inch or less? if its easy to cut, i might cut out a 4inch frame, but carbon is already pretty cheap for frames that small

    • @MrSolLeks
      @MrSolLeks 2 ปีที่แล้ว +2

      I'v got G10 grips for one of my pistols, I never thought it would be used for a print surface lol.

    • @KernsJW
      @KernsJW 2 ปีที่แล้ว

      Now that i think of it, I do have some old drone frames made from g10. I imagine it would work well on a rekon 1s lr instead of 3d printing the frame

  • @wayneparker4708
    @wayneparker4708 2 ปีที่แล้ว +43

    My CR20 has a G10 print bed with a fake build tack surface applied as a sticker. After watching this video, I flipped the bed over and the result was amazing. The first layer surface has a mirror finish like glass. Forget the over documented and TH-camd "Must Have" upgrades. This tip has been the single biggest improvement in my 3D printing since I started. Thanks Angus!

  • @Zeldur
    @Zeldur 2 ปีที่แล้ว +189

    On the topic of making things for printers well known, something that can help clean out the nozzle are guitar strings. They're really thin, flexible, and you can buy a ton for a few bucks

    • @ironbeagle1610
      @ironbeagle1610 ปีที่แล้ว +3

      lmao for a second I thought of my dad's thick metal acoustic guitar strings and I had a heart attack thinking about running those through a printer lol.

    • @Zeldur
      @Zeldur ปีที่แล้ว +4

      @@ironbeagle1610 I'm not sure if these are acoustic or electric. Surprisingly, it has the diameter of the string in mm on the packages. But yeah, not the lower strings with the coil, the higher pitched ones

    • @clammaster4
      @clammaster4 ปีที่แล้ว +3

      i hadnt thought about that...and i have a bunch of used ones i wanted to recycle! thank u!

    • @Der_Kleine_Mann
      @Der_Kleine_Mann ปีที่แล้ว +2

      I use acupuncture needles for cleaning my nozzles.

  • @matthewweinberger7023
    @matthewweinberger7023 2 ปีที่แล้ว +162

    if your sheet does warp just bake the sheet between 2 sheets of glass at ~130 for a couple hours then let it cool slowly

    • @hyperspeed1313
      @hyperspeed1313 2 ปีที่แล้ว +10

      Celcius?

    • @matthewweinberger7023
      @matthewweinberger7023 2 ปีที่แล้ว +18

      @@hyperspeed1313 yep. Make sure the glass is flat and cool the sheet as slowly as you can

    • @rjwaters3
      @rjwaters3 2 ปีที่แล้ว +15

      to elaborate for anyone else that stumbles in here, you want to let the temperature lower on the sheet as evenly as possible, else itll shatter as one part cools faster and bends, well its a glass like thing, glass doesnt bend it shatters. need to heat it evenly too or the same will happen if it even matters for this material.
      also unless itll adhere to stuff at that temperate wouldnt any sort of really flat+smooth and rigid material work (e.g. a metal sheet?)

    • @0thorgal0
      @0thorgal0 2 ปีที่แล้ว +11

      @@matthewweinberger7023 Not all polymers have a glass transition temperature and most of the epoxy resins are among of them. Once the are cured the reaction is done and you have one board size molecule of polymer that can't be shaped by temperature like thermaplastics do. The only thing that is working here is pressing them flat.

    • @matthewweinberger7023
      @matthewweinberger7023 2 ปีที่แล้ว +1

      @@0thorgal0 then mine was plastic. It was warping under heat, now it doesn't

  • @mathewfitzpatrick5645
    @mathewfitzpatrick5645 2 ปีที่แล้ว +250

    I've always known of G10 as "the standard" in knife handles, didn't know it was so useful elsewhere.

    • @BEdmonson85
      @BEdmonson85 2 ปีที่แล้ว +29

      It's funny that it has so many different trade names. I've never heard of G10, but I've made custom circuit boards at home for years and so I've used it heaps, but always known it as FR-4. (btw, with the cheap pcb services available now, it's pretty impractical to diy boards at home these days)

    • @bunit1701
      @bunit1701 2 ปีที่แล้ว +10

      Same, I only knew it was used for handgun handles, had no idea it was in PCBs.

    • @Tom-uj4uf
      @Tom-uj4uf 2 ปีที่แล้ว +4

      What's up fellow knife guy!

    • @johngregory4801
      @johngregory4801 2 ปีที่แล้ว +8

      Or grips for pistols, mainspring housings for 1911's

    • @slipjointyjan548
      @slipjointyjan548 2 ปีที่แล้ว +2

      Same, it was a nice surprise to learn it has more applications than knife handles.

  • @brianmiller40
    @brianmiller40 2 ปีที่แล้ว +4

    Thank you soooo much. I use PETG for most of my projects and over time I have destroyed around a dozen beds of all types. Since switching to G10 I have had 0 failures and I'm still using my first G10 bed. I have been using the 1.5mm sheets on both of my printers for about a month running on average 20 hours a day. Great first layers and they always release when cool. Best $12 I have ever spent plus like you said you can get them in different colors. Thanks again. Great channel, great content, keep it going!!!!

  • @christopherhsu5946
    @christopherhsu5946 2 ปีที่แล้ว

    This material has been a true game changer for me. No more issues with build plate adhesion. Thank you, thank you, thank you for making this video!!!

  • @nunyabusiness8538
    @nunyabusiness8538 2 ปีที่แล้ว +210

    i’ve been into pocket knives for years. G10 is like a like a household word for me lol

    • @Samplehorse
      @Samplehorse 2 ปีที่แล้ว +44

      Thays exactly what I thought “G10? Like the same G10 that every knife company makes handles out of?”

    • @jackallen3742
      @jackallen3742 2 ปีที่แล้ว +7

      My thought exactly

    • @CSGraves
      @CSGraves 2 ปีที่แล้ว +17

      Hey, I heard this is where the knife bros hang out.

    • @P-tricky13
      @P-tricky13 2 ปีที่แล้ว +7

      Ahh my people!

    • @Freakmaster480
      @Freakmaster480 2 ปีที่แล้ว +5

      I had the same thing happen to me. More into fixedblades so I don't hear about g10 as often but still relatively frequently.

  • @FilamentFriday
    @FilamentFriday 2 ปีที่แล้ว +522

    I’ve been using the Elegoo Neptune 2 with the G10 bed flipped over as you mention. Works better than their Buildtak which sticks too well. Great video.

    • @MakersMuse
      @MakersMuse  2 ปีที่แล้ว +78

      It's beyond me why they whack that terrible surface on an already good one!

    • @flixmyswitch
      @flixmyswitch 2 ปีที่แล้ว +4

      fR4 may be better I will have to check the data sheets. PCB are made from fr4 and not g10

    • @Jehty21
      @Jehty21 2 ปีที่แล้ว +2

      @@MakersMuse is Buildtak more durable than G10?
      Because that would explain it.

    • @unusualcomment9731
      @unusualcomment9731 2 ปีที่แล้ว +2

      @@MakersMuse From my experience buildtak is quite good, but in the other hand I never been able to make my parts stick to much expensive ultrabase plate so everyone has to find the material that suit him well!

    • @UncleJessy
      @UncleJessy 2 ปีที่แล้ว +4

      🤯 never even thought about printing on that flipped side

  • @seangreenhalgh7961
    @seangreenhalgh7961 2 ปีที่แล้ว +15

    If you want to use the thinner FR4 you can buy large sheets of thermal interface silicone. Basically this is the stuff that goes on heat sinks between heat sink and surface. Works pretty well as a low tack adhesive so you can remove the surface

  • @jkosh2046
    @jkosh2046 2 ปีที่แล้ว +1

    Thank you for this video. Just started using g10. I have to say that this is the best upgrade I have done to my printer so far. First layer print is beautiful. I have been able to tune my bed level for amazing adhesion with no elephant foot and they basically fall off the bed when cool. Thank you very much. I have a 1/32 sheet. Bought a cheap one just to try it. Going to go to a thicker sheet even though I've had no issues with it and I've ran 20 or so prints so far, only had 1 part warp.

  • @KernsJW
    @KernsJW 2 ปีที่แล้ว +11

    Many knives use G10, its a very popular handle material. If it gets marked up, you can just wet sand it smooth. 320 will knock it down quick and then take it from there to however shiny you want. For a matt to glossy finish, you will not have to go too high. If you want glossy smooth like glass, you will need to use a plastic polish.
    Nice video!

  • @startedtech
    @startedtech 2 ปีที่แล้ว +63

    As soon as you showed the G10 with your old project, instantly knew it was PCB material! Looks a lot like the uncolored pcbs you see in old electronics.

  • @Pippatis
    @Pippatis 2 ปีที่แล้ว +11

    Thanks for making this video! I'd been having the exact same issues with PETG sticking too well or not at all, but I needed to print with it because PLA is too brittle for my needs - So, when I first saw this, I instantly went and bought some. Haven't had a single issue with bed adhesion since and the parts just snap right off with little to no resistance. It's a real game changer!

    • @mollyallen2400
      @mollyallen2400 2 ปีที่แล้ว

      This is helpful! I'm helping students learn the ropes and PLA has been snapping during loading and refuses to stick. Finally got it to stick with borosilicate bed plate and gluestick, and print starts looking like a slug after about 1/2 - 3/4" height off of plate (with exception of pre-loaded gcode on sd card (a cat). I think I'll give it a go with a different filament! :) (and order some G10!!)

    • @floodo1
      @floodo1 10 หลายเดือนก่อน

      aight, gonna try this with new roll of PETG …

  • @fapangel7771
    @fapangel7771 2 ปีที่แล้ว +4

    After smashing my head against a wall trying to print PETG for the first time, I found this video. After some tweaking, calibrating, and discovering that a warped aluminum bed on an Ender can, indeed, bow the glass on top of it a bit, I've got a sheet of 1/32nd FR4 on my printer that works exactly as advertised - sticky when warm, releases easy when cool, just like the Creality beds with the special coating on them that spoiled me so much. I'll have to do a little tweaking to get PLA+ dialed in on this surface too, but once I do, I'll finally have a multi-plastic build surface that's no effort, no muss, no fuss, no blue tape and no goddamn glue.
    Can't thank you enough for this video.

    • @MakersMuse
      @MakersMuse  2 ปีที่แล้ว +1

      I went through all the same struggles, so glad to hear the FR4 solved it for you!

  • @AerikForager
    @AerikForager 2 ปีที่แล้ว +186

    You may have better luck searching for FR4, which is the fire retardant version of G10 used in printer circuit boards. :)

    • @jimurrata6785
      @jimurrata6785 2 ปีที่แล้ว +23

      FR4 is also great for model rocket fins and bulkheads.

    • @t_z1030
      @t_z1030 2 ปีที่แล้ว +12

      That's mentioned as one of its names in the video. As an Australian, I can also corroborate that it is has been very hard to find here whether you look for G10, FR4 or Garolite.

    • @someoneonly
      @someoneonly 2 ปีที่แล้ว +5

      Hold up if its similiar to FR4 cant you print directly on the reprap heated bed pcb o_o

    • @0thorgal0
      @0thorgal0 2 ปีที่แล้ว +6

      @someoneonlylol Yes and no. Those bed have typically copper on both sides, covered in solder mask. I have mine made of single side PCB without solder mask, but i still like to cover it with glass, because you won't find 3mm thick PCB easily and thinner likes to bend alot.

    • @mrmas2535
      @mrmas2535 2 ปีที่แล้ว +1

      @@t_z1030 Maybe try Glass Phenolic Plastic Sheet, the seller i found on ebay had this in his description

  • @GRBtutorials
    @GRBtutorials 2 ปีที่แล้ว +91

    0:00 G10, what is that?
    0:36 Oh, it’s FR4, the same material used in PCBs! That also has the extra advantage that you can use a PCB if you can’t find alternatives.

    • @KentoCommenT
      @KentoCommenT 2 ปีที่แล้ว +15

      Same. I was like
      "Wow, I've heard about so many beds, even rare ones like FR4 for Nylon, but not G10. Let's find out what this mysterious material is"
      "Oh it's just FR4"
      "Oh. You can use it for more than just Nylon??"

    • @flixmyswitch
      @flixmyswitch 2 ปีที่แล้ว +5

      @@KentoCommenT fr4 is better read some of the other comments high temp and fire retardant

    • @sonosus
      @sonosus 2 ปีที่แล้ว +2

      Hmm so I could design a PCB without copper or solder mask and have JLCPCB fab it.... Might have to give that a go

    • @KentoCommenT
      @KentoCommenT 2 ปีที่แล้ว +1

      @@sonosus Wouldn't a copper ground plane each side aid in heat uniformity?

    • @sonosus
      @sonosus 2 ปีที่แล้ว +1

      @@KentoCommenT Isn't it the raw FR4 that gives the material the stickiness? Maybe having a ground plane on one side could work though. I'll give it a shot on my Ender 3 sometime.

  • @RASbit
    @RASbit หลายเดือนก่อน

    This is why I am subscribed to you. You provide such great information on 3d printing. I am new to 3d printing and have just started my printing journey using a Anycubic mega pro 3d printer. I've only printed three prints so far and they all came out OK but man where they hard to remove from the build plate. I've never heard of this material G10 but seeing you remove your print with such ease made my jaw drop. I will definitely stay tuned for more :)

  • @nay1978miles
    @nay1978miles ปีที่แล้ว

    The best 3D Printing content creator I've seen....Even better that you're an Aussie too mate. Straight to the point, highly technical if you need to be and no nonsense explanations. Very much appreciated!!

  • @eideticex
    @eideticex 2 ปีที่แล้ว +35

    No need for bed clips with G10. It's very easy to form under heat. Just take a heat gun along the edge and use a ruler to push it squared with the corner, when it cools it'll shrink just enough for an interferrence fit.

    • @macgyver9134
      @macgyver9134 2 ปีที่แล้ว +2

      there is going to be some deflection upwards if you do this, leaving you with a bowl shaped bed.

  • @outofdarts
    @outofdarts 2 ปีที่แล้ว +180

    That's an awesome material! I might have some ideas for use besides just a print sheet…

    • @MrJelle18
      @MrJelle18 2 ปีที่แล้ว +14

      Hybrid 3D print and laser cut blaster design, you say?

    • @MakersMuse
      @MakersMuse  2 ปีที่แล้ว +23

      @@MrJelle18 Definitely never laser fibreglass, but it CNC's nicely with a carbide burr :D

    • @MrJelle18
      @MrJelle18 2 ปีที่แล้ว +7

      @@MakersMuse Ah, my bad! Always learning, I thought milling it would be worse than lasering on account of the fine particles, just goes to show what I know.

    • @BEdmonson85
      @BEdmonson85 2 ปีที่แล้ว +3

      @@MakersMuse can you elaborate? I've never used a laser cutter, why shouldn't fiberglass be laser cut?

    • @expertoflizardcorrugation3967
      @expertoflizardcorrugation3967 2 ปีที่แล้ว +5

      @@MrJelle18 for fine particles it's usually a case of better safe than sorry, but I don't know terrible much about fiberglass or how it decides to behave when you laser or mill it

  • @trustyourforce4041
    @trustyourforce4041 ปีที่แล้ว +1

    I just got this and it's amazing. Sticks perfectly and comes off easily.

  • @knightsljx
    @knightsljx ปีที่แล้ว +2

    I managed to put a G10 print bed onto a Prusa MK3S+. You need a some sort of single sided spring steel sheet, I happen to have a Creality one, but you need one that has the bare spring steel exposed. And you need a 1mm G10 sheet. The closest on Aliexpress is a 250mm x 250mm x 1mm sheet. Then you must set your PINDA such that it is only about 1mm above the tip of your nozzle. Set the spring steel sheet bare metal side up then clip the G10 on top of the spring steel. This really pushes the limit of the tolerance of the available space for the PINDA to work. IF you encounter the tip of the nozzle colliding with the G10, the printer will throw an error. This means your PINDA probe needs to be lowered more. If you get it right, there will be just enough space for the PINDA to complete its mesh leveling and then you can do the Live-Z adjustment

  • @MrCarlozan96
    @MrCarlozan96 2 ปีที่แล้ว +4

    Awesome video. Love the extent of the research you put into every project. Keep it up.

  • @woodwaker1
    @woodwaker1 2 ปีที่แล้ว +3

    One of the best videos in ages. I agree that too many products are hyped especially to new users that are having trouble with first layers. I just had a local glass shop cut some 1/4 in ( about 6mm) glass for me at 235 x 235 mm. They work great on my Ender 5 - heavy, but the heat is even and they are FLAT - $6.5 each. I now want to test the G10. Thanks for letting us know about this.

  • @YuanLiuTheDoc
    @YuanLiuTheDoc 2 ปีที่แล้ว +2

    My jaw physically dropped when you showed the warp. Really useful info!

  • @eddiewilliams219
    @eddiewilliams219 2 ปีที่แล้ว

    After months of fighting adhesion issues with the stock glass on my Ender 5 plus, I got a sheet of G10 and it works flawlessly! Excellent video!

  • @elsegan
    @elsegan 2 ปีที่แล้ว +34

    I've been doing this since 2016!! But I have an unetched PCB, the copper sheet makes my bed temperature infinitely more reliable!

    • @BrazenRain
      @BrazenRain 2 ปีที่แล้ว

      Nice idea!

    • @McNibbler
      @McNibbler 2 ปีที่แล้ว +1

      That sounds brilliant! What thickness do you use, 62.5mil?

    • @McNibbler
      @McNibbler 2 ปีที่แล้ว

      Do the copper pours cause any issues with heating times

    • @ProtonOne11
      @ProtonOne11 2 ปีที่แล้ว

      You are basically talking about a different material then, as the soldermask on top of the copper is another surface than the raw epoxy resin of an FR-4 PCB. If it still works for your plastics, thats great. But i guess you could end up having issues, depending on the soldermask they used.

    • @pmc_
      @pmc_ 2 ปีที่แล้ว +9

      @@ProtonOne11 An unetched PCB doesn’t have any solder mask - solder mask is applied after etching

  • @RajvirSingh1313
    @RajvirSingh1313 2 ปีที่แล้ว +104

    did anyone realize that he is wearing an LTT t-shirt?

    • @MakeItWithCalvin
      @MakeItWithCalvin 2 ปีที่แล้ว +8

      If you look back in old videos you see his LTT hoodie ;-)

    • @Tazarul
      @Tazarul 2 ปีที่แล้ว

      Literally the first thing I noticed

    • @Steph.98114
      @Steph.98114 2 ปีที่แล้ว

      Wow, they cost so much to get shipped to Australia

    • @tylersutton2216
      @tylersutton2216 2 ปีที่แล้ว

      i didnt,lol

  • @andrewb9774
    @andrewb9774 ปีที่แล้ว

    Hey Angus congrats on hitting the 1 million subscriber mark and thanks for making this video; I'll be testing G10 out!

  • @hansdampft561
    @hansdampft561 2 ปีที่แล้ว +1

    Thank you for the Video! I watched your video and went to my cellar started my CNC mill grabed on of my 1.5mm FR4 sheets and milled it to fit my Ender 5 Plus. Printed some complex models with PETG. Awesome results, no problems at all!

  • @urano1988
    @urano1988 2 ปีที่แล้ว +7

    I have a custom heated bed made by cutting a spiral in a single sided copper plated FR4. I have a sheet of glass on it's top as the actual printing surface, but nice to know that I can also print on the back of my heating element!

  • @JohnAldred
    @JohnAldred 2 ปีที่แล้ว +5

    I've been printing PETG on FR4 for the last three years. It's fantastic stuff. No glue, no spray, no tape, no mess. Great for PLA, too. Bit too sticky with TPU, but it works. :)

  • @abc_def-55
    @abc_def-55 ปีที่แล้ว

    Had been printing with PETG for a while on my carborundum glass plate with no issues, but changed filament vendors and a large print finally did what everyone warns of and took couple small shards of the glass with it... Bought a G10 sheet due to this video, and so far have been very happy with it. Works just like the carborundum one, even using similar settings for bed temp etc, but with the benefit that I can bend the 1mm sheet to pop parts off if I'm in a hurry. TYVM for the tip and recommendation! :)

  • @user-wu7rf6kl6j
    @user-wu7rf6kl6j 2 ปีที่แล้ว +1

    Thanks Aungus, I found the supplier before I found your vid. Google actually led me to your vid when I was trying to research if I could use the knife makers g10 for a build plate surface. I was looking at the .5mm sheet but now seeing your results I'm going for the 1.5 and 3mm cause I want to have a crack at nylon. Thanks again and keep up the good work mate

  • @EnricoConca
    @EnricoConca 2 ปีที่แล้ว +159

    I guess that the G10 sheet deforms because you are hitting the glass transition temperature when printing. It might be worth to experiment with higher Tg FR-4 (155 °C is common in PCB manufacturing, 170 °C is also available)

    • @0thorgal0
      @0thorgal0 2 ปีที่แล้ว +14

      As the fiber glass is bound with epoxy resin in G10 it do not have a glass transition temperature. And I remember that 120-150°C is the point then most of epoxy resins will start to desintegrate when kept under those temperatures for longer period of time. The deformation is solely done by the forces that would otherwise cause delamination or warping.

    • @mariohernandez1111
      @mariohernandez1111 2 ปีที่แล้ว +13

      @@0thorgal0 every polymer has a glass transition temperature. That includes epoxy. You can find the glass transition temperature of most reputable epoxies in their respective datasheets.

    • @donaldasayers
      @donaldasayers 2 ปีที่แล้ว +1

      @@mariohernandez1111 Er no, thermosets don't

    • @mariohernandez1111
      @mariohernandez1111 2 ปีที่แล้ว +27

      @@donaldasayers You are confusing concepts. Thermosets have melting points above the decomposition temperature (so, you could say they don't have a melting point). Thermoplastics, on the other hand, have melting points below decomposition temperature. Both types of polymers may have a glass transition temperature below the decomposition temperature.
      Look up examples on epoxies and their glass transition temperatures. This is something you can easily find by googling.
      PS: I was making a simplification when I said every polymer has a glass transition. Only amorphous or semi-crystalline polymers have a glass transition. Most polymers are like this, thermoset or thermoplastic.

    • @GENcELL2014
      @GENcELL2014 2 ปีที่แล้ว

      Aka FR5

  • @realryleu
    @realryleu 2 ปีที่แล้ว +3

    IPA is amazing. It evaporates so quickly (so it doesn't damage electronics unless you're stupid with it) and it does a great job of breaking up gunk. 10/10, would recommend.

  • @edumaker-alexgibson
    @edumaker-alexgibson 2 ปีที่แล้ว +5

    For your PETG/Glass issues: I use (genuine) 3D-Lac and this defeats the excessive stick especially if you twist the part off. This also works for TPU onto G10/FR4.

  • @sparkycorkers1196
    @sparkycorkers1196 2 ปีที่แล้ว

    thank you for taking the time to list suppers in different countries!

  • @williamgreen5575
    @williamgreen5575 2 ปีที่แล้ว +17

    You do realise this exactly what 'printbite' is. I've been using the FR4 side of copper clad PCB for years. The copper gives a more even heated surface too

  • @michaelteta875
    @michaelteta875 2 ปีที่แล้ว +6

    You are right, I have never heard of this! That’s insane

  • @gamecoartisansupplies8568
    @gamecoartisansupplies8568 2 ปีที่แล้ว +1

    Thanks for the shout-out, much appreciated 👍. We're glad you like G10.

    • @MakersMuse
      @MakersMuse  2 ปีที่แล้ว

      Thanks for being a great local supplier! It's good stuff.

  • @CrowClouds
    @CrowClouds 2 ปีที่แล้ว

    You're unreasonably happy and I love it

  • @patrickfle9172
    @patrickfle9172 2 ปีที่แล้ว +3

    It's a very versatile material. A friend of mine made leaf springs for a bicycle project from it

  • @janisdambergs4362
    @janisdambergs4362 2 ปีที่แล้ว +3

    Bought G10 2mm. Works realy well so much better than original glass plate on ender 3 v2. Amazing. Sticks every time. Amazing stuff. Thank👍👍👍🇱🇻

  • @ruftime
    @ruftime 2 ปีที่แล้ว

    Thank you Angus!
    Love g10, never felt the need for it on my Prusas, but we’ve been making multi rotor and rc vehicle frames for years😎

  • @eyemeanattia
    @eyemeanattia 2 ปีที่แล้ว +1

    Just received my G10 sheets. Wow this stuff is amazing.
    Thanks alot for making this video.

    • @MakersMuse
      @MakersMuse  2 ปีที่แล้ว

      Nice! Thanks for letting me know

  • @digitalfire01
    @digitalfire01 2 ปีที่แล้ว +22

    I've always had issues printing PETG, usually on the first few layers regardless of what I do. And I mostly print with much more difficult filaments such as glass reinforced nylon. Will try garolite, thanks for the share.

    • @hyksos2
      @hyksos2 3 หลายเดือนก่อน

      I know this is very old, but I also had lot of trouble with initial layer adhesion with PETG, even if I cleaned with alcohol, my trick to print PETG is to increase bed temperature to 90 degree and hot end to 250, then disable fan for the initial layer, after the initial layer bring fan and temperature to normal setting (bed to 80, hot end to 240), I had 100% success rate with this.

  • @BillieRuben
    @BillieRuben 2 ปีที่แล้ว +15

    ooh! this is so cool Angus! Thank you for sharing!! I love printing on smooth surfaces, and I gotta admit, the idea of a pastel pink bed is wildly appealing. 😁

    • @MakersMuse
      @MakersMuse  2 ปีที่แล้ว +6

      Pink makes everything better :D

  • @cwjdog57
    @cwjdog57 2 ปีที่แล้ว

    FR4 is my favorite material for keyboard plates as well, glad to see that it's just a valuable material no matter what hobby I get into!

  • @maulitdipshooter
    @maulitdipshooter 2 ปีที่แล้ว

    GREAT VIDEO! Angus I have always enjoyed your videos. Great work and keep it up!

  • @janzwiebel8518
    @janzwiebel8518 2 ปีที่แล้ว +5

    Been using this for years. Only I buff it with sandpaper so I don't have a glossy underside. Works like a charm

    • @sevdev9844
      @sevdev9844 2 ปีที่แล้ว +1

      Ah, thanks. But let's remind each other about security: Masks, maybe wet sanding, maybe working outside.

  • @testtesting5088
    @testtesting5088 2 ปีที่แล้ว +4

    I've been printing on an Ender 3 pro for about a year on G10. Everything sticks to this, only issue is you need either a klinky probe og bltouch type probe to do a bed mesh. I have printet Nylon, ABS, ASA mainly on this surface and i agree with you Angus. This is one of the better unknown facts that this surface just is insanely good for FDM printers.

  • @karl80126
    @karl80126 2 ปีที่แล้ว +1

    I didn't realize that Garolite and G10 were the same. I had shopped for Garolite in the past and it was much much more expensive than G10.
    Thank you.

  • @DoryVideo
    @DoryVideo ปีที่แล้ว +1

    you are a genius! I just bought some of this for my Ender 3 Max and it was just as you claimed it would be.... a 300 x 300 mm sheet of this material in the UK was less than £10 (i bought 1.6 mm, 2 mm & 4 mm) and the glassy first layer is something to behold! So far no issues and 10 prints in the release when cooling is excellent. I've been using 60 degrees on the bed and when it gets to room temperature (around 18-20 degrees) the prints just pop off, even at close to 30 degrees prints come away with very little effort (you can't say the same for the glass beds!). Thanks for the tip!

  • @EmbraceMaking
    @EmbraceMaking 2 ปีที่แล้ว +13

    Will work well with Nylon and this is what Markforged uses for their print beds. Edit to add, markforged does not use a heated bed, and the platform is roughly 6mm thick... so it's extremely rigid unlike the test here with Nylon on a very thin sheet. I've printed 100s of hours on those machines with the reinforced nylon and I have yet to replace the print bed.

    • @huberttrzewik5644
      @huberttrzewik5644 2 ปีที่แล้ว

      They use G10 or FR4 or what?

    • @SianaGearz
      @SianaGearz 2 ปีที่แล้ว +1

      @@huberttrzewik5644 they won't tell you, but it's probably FR4.

  • @johnbickford9221
    @johnbickford9221 2 ปีที่แล้ว +3

    I discovered Garolite (G10) when researching how to print with nylon on my MakerSelect V2. I had no idea it was useful for all the other materials you mentioned. I am in the states so yay McMaster-Carr!

  • @stonecraft745
    @stonecraft745 2 ปีที่แล้ว

    First test came out so good, thank you so much!

  • @sphericalmobius
    @sphericalmobius 2 ปีที่แล้ว +1

    It really works! I peeled the surface off the default Ender3 and hiding beneath, G10. Thanks for sharing. Definitely earned this sub

  • @TheEricSchubert
    @TheEricSchubert 2 ปีที่แล้ว +11

    Tip for keeping the build plate stuck to the aluminum bed: use some silicone thermal pad between the bed and the G10 surface. It helps with getting good thermal contact, and also provides a moderately-sticky surface to keep the build plate from sliding around at all. I currently use it with my glass bed and it's worked great without any clips.

    • @brentowen8857
      @brentowen8857 2 ปีที่แล้ว +1

      Where do you get this thermal pad that is large enough?

    • @TheEricSchubert
      @TheEricSchubert 2 ปีที่แล้ว +1

      @@brentowen8857 I bought mine on Amazon. I only found one that was 200x200mm, which worked okay for my Ender 3. But you can buy another and cut strips to fit empty portions of the bed.
      I will mention, now that I've used it for a while, that the bottom of the glass bed needs to be clean for it to stick well to the thermal pad. This happens a lot when I remove the glass bed. If I get fingerprints on it, the bed can gradually slide out of position. A bit of alcohol will fix it up again. But test that the bed won't move after replacing it. Dust and junk can also gradually get stuck in the thermal pad and make it less effective at sticking to the bed over time.
      I've recently swapped to a magnetic spring steel bed with PEI on it. That thing isn't going anywhere.

  • @theftking
    @theftking ปีที่แล้ว +3

    Every pocket knife enthusiast is like "Psh I know all about G10!"

    • @l_Knights_l
      @l_Knights_l ปีที่แล้ว

      You already know 😎

  • @themeek351
    @themeek351 2 ปีที่แล้ว +1

    Wow, my dad had some of this stuff when I was just a kid! I wish I knew about this stuff years ago, since bed adhesion is the biggest issue I've had to deal with! The only problem with this material is the fact that both of my printers use the hot hotend to touch the bed in a grid to automatically level it, so I think it would melt it! Had this problem with buildtak too! So, I will have to change the order of the heating and leveling in the custom g-code and I will probably have to udjust the Z-offset to compensate for the thermal expansion of the nozzle! Thanks for this great video!

  • @t0nito
    @t0nito 2 ปีที่แล้ว

    Never heard of this before this video, I went ahead and ordered a sheet for my 3D printer and it's pretty amazing!

  • @JohnOCFII
    @JohnOCFII 2 ปีที่แล้ว +4

    I use the MatterHackers Garolite. It is attached to a spring-steel sheet. I’ve only used it for nylons so far - primarily use textured PEI for PLA and PETG

  • @ScriptonicPipes
    @ScriptonicPipes 2 ปีที่แล้ว +3

    I work at McMaster-Carr! Looks like I gotta pick up some G-10 next week!

    • @the_irav
      @the_irav 2 ปีที่แล้ว

      You work a maker's paradise haha

  • @janvaniersel9476
    @janvaniersel9476 ปีที่แล้ว

    I've been using FR4 1.5mm on my Prusa, on top of my steel bed to keep the pinda working. Just fits. Ever since I've been using it (6 months now), the prints (PLA and PETG) simply work beautifully. No needs for adhesives and after the cool down, the prints are often already fully separated on the print bed. After a lot of hassle, this makes it so much nicer. Thanks!

  • @gallantpawn
    @gallantpawn 6 หลายเดือนก่อน +1

    Started using G10 after I too had problems with PETG. Awesome adhesion now! Printing eSun PETG on an Ender3 settings are 245 degrees C on a .4 nozzle / 80 degrees C on the bed / 50% print speed (see on the printer) / 0.85 Z-offset. Thanks Maker's Muse!

  • @dbackscott
    @dbackscott 2 ปีที่แล้ว +7

    I’ve been having great success with smooth pei adhered to a spring steel sheet (w/ after-market magnetic base). I roughed it up with a bit of 00 steel wool and gave it a light coat of hairspray. I mainly print with petg, pla, and tpu, and all three work well. I’m printing with a Longer LK4 with a BL Touch and a slightly modified extruder to accommodate flexible filament.

    • @secretweaponevan
      @secretweaponevan 2 ปีที่แล้ว +3

      When I first got into 3d printing 3 years ago, I was told to get PEI coated spring steel from a veteran printer.
      I was stubborn/scared because I had a slightly-warped Ender 3 bed, so I only used the borosilicate glass for flatness, utilizing hairspray and isopropyl.
      I went with PEI coated spring steel about 2 months ago, and I'll never go back.
      I only print PLA and PETG so far, and the prints stick like glue when bed is heated, and release cleanly when cooled/flexed.
      Use what works for you, but this $30 bed is amazing.

    • @Vortex-gz8se
      @Vortex-gz8se 2 ปีที่แล้ว +1

      @@secretweaponevan PLA releases pretty easily from PEI; however, PETG on PEI requires a release agent. You might get away with no release agent for PETG on PEI for a while, but eventually you will damage the it.

    • @engineer1692
      @engineer1692 2 ปีที่แล้ว

      @@Vortex-gz8se I've been printing with PETG and PLA on PEI spring steel sheet at 60C with no need for release agent.

    • @Vortex-gz8se
      @Vortex-gz8se 2 ปีที่แล้ว

      @@engineer1692 like I said you might get away with no release agent when printing PETG on smooth PEI for a while, eventually you will almost certainly damage it. Don’t you notice that PETG is a lot harder to remove that PLA?

  • @octogunsalata
    @octogunsalata 2 ปีที่แล้ว +25

    Guys... this is called epoxy resin. When printing on either carbon or fiberglass, you're printing simply on epoxy resin. If you like the properties of it, you can convert any printing surface of your choice to it by simply getting some laminating resin and putting a thin layer of it onto the surface (after sanding and degreasing it), and then harden it in your oven for some hours, according to instructions. If putting it on spring steel, you shouldn't over-bend the plate of course as the epoxy film could break. (what, on the other hand, helps in getting it off if you want to renew it) The fibers only give it their stiffness and strength, they do nothing to the surface itself.

    • @octogunsalata
      @octogunsalata 2 ปีที่แล้ว +5

      Hint: to prevent having a bulge form at the borders because of the surface tension of the resin, you should put a sheet of wax paper below that's larger than the printing surface and overlap the borders all-around a little with resin for about a half-inch. After hardening, you can carefully break or cut it off and sand it to get clean borders.
      However, it won't work with some of the exotic, overly thick printing surfaces that some people use, (like, several mm thick) as the difference in height to the wax paper is too large to have any effect. (depending also on the viscosity of the resin)

    • @aidankilleen5889
      @aidankilleen5889 ปีที่แล้ว +3

      You're right, but the cost and availability is what's really on display here. I work at a machine shop that does a lot of plastic work, I wonder how some of that would do... PEEK, for example, and some proprietary blends...

    • @octogunsalata
      @octogunsalata ปีที่แล้ว +1

      ​@@aidankilleen5889 The majority of inventions were discovered by trial & error and accidents, so, if you have access to unusual materials, I suggest trying to get your hands on some samples. However, before getting your hopes up after discovering a great, "new" material, I'd thoroughly check if it already has been discovered. In 3D printing, for example, I've seen plenty of unusual stuff exclusively in the world of highly expensive industrial 3D printers.

    • @octogunsalata
      @octogunsalata ปีที่แล้ว

      @@aidankilleen5889 Regarding PEEK - I think I've already seen printing surfaces made from it on a manufacturer site of industrial 3D printers.

    • @gameworkerty
      @gameworkerty ปีที่แล้ว

      what about the dimensional stability under heat part?

  • @SnorreSelmer
    @SnorreSelmer 2 ปีที่แล้ว

    3D printer tip of the year!
    As you said, a lot of printers come with a G10 print-bed with some surface on it. My TronXY X5ST came with a base G10 board, and a surface that I had to add. That surface eventually cracked due to temperature expansion and contraction, so I after watching this video I ripped off the surface and did a test-print.
    Amazing result, print let go with zero effort!

  • @ParedCheese
    @ParedCheese 2 ปีที่แล้ว

    Thanks for this!
    Bought a sheet of 0.6mm G10 to try, and it's great! It's the *only* surface I've been able to reliably print PETG on.

  • @McNibbler
    @McNibbler 2 ปีที่แล้ว +42

    This stuff is literally the only material where I could reliably get nylon to stick. The closest contender was glass, but it's still a far cry from how insanely effective this was.
    I finally don't hate nylon because of it lol

    • @Alluvian567
      @Alluvian567 2 ปีที่แล้ว

      I hated nylon mostly because even in California scrubland with no rain all year it somehow still managed to soak up moisture and pop and fizz. Adhesion was a pain as well, I was using smooth PEI on a lulzbot mini with gluestick and it was hit or miss. Ultimately I ended up throwing away half the roll as it kept getting worse and worse with moisture like issues even though I kept it sealed up and in california with no rain in it's lifetime. I should have tried baking it at some point, but never did. I am in a much wetter area now and the thought of going back to it makes my eye twitch, heh.

    • @xiaorulez
      @xiaorulez ปีที่แล้ว

      Could you do it without using a enclosure or draft shield?

    • @McNibbler
      @McNibbler ปีที่แล้ว +1

      @@xiaorulez not a chance hahaha

    • @DD-sw1dd
      @DD-sw1dd 6 หลายเดือนก่อน

      @@Alluvian567
      I live in GA. It’s always humid here.
      I’ve resorted to buying a medium size room dehumidifier, closing that room off, and running it at 100% for a day before printing Nylon. Actually have the dehumidifier’s drain tied into the A/C’s condensation water drainage line. That way it can run w/o having to empty the water.
      Power draw sucks when I run it like that…but it works. Afterward I turn the dehumidifier back to a reasonable humidity level and go on about my business.
      Since I use the same room for other things I want to avoid rusting it works out.
      Also, that particular room in my basement has no A/C returns or vents…so no humidity entering through the A/C directly to hamper the dehumidification process.
      This was my nuclear option. On the plus side…I don’t need to print from a dry box. I don’t know how low the humidity actually is in the room at 100% dehumidifier….but I do know I can feel the difference big time between that room and just outside the door.

  • @empty9360
    @empty9360 2 ปีที่แล้ว +4

    I have starting printing everything on FR4 (Fire Retardant Material that is like G10) only sanded it a bit with 200grid sandingpaper and it was such an improvement

  • @JBALLMORE
    @JBALLMORE 3 หลายเดือนก่อน

    Just installed my G10 print surface on my Ender 3D printer today and I was blow away of how good the prints stick and how easy they come off when the print bed has cooled down :D Thanks for the video and you commitment to making 3D printing accessible to the lay-man like me

  • @RubSomefastOnIt
    @RubSomefastOnIt 2 ปีที่แล้ว +2

    We used G10 for pool cues for a long time, break tips and furrels, joint collars and but caps. Also use it to make parts in machining too, bakelite and the other composits like micarta and g10 are used a ton, some of them are precursors to thermo plastics.

  • @stever1412
    @stever1412 2 ปีที่แล้ว +19

    Crazy hearing someone say "this stuff costs next to nothing" I know of G10 from high end hand made knives, and vapes. And g10 really raises the prices on those things lol

    • @MakersMuse
      @MakersMuse  2 ปีที่แล้ว +22

      Well I guess compared to speciality print bed products it's cheap heh

    • @SianaGearz
      @SianaGearz 2 ปีที่แล้ว +22

      It's an inexpensive material that eats tools for breakfast. Yes, products made from it are going to be justifiably expensive.

    • @MakersMuse
      @MakersMuse  2 ปีที่แล้ว +9

      @@SianaGearz haha very true, the speed at which it blunts carbide burrs is incredible. Even under a waterbath.

    • @Anyone700
      @Anyone700 2 ปีที่แล้ว +6

      @@SianaGearz Two methods I have seen of cutting G10 that should make it more affordable for knives: Waterjetting, and high powered fiber lasers. Id be surprised if knife makers havent started to use products like the waser or 5kw desktop fiber lasers by now. Both are in the 20-30K range to implement and I bet would save a ton in tools.

    • @MyLonewolf25
      @MyLonewolf25 2 ปีที่แล้ว +2

      The material is cheap. Machining it is expensive

  • @williamchamberlain2263
    @williamchamberlain2263 2 ปีที่แล้ว +340

    It's like G7, but three whole countries better

    • @manaspatil3996
      @manaspatil3996 2 ปีที่แล้ว +5

      Ohhmygod, XD

    • @rybread3981
      @rybread3981 2 ปีที่แล้ว +6

      I came here for relaxing print talk, and you provide shade.
      Legend.

    • @siddharthmohanty5731
      @siddharthmohanty5731 2 ปีที่แล้ว +2

      And 100x more effective

    • @dexter2811
      @dexter2811 2 ปีที่แล้ว +5

      Meh, it's half G20

    • @BobbRosborough
      @BobbRosborough 2 ปีที่แล้ว +1

      Garolite G-7 sheets tolerate higher temperatures. Up to 215 Degrees C. I was looking to see if anybody had tried G-7 for printing PETG.

  • @marvincortez6209
    @marvincortez6209 ปีที่แล้ว

    Good damn, I like you’re content, straight to the point, the pros and cons, links🤟🏻, you’re amazing

  • @vhoward1122
    @vhoward1122 2 ปีที่แล้ว

    Thanks for reminding me about this stuff. Back in 2018 I had bought 5 sheets that were 12 inches square. It cost me $5. But it was really thin. Too thin to use it by itself. But now I have a few printers that have steel flex plates. So I cut one of those sheets down to size and put some heat resistant double sided tape on it and stuck it to a flex plate and now it work perfectly.

  • @dylanmckenzie33
    @dylanmckenzie33 2 ปีที่แล้ว +3

    I have been using g10 phenolic for awhile. I sand mine down and if it gets damaged I fill in the spot with epoxy and sand it down again. My sheet is about 1 year old and still looks great!

  • @arthurmorgan8966
    @arthurmorgan8966 2 ปีที่แล้ว +5

    10:20 when having thermal runaway at extreme temps, try heating bed and hotend separately. It might be a power issue. Board is not able to cope with it.
    I encountered these on my Ender 3 v2 after modding it to all metal hotend, high temp thermistor etc. Happens only when going very hot.

  • @ComputerAnarchy
    @ComputerAnarchy 2 ปีที่แล้ว

    Sounds like the perfect material for my RV repair job!

  • @Commander_Vash
    @Commander_Vash 2 ปีที่แล้ว

    Using this since my sparkcube XXL. Love it.

  • @MakenModify
    @MakenModify 2 ปีที่แล้ว +8

    Glad you like it :D i use G10/FR4 for years now. Recently took the thin stuff and glued it to a spring steel sheet. That way you dont need clips, heats faster and is my absolute favorite surface :) great video 👍

    • @benclimo461
      @benclimo461 2 ปีที่แล้ว

      Just wondering why use this over spring steel suck as the pei bases? Most people have excellent quality from using just that.

    • @backgammonbacon
      @backgammonbacon 2 ปีที่แล้ว

      @@benclimo461 Nylon....people seem to have issues getting nylon to stick to pei. If you don't print nylon G10 looks to be a waste. The storage issues of nylon make it a pain for hobbyists so its probably the reason G10 isn't very popular.

    • @super_slo
      @super_slo 2 ปีที่แล้ว

      Is there much truth in the stories of destroying a pei sheet when printing PETG? I was afraid to try PETG as my first print on my new pei bed...

    • @WarrickTaylor
      @WarrickTaylor 2 ปีที่แล้ว

      @@super_slo I frequently print PETG on a Prusa mk2.5 with standard settings with a spring steel pei bed with no issues. I do generally preheat the bed to approx 40 degrees to remove the print tho. It was my first try at flexible that ripped a hunk out of the pei! At least I think it's pei that Prusa use.

    • @MakenModify
      @MakenModify 2 ปีที่แล้ว

      @@super_slo for powder coated beds its less of an issue I think but those with a glued on sheet tear up after a while if you don't nail the first layer height.

  • @onesadtech
    @onesadtech 2 ปีที่แล้ว +7

    G10 has been very common for years in knife manufacturing for scales and hard sheaths! Cool to see it being use in another hobby I am getting into.
    I wonder if FRN would make a decent print plate, it's extremely tough, the scales from my BM Mini Grip are insanely rigid for how thin they are when removed, always blows my mind. Not sure about heat resistance though.

  • @jimkoster5070
    @jimkoster5070 2 ปีที่แล้ว

    Thanks for the Tip! I've used G10/FR4 a lot before. But never really tough about using it as a bed material. I'll def try it.

  • @stormboy8544
    @stormboy8544 2 ปีที่แล้ว

    1 minute into the video and im already looking on ebay to buy some! Awesome video yet again mate!

  • @jonathantaylor2584
    @jonathantaylor2584 2 ปีที่แล้ว +12

    Markforged uses a g10 bed on their printers. The bed is about 10mm thick and machined flat. Just a glue stick layer is needed for their cf nylon (unheated bed). Really nice machines but the cost is out of my reach. As a proprietary system they're excellent from slicing with their online tool to printing.

    • @user-zx4vq4uk9c
      @user-zx4vq4uk9c 2 ปีที่แล้ว +1

      Wait really? We have 2 markforgeds at my robotics team, I never knew it was garolite

    • @noway8233
      @noway8233 2 ปีที่แล้ว +1

      A glass and the glue layer do the same, i use now the creality surface , but i use the glass side, its works great, its very solid "black glass",with hair spray or glue(only for abs)

    • @jonathantaylor2584
      @jonathantaylor2584 2 ปีที่แล้ว +1

      @@user-zx4vq4uk9c Next time you use it look at the bed and you can see the pattern of the woven fiberglass fabric in the surface

  • @T00LF00L
    @T00LF00L 2 ปีที่แล้ว +14

    Once you score the board with a knife bend it the other way, AWAY from the cut and it snaps in half much easier!

  • @TimoBirnschein
    @TimoBirnschein 2 ปีที่แล้ว +2

    Great video, thank you! I have experimented with etching heating coils straight to the material and print directly on the other side. Designing uniform heating elements is not easy, though, and I failed. Having said that, commercially available, cheap, heated beds are made from the same material, but they have a layer of solder mask and are not bare! That changes the adhesion properties quite a bit and might make it unusable as a direct printing surface.

  • @Crafty_Chops
    @Crafty_Chops ปีที่แล้ว +1

    After hunting high and low for G10 sheets (cut to size), I eventually got my grubby paws on some, and OMW. Angus, I am sooo glad I came across this video. I've been printing on the stock glass that came with my Ender V2. It's not been bad, but G10 is the bomb.
    After adjusting the Z-height microswitch and doing a bed level, all I can say is WOW.
    Thank you so much.

    • @MakersMuse
      @MakersMuse  ปีที่แล้ว

      Nice! I felt the same way when I first tried it haha. Glad you could track some down .

  • @Myndale
    @Myndale 2 ปีที่แล้ว +3

    One of my homemades uses a sheet of single-sided PCB that I picked up from Jaycar (copper side down of course). Works fine.

    • @dhairya8238
      @dhairya8238 2 ปีที่แล้ว +1

      That's exactly what I was looking for since regular Garolite sheets aren't available in my country. So regular single side FR4 PCB sheets work just as well?

    • @Myndale
      @Myndale 2 ปีที่แล้ว

      ​@@dhairya8238 seems to. The biggest problem with the Jaycar ones though is the size: 150x150mm. Only good for small printers. And even if they were larger, I'd be worried about warping due to their storage and display conditions, it's not really a use-case scenario that the stores are thinking about. Worked for me in a pinch, but YMMV.

    • @dhairya8238
      @dhairya8238 2 ปีที่แล้ว +1

      @@Myndale got it, I've seen plenty of 300x300 sheets selling for like $5 each in some local maker stores. I'll try one out.

  • @jonathanwood1990
    @jonathanwood1990 2 ปีที่แล้ว +4

    Hey after seeing your video, I just wanted to let you know how I get a very smooth first layer. I have been glueing transparent sheets to an old print bed using a glue stick and then I smooth it out and take out any extra glue with a card. Since I’ve been doing This every print has been almost perfect! :)

  • @BilliumRidesNC
    @BilliumRidesNC 2 ปีที่แล้ว

    I've been having a heck of a time printing on my glass bed lately. Think I'll give this G10 a shot. Thanks for the tip!

  • @OldCurmudgeon3DP
    @OldCurmudgeon3DP 2 ปีที่แล้ว +2

    Sorry to hear of your prior PETG woes. I've been using PEI on flex steel for about a year now and all I do between PLA and PETG is change the temp and add a smidge of clearance for PETG vs PLA.
    If I didn't already have a PEI sheet for my next printer, I'd get a magnet for some of this stuff and try it out.

  • @dekurvajo
    @dekurvajo 2 ปีที่แล้ว +6

    I just checked. Its very expensive here. The best cost/value surface to me is the sandblasted glasses so far. I am just making them as many i want. No adhesive need on the surface, i put water on it if i want to remove the print earlier. I like the even matte surface.

    • @vignesh_waran
      @vignesh_waran ปีที่แล้ว

      Does sandblasted glass require heatbed for printing pla and petg ?

  • @vectorfinesse
    @vectorfinesse 2 ปีที่แล้ว +6

    Brb, replacing the print surfaces for our PETG headphone parts!

  • @leetpg
    @leetpg 8 หลายเดือนก่อน

    Used this many times for knife handle spacers and for my drone frame. Great idea, sheets of it up stairs.

  • @Yakeru35
    @Yakeru35 2 ปีที่แล้ว +1

    Dude ... THANK YOU ! I was struggling so hard with my glass print bed. Results were completely random, which was frustrating since many people have great success with it. Put kapton on it, sticked well .... to well. Then I tried G10, and it works like magic ! Transformed a very frustrating experience into a really enjoyable one, made me fall in love with my printer again :D

    • @MakersMuse
      @MakersMuse  2 ปีที่แล้ว

      That's awesome to hear! I felt the same after discovering it haha