Excellent detailing..one of the best...better than many procedures...only wish you have covered infuctionsnd insulation band...
Thanks a lot for your support
Fine explanation 👍✨
Very Good and usefull information. Thanks 🙏you for such easy way to explain
Thanks for your valuable comment. Please share and subscribe my channel to get more updates.
Thankyou very much, very nice to remember
Please Like, Share and subscribe my channel to get the regular updates . My channel link...th-cam.com/users/WeldingNDTInspection
Can you give me reference standard for that soaking timw will be 2 hours where it is mentioned in asme or IBR standard ??
Sir can you doon interpass temperature of various steeel
Great n please keep posting
Thanks a lot, Please like , share and subscribe my channel to get the regular updates
Thanks for giving such useful information keep doing bro 👍
thanks a lot , please like , share and subscribe my channel to get the regular updates .
In section -ix SA335 P91 have PNo.-15E and Group no.-1
What is b9 in9015b9
B9 is used for 9%cr and 1%molybdenum, that is p no 15E.
Sir, can you please do a video on welding procedure for ASME-BPE pipe (sanitary steel pipe)
will make a video soon
In SEC IX Non Mandatory Appendix D, P No for P91 is 15E
P number P15E
Excellent detailing..one of the best...better than many procedures...only wish you have covered infuctionsnd insulation band...
Thanks a lot for your support
Fine explanation 👍✨
Very Good and usefull information. Thanks 🙏you for such easy way to explain
Thanks for your valuable comment. Please share and subscribe my channel to get more updates.
Thankyou very much, very nice to remember
Please Like, Share and subscribe my channel to get the regular updates . My channel link...
th-cam.com/users/WeldingNDTInspection
Can you give me reference standard for that soaking timw will be 2 hours where it is mentioned in asme or IBR standard ??
Sir can you doon interpass temperature of various steeel
Great n please keep posting
Thanks a lot, Please like , share and subscribe my channel to get the regular updates
Thanks for giving such useful information keep doing bro 👍
thanks a lot , please like , share and subscribe my channel to get the regular updates .
In section -ix SA335 P91 have PNo.-15E and Group no.-1
What is b9 in9015b9
B9 is used for 9%cr and 1%molybdenum, that is p no 15E.
Sir, can you please do a video on welding procedure for ASME-BPE pipe (sanitary steel pipe)
will make a video soon
In SEC IX Non Mandatory Appendix D, P No for P91 is 15E
P number P15E