@@TonyMontana-jg2gu 60 potassium perchlorate 40 aluminum, after mixing those 2 I added a bit of magnesium powder for the sparks. The strontium is sealed off in a different compartment, so it doesn't mix with the flash composition, so: 60/40 ratio KCIO4/Al. Magnesium is optional.
💥💥💥
Mooie klap, die rode vlam en dat titanium maken ‘m helemaal af, super vet gedaan 💥
Thanks man! 💯
🔥🔥🔥
woher kclo4?
@@AstralisCM Private seller
Whats the mix ratio? Can you add a pinch of titanium to the flash powder or mix with everything?
@@TonyMontana-jg2gu 60 potassium perchlorate 40 aluminum, after mixing those 2 I added a bit of magnesium powder for the sparks. The strontium is sealed off in a different compartment, so it doesn't mix with the flash composition, so: 60/40 ratio KCIO4/Al. Magnesium is optional.
Why not 70:30?
@@Xenthiums I prefer 60/40, though 70/30 isn't bad either, I just like to use 60/40 over 70/30😄