The 770 results are very disappointing. Doesn’t seem right, Bob Barney claims it’s 78% solids, yet your tests are saying 40%. I’m not saying you’re lying, or that are method is bad, just doesn’t seem right. I’ve use several high builds, including half of what’s in this test. A 770 puck has no shrinkage in the cup, fits back in like a perfect mold. I know that’s not nearly as scientific of a test, but it does give you a rough ballpark. Congrats on this new product, make it in black and white please. Look forward to trying it.
Great test!
I can see poly being done shrinking but epoxy usually shrinks for quite a bit longer, cool test!
Damn im about to use featherfill on a shaved engine bay this test is cool to see thank you for documenting this.
As long as you can sell your product at an affordable price. That’s the kicker.
The 770 results are very disappointing. Doesn’t seem right, Bob Barney claims it’s 78% solids, yet your tests are saying 40%. I’m not saying you’re lying, or that are method is bad, just doesn’t seem right. I’ve use several high builds, including half of what’s in this test. A 770 puck has no shrinkage in the cup, fits back in like a perfect mold. I know that’s not nearly as scientific of a test, but it does give you a rough ballpark. Congrats on this new product, make it in black and white please. Look forward to trying it.