Making 3D prints actually waterproof

แชร์
ฝัง
  • เผยแพร่เมื่อ 15 ก.พ. 2024
  • 3D printing from $0.3, sign up to get up to $60 coupons: jlc3dp.com/?from=CPSdrone
    And check out our DIY underwater drone course: www.cpsdrone.com/
    - Our 3D printer (FDM) FlashForge M5 Pro: www.flashforgeshop.com/produc...
    - Dichtol AM Hydro: www.diamant-polymer.de/en/sho...
    Let us know what else should we build!
    If you feel like this video has improved your life, share it with:
    - Your dad, mom, brother, uncle and your entire family (if you have one)
    - Your life partner (boyfriend / husband / girlfriend / wife)
    - Your 10 best friends
    - Your drink buddies
    - Your university / high school teacher
    - Your coworker / coworkers
    - Your boss
    - All of your employees (if you own a business)
    - Your university / high school colleges who you don’t consider friends
    - Your hairdresser
    - Your therapist
    - Your doctor / dentist
    - A random person on the street (you can use this video as a pickup line)
    - Your dog / cat / rat / fish (this will get us some extra views)
    ____________
    ♪ Sunset (Prod. by Lukrembo)
    Link: • (no copyright music) j...
  • วิทยาศาสตร์และเทคโนโลยี

ความคิดเห็น • 619

  • @CPSdrone
    @CPSdrone  2 หลายเดือนก่อน +57

    Here are all the models from the video: www.printables.com/model/768471-waterproof-3d-printing-tests-oceangate-titan
    Have fun and don't make full scale models!

    • @czaro8006
      @czaro8006 2 หลายเดือนก่อน +4

      Studenci PG na Traugutta? 🤣

    • @OneHappyCrazyPerson
      @OneHappyCrazyPerson 2 หลายเดือนก่อน +7

      Whahahaha oceangate test models 😂😂

    • @johnnyrocket3200
      @johnnyrocket3200 2 หลายเดือนก่อน

      Pro Tip: When staying in one unit, positions after the decimal point are called out one by one. So 0.25g is "zero point two five gramm" otherwise good luck with pi. ;-)
      With money, you change units. 3,75€ is three euros and seventy-five cents. That's why "three seventy-five" is ok. Same with hight.

    • @justusxavierbarboza246
      @justusxavierbarboza246 2 หลายเดือนก่อน +2

      oh no mini oceangate sub has imploded

    • @Khorde_theHusk
      @Khorde_theHusk 2 หลายเดือนก่อน +3

      why not paint the 3D print in a layer of epoxy to fill the pores?

  • @tricycleboi
    @tricycleboi 2 หลายเดือนก่อน +567

    I like how he prints the scissors gripper to prevent himself from touching the dichtol but still dips his fingers in it to use the grapper

    • @BrunodeSouzaLino
      @BrunodeSouzaLino 2 หลายเดือนก่อน +46

      Why use the appropriate gloves when you can over engineer a solution, right?

    • @BobWidlefish
      @BobWidlefish 2 หลายเดือนก่อน +44

      @@BrunodeSouzaLinoengineer a solution then not use it.

    • @roidroid
      @roidroid 2 หลายเดือนก่อน +21

      This is the first video I've seen on this channel. Is it a parody channel?
      The switch from "this stuff will kill you if you touch it" to "I'm too stupid to care" made me legit angry. There's also other weird inaccuracies in the vid that ppl who know about water pressure should know better than. If the whole video is parody then that would make sense.
      edit: it's possible the other inaccuracies were just language issues tho.

    • @tricycleboi
      @tricycleboi 2 หลายเดือนก่อน +6

      @@roidroid ok sure thing blud

    • @TwigPB
      @TwigPB 2 หลายเดือนก่อน +11

      @@roidroid Bro doesn't understand jokes

  • @Twig_ash2610
    @Twig_ash2610 2 หลายเดือนก่อน +135

    That creation in the thumbnail is absolutely *imploding*

  • @CarlinPlayz
    @CarlinPlayz 2 หลายเดือนก่อน +423

    That 3D metal sub was cool. You're probably right that it could go deeper then the real thing

    • @sirisawadcharoensuk6569
      @sirisawadcharoensuk6569 2 หลายเดือนก่อน +28

      💀💀💀💀💀

    • @CarlinPlayz
      @CarlinPlayz 2 หลายเดือนก่อน +3

      @@sirisawadcharoensuk6569 💀💀💀

    • @jeremy6384
      @jeremy6384 2 หลายเดือนก่อน +5

      Is the bottom of the ocean not deep enough?

    • @Sainsburys_Femboy
      @Sainsburys_Femboy 2 หลายเดือนก่อน +2

      @@CarlinPlayz💀

    • @CarlinPlayz
      @CarlinPlayz 2 หลายเดือนก่อน +4

      @@jeremy6384 nah. Gotta go deep. Like Europa deeper. I'm pretty sure those oceans are much deeper then earth's

  • @noen-_-7446
    @noen-_-7446 2 หลายเดือนก่อน +171

    I love all the little jokes and reverence in the video, makes the video way more fun to watch and gives a nice atmosphere.

  • @fin7152
    @fin7152 2 หลายเดือนก่อน +81

    In industry, reinforced O-rings are used to seal vacuum lines. These have a metal ring on the vacuum side that prevents the seal from slipping.

    • @fin7152
      @fin7152 2 หลายเดือนก่อน +8

      google centering ring ISO-K to see it

  • @sydnerd
    @sydnerd 2 หลายเดือนก่อน +33

    Props to JLCPCB/3DP for supporting this channel, shame others wouldn't because you folks are doing an amazing educational and inspirational job combined with top tier engineering.

  • @Arek_R.
    @Arek_R. 2 หลายเดือนก่อน +51

    Doing second process with the dichtol stuff probably will seal it even more.
    Btw. another technique to seal a FDM 3DP is by printing it in ABS and then doing acetone smoothing, it dissolves surface of the part and once dried creates solid layer all around.

  • @saturated2350
    @saturated2350 2 หลายเดือนก่อน +48

    Would be quite interesting if someone made a full scale model for testing!

    • @draco5991rep
      @draco5991rep 2 หลายเดือนก่อน +27

      I would use carbonfibre for the hull, since it is pretty stronk. Also it doesen't like to deform 🤡

    • @happninmojo
      @happninmojo 2 หลายเดือนก่อน +15

      I can take millionaires for rides in it!

    • @happninmojo
      @happninmojo 2 หลายเดือนก่อน +20

      It's pretty expensive, I'll save money by using an xbox controller to pilot it.

    • @draco5991rep
      @draco5991rep 2 หลายเดือนก่อน +13

      @@happninmojo genius idea, we should start a company but what should we call it 🤔

    • @paulrippcord506
      @paulrippcord506 2 หลายเดือนก่อน +15

      @@draco5991rep The name should reflect that we are a gateway to the ocean, any ideas?

  • @maximthemagnificent
    @maximthemagnificent 2 หลายเดือนก่อน +27

    Love your sense of humor.

  • @AronFigaro
    @AronFigaro 2 หลายเดือนก่อน +7

    Cheers from the openROV team. We actually thermally annealed our PLA to waterproof ours back in 2014, and this worked quite well by boiling them in hot water just to the point of deforming and then letting them cool. If you get the temp correctly it will work, though less well for solid fill.

  • @KiritaChan
    @KiritaChan 2 หลายเดือนก่อน +3

    You could of use resin printers because it just prints each layer in a second because it uses uv lights to solified it

  • @segment932
    @segment932 2 หลายเดือนก่อน +14

    To both prevent water damage your electronics and make the sub survive a deeper dive you could submerge the electronics in baby oil.
    Then the submarine drone don't have any air in it, thus can not break from over pressure.

    • @UncleKennysPlace
      @UncleKennysPlace 2 หลายเดือนก่อน +5

      Or ordinary mineral oil, to avoid that smell reminding you of changing time and diaper rash.

    • @bastienx8
      @bastienx8 2 หลายเดือนก่อน +4

      It's the same thing used in some dive watch, it prevent them to collapse, and since oil dont mix well with water it also prevent small water drops to enter.

    • @johns_craft8582
      @johns_craft8582 2 หลายเดือนก่อน +1

      Also get a better receiver so the controller dosent disconnect

    • @Duolingo.524
      @Duolingo.524 2 หลายเดือนก่อน

      The sub I think comes with a Xbox

  • @Max-mb2el
    @Max-mb2el 2 หลายเดือนก่อน +59

    “i think it will collapse”

    • @Jrynx
      @Jrynx 2 หลายเดือนก่อน +1

      E

    • @Marder_IFV
      @Marder_IFV หลายเดือนก่อน +1

      A

    • @FrankIsHere794
      @FrankIsHere794 16 วันที่ผ่านมา

      Sports it's in the game

  • @glenndhooge6787
    @glenndhooge6787 2 หลายเดือนก่อน +3

    it's awsome to see you guys continously working to improve your underwater drones

  • @LeeRox91
    @LeeRox91 2 หลายเดือนก่อน +5

    You could use a "clear transparent" setting for getting a really solid print which reduces gaps in between layer walls

  • @bodach2921
    @bodach2921 2 หลายเดือนก่อน +3

    You can put the print in dichtol and put it in a vacuum chamber. This allows air to escape from the pores and at normal pressure the dichtol diffuses into the pores.

  • @DrTheRich
    @DrTheRich 2 หลายเดือนก่อน +4

    For the O ring, you need to design the seating of the seal in such a way that the pressure of the water tightens the seal. then the higher the pressure, they better the seal.

  • @Travis141123
    @Travis141123 2 หลายเดือนก่อน +3

    I used to repair cracked/seeping plastic fuel tanks by pulling a vacuum on it, then applying epoxy. The same could be done with your printed vessel and the dichtol. Also pressure regulating the hull is a good idea.

  • @user-sf3pd8yk6x
    @user-sf3pd8yk6x 2 หลายเดือนก่อน +2

    Finally waiting for you to release a new video. I'm so excited.

  • @waterstudio5571
    @waterstudio5571 2 หลายเดือนก่อน +1

    I have some reasons for love your videos:
    1. Good video editing
    2. Stilling voice
    3. Gripping content

  • @AnotherOtherMan-alive
    @AnotherOtherMan-alive 2 หลายเดือนก่อน +3

    When using a gasket or o-ring, you need to design around it with a groove for it and having multiple sealing layers. You want to maximise the path the water takes to get in from a deliberate opening.

  • @atranas6018
    @atranas6018 2 หลายเดือนก่อน +1

    I just painted the FDM prints with thick paint & brush when I need it to be water/gas-proof. Works every time.

  • @I.no.ah.guy57
    @I.no.ah.guy57 หลายเดือนก่อน

    I love your videos guys, and the scientific process you guys have and the documentation as well! Keep it up!

  • @magdalenao4229
    @magdalenao4229 2 หลายเดือนก่อน +32

    Panowie wysoki poziom. Fantastycznie opowiadacie o swojej pracy. Czapki z głów. Powodzenia

    • @decoy741
      @decoy741 2 หลายเดือนก่อน +1

      A najważniejsze jest to że on jest Polakiem najprawdopodobniej

    • @beatrizmf9965
      @beatrizmf9965 23 วันที่ผ่านมา

      He is polish

    • @armanayuban9225
      @armanayuban9225 5 วันที่ผ่านมา

      @@beatrizmf9965 okay

  • @user-yc8hn7ki3b
    @user-yc8hn7ki3b 2 หลายเดือนก่อน +1

    Everyone has been made for some particular work, and the desire for that work has been put in every heart.

  • @Robinlarsson83
    @Robinlarsson83 2 หลายเดือนก่อน +6

    One note about o-rings and other rubber seals, the one you used looked more like a EPDM "string" rather than an o-ring.
    Way better to design around an off the shelf available o-ring (proper one in fairly hard NBR or similar rubber) than trying to glue something together.
    Glueing seals with CA glue or really any glue that is harder than the rubber will be a problem, it creates a hard point that almost always leaks.
    The usual way of doing it is to have nice cuts that mates well and make the seal a bit to long, so the ends gets compressed into each other. No glue :)
    Or getting some way to vulcanise the rubber together, but yeah :P

    • @Trust_me_I_am_an_Engineer
      @Trust_me_I_am_an_Engineer 2 หลายเดือนก่อน +2

      "creates a hard point that almost always leaks" sounds right, but is completely wrong. I've worked at Engineered Pressure Systems ( EPSI) at Sint Niklaas for seven years and we ALWAYS glue the large O rings (Nitrile cord) with a standard cyanocrylate glue, because noone makes standard O rings with a 800-1000 mm diameter at an acceptable price and delivery time. Perpendicular cut with a sharp knife . These O rings will easily seal high pressure vessels up to 9000 bar (900Mpa). BUT you need a very proper fitting groove and the exact amount of compression for a proper seal. I don't think he used an EPDM cord, but a nitrile one. Of course you're absolutely right about designing around an off the shelf standard is always better . In this case I 'm pretty sure the leak comes from the fact that his O ring is rather thick and not properly pressured ( seriously only 4 little screws holding the lid down ?? )

  • @hazimreitz
    @hazimreitz 2 หลายเดือนก่อน +3

    The design is very human

  • @bendixflight7310
    @bendixflight7310 2 หลายเดือนก่อน +2

    0:55 better performance than the real thing

  • @ishanmelwani6924
    @ishanmelwani6924 2 หลายเดือนก่อน +3

    Awesome!! Super interested about your DIY Pressure chamber, do you have any vids/posts talking about how you made it?

  • @jedert9774
    @jedert9774 2 หลายเดือนก่อน +5

    That submarine design is amazing I bet it would make it to the Titanic

    • @imtube333
      @imtube333 2 หลายเดือนก่อน

      hahahahahaha

    • @eliel0503
      @eliel0503 2 หลายเดือนก่อน

      ermmm actually, the Titan did actually made it to Titanic multiple times 🤓

  • @user-tp7bh2yw4k
    @user-tp7bh2yw4k 2 หลายเดือนก่อน +1

    She felt that chill that makes the hairs on the back of your neck when he walked into the room.

  • @Monki48
    @Monki48 หลายเดือนก่อน +1

    Bro is so good at 3d printing that his ocean gate didt crumble

  • @lionnelmurimi651
    @lionnelmurimi651 2 หลายเดือนก่อน

    Loving the content, shall be binging and looking out for more.

  • @user-gx5hp5kg1v
    @user-gx5hp5kg1v 2 หลายเดือนก่อน +1

    Behind the window was a reflection that only instilled fear.

  • @EKUL34
    @EKUL34 2 หลายเดือนก่อน

    I needed to make prints air tight under significant pressure, I found a few layers of spay clear coat automotive paint works well.

  • @surmur
    @surmur 2 หลายเดือนก่อน

    The vase printing method made pretty waterproof walls even it was only 1 wall thick. It leaked a bit, few droplets on walls if left for hours but it stopped leaking

  • @KaliKavala
    @KaliKavala 2 หลายเดือนก่อน

    Guys, there is a Prusa wiki article for the infill types in 3d printing. THere are a few that are extremely well for filling up the infill part with something.
    This way you can print your model and fill up the "infill" space with 2 part resign. After curing it should be pretty much waterproof inner skin of your model.

  • @JumpeFurby
    @JumpeFurby 2 หลายเดือนก่อน +5

    Funfact: opensls brings sls printing to the hobby space for 2000-2500 euro. Print metal at home with lasers!

  • @-SEB-835-
    @-SEB-835- 2 หลายเดือนก่อน

    Hi, Thanks for the video and all the good work.
    It might be a stupid question but what about remelting the print in salt, or/and intrelocking the print layers like shown by the CNC kitchen ?
    Thanks in advance

  • @raphaelboll6096
    @raphaelboll6096 2 หลายเดือนก่อน +3

    With the Oring test i think it might be better to either use more screws or maybe even print the entire cap with a built in thread, since it only needs to tighten enough to press on the o ring consistently.
    You can look at watch caseback designs here. The caseback has a thread and screws onto the case, making enough pressure on the (sometimes multiple) O-rings to withstand immense depths. Most common dive watches are certified to 200m but it is not uncommon for them to go to 600m. Some of them like the omega Ploprof or the rolex deepsea can go far deeper than that (some have been taken to the mariana trench on the outside of a submarine)

    • @bastienx8
      @bastienx8 2 หลายเดือนก่อน +1

      These dive watch are often filled with oil to prevent them to collapse, and since oil dont mix well with water it also prevent small water drops to enter.

  • @tomcarroll6744
    @tomcarroll6744 2 หลายเดือนก่อน

    Impressive work. I've been around a long time and you guys are OK. Keep going.

  • @SimonFiliatrault
    @SimonFiliatrault 6 วันที่ผ่านมา

    Super excited to try this product, but cannot find a way to get it in Canada!

  • @DanielLopez-up6os
    @DanielLopez-up6os 2 หลายเดือนก่อน +4

    Tbh the Way you do the Drones with the watertight pressure resistant tube inside the shells, is how actual submarines work. Like for ex the Russian typhoon, is an outer aerodynamic hull and stealth hull. And the there's 3 or 4 pressure tubes inside, and ut doesn't that wat natter if some water gets trough the first layer

  • @MrKiar1611
    @MrKiar1611 2 หลายเดือนก่อน

    from my pov, only abs-like and the Siraya Tech BLU (the one in video) are kind of usable for mechanical purpose while stay with relatively cheap price.
    Otherwise, I would have gone for esun PA100 nylon/esun hard tough/Phrozen Onyx series for something as critical like this.
    Also, those UV resin perform differently over time even without sunlight shining on it. I usually let it dry for a few days instead of using UV cure station. anti UV clear paint is another trick to stop its curing over time. Although UV light can cure the resin, it is still polymer which can be break down by UV light. So when curing as thin as 0.8mm/1mm, you can easily over cure some part of it and causing small cracks(since the UV light isn't spread evenly on your print), hence, brittleness.

  • @notfunnirobloxyt9494
    @notfunnirobloxyt9494 8 วันที่ผ่านมา +1

    I love the subnnatica reference!

  • @KeozFPV
    @KeozFPV 2 หลายเดือนก่อน

    Ok, now i need to buy this dichtel for my outside encloses!

  • @oljobo
    @oljobo 2 หลายเดือนก่อน

    My first idea was using lightweight PLA (with deliberate foaming), and then dip it into - or paint it with epoxy, which will be absorbed into the print, making it very solid and also waterproof.

  • @paulrossjones2234
    @paulrossjones2234 หลายเดือนก่อน +1

    hi, great video. What filament are you printing with? cheers Paul

  • @Leo_Aqua
    @Leo_Aqua 2 หลายเดือนก่อน

    have you tried printing a part with fdm then coating it with resin and curing it? This would fill up the gaps pretty well. I haven't tried it but it could work

  • @allenplaysal
    @allenplaysal 8 วันที่ผ่านมา

    What flashforge printer do you use? My school uses the adventurer 4

  • @avigetsbored
    @avigetsbored หลายเดือนก่อน

    i wonder what the performance of a nontoxic conformal coatings or nail polish would be on water proofing it, i've used both to effectively weatherproof pcbs and it could be a less toxic alternative to the dichtol stuff

  • @pooppyybuhhole
    @pooppyybuhhole 2 หลายเดือนก่อน

    any details available on that water pressure chamber? is that a DIY or bought? would love to get one myself to run additional tests!

  • @dustin7970
    @dustin7970 2 หลายเดือนก่อน +1

    What if you put the dichtol in the pressure chamber with the printer? That way im guessing you force it into even more cracks

  • @thear1s
    @thear1s 2 หลายเดือนก่อน

    Just curious, did you try soaking the FDM prints in resin to see if you could get the same results as with the dichtol? I've got a fair experience with SLA printing and I'm not surprised that you got bad results, resin doesn't have the same strength as FDM and opening two holes kinda miss the point of making a singlepiece submarine.

  • @gameeverydaygamer3527
    @gameeverydaygamer3527 2 หลายเดือนก่อน +1

    these are the only ones that you should use a logitech controler for

  • @GamerLudwig
    @GamerLudwig 2 หลายเดือนก่อน

    I assume the rubber oring shrinks faster under pressure than the submarine
    Pressure from the outside may have a different effect than pressure from the inside afterall

  • @TriremeBoy
    @TriremeBoy หลายเดือนก่อน

    This is probably the best Dichstol advertisment

  • @timothytilley5594
    @timothytilley5594 2 หลายเดือนก่อน

    Did the Dictol (or whatever you call it) increase the strength of the part, as well as water proof it? Did you test that? I’m excited to try that.

  • @flyingkiwi14
    @flyingkiwi14 2 หลายเดือนก่อน

    Have you tried acetone smoothing the inside of ABS printed parts?

  • @tejap8882
    @tejap8882 หลายเดือนก่อน

    can u make a video on how you made the pressure chamber

  • @benjaminandersen1097
    @benjaminandersen1097 2 หลายเดือนก่อน

    very cool, glad i found your channel!

  • @porek965
    @porek965 2 หลายเดือนก่อน +1

    "Actually i think this hull might be pretty pressure resistant." Leaked footage from certain ocean exploring company

  • @jakrabitmn
    @jakrabitmn 2 หลายเดือนก่อน

    have you tried annealing your 3d prints? I've had decent luck with annealing in sand (to mitigate warping/shrinking) at 100C°

  • @MrTryice
    @MrTryice 2 หลายเดือนก่อน +1

    Incredible video !

  • @dalivanwyngarden3204
    @dalivanwyngarden3204 2 หลายเดือนก่อน

    If the pressure doesn‘t matter thaaat much you can just dip the printed parts in some resin or even coat it from the inside as well.

  • @G.S.W.
    @G.S.W. 2 หลายเดือนก่อน

    At what point will you mount that underwater 3d printer to your ROV?

  • @Roobotics
    @Roobotics 2 หลายเดือนก่อน

    Are any of the powder-sintered ones actually hollow though? Technically they should be full of unsintered powder with how those machines work, each sub would be sinking down into the powder bed and having powder pushed into it per-layer, then sealed up while still like that..

  • @chriszuhlke8380
    @chriszuhlke8380 2 หลายเดือนก่อน

    Do you think a vertical print with a fdm printer would be stronger than a horizontal one?

  • @xscitobor1233
    @xscitobor1233 2 หลายเดือนก่อน

    What slicer do you guys sue with your flash forge? I can't imagine getting waterproof prints let alone consistently on my ff Creator Pro

  • @chickennugget3883
    @chickennugget3883 2 หลายเดือนก่อน

    What type of printer did you use to print the subs?

  • @doctorgregg6847
    @doctorgregg6847 2 หลายเดือนก่อน

    Did dichtol Made the prints more resistant with dry tests? Should do a test.

  • @raffaelwoller3630
    @raffaelwoller3630 2 หลายเดือนก่อน

    Would a coat of resin or epoxy also work for making a print waterproof?

  • @OAikoT
    @OAikoT 2 หลายเดือนก่อน

    How did you install the O-rings? This is the crucial part. Remember its about which way they are squished that makes them work properly.

  • @damianbrew5056
    @damianbrew5056 2 หลายเดือนก่อน

    Super materiał. Przyjemnie się ogląda, tak 3mać:)
    Jako że pracuje w różnych technologiach druku 3d to podpowiem:
    MJF, SLS i SLM to technologie druku w proszku i nie da się drukować w nich zamkniętych pustych przestrzeni jeśli nie zrobi się otworu na wysypianie nieutwardzonego/s topionego proszku. Więc jeśli rozetniecie te wydruki to albo wysypie się z nich proszek albo technik w firmie zauważył ten problem i poprawił modele że są pewne w środku bez powietrza i bez luźnego proszku. Powodzenia w kolejnych eksperymentach!

  • @mishtrong
    @mishtrong 2 หลายเดือนก่อน +2

    Me with an SLA printer: I am waterproof!

  • @tomwagemans1872
    @tomwagemans1872 2 หลายเดือนก่อน +1

    Did you try phapor smoothing?

  • @MRSPORTYTRUCKER
    @MRSPORTYTRUCKER 2 หลายเดือนก่อน +3

    Why dont you just put expoxy on the outside of the print then use sealant on the joints
    Or coating FDM prints with printer resin

  • @user-wj7dw9co7y
    @user-wj7dw9co7y 2 หลายเดือนก่อน

    I think there's one more thing you could try. For example, placing a thin model of a bathyscaphe inside would create areas of artificial overextrusion in the shell, possibly making it less porous overall.

  • @UntitledBeanie195
    @UntitledBeanie195 2 หลายเดือนก่อน

    THE PHOTO AFTER HE SAID ITS LOOKS PRETTY STRONG OMGGGG

  • @MrDeepwoodtickles
    @MrDeepwoodtickles 2 หลายเดือนก่อน

    For depthproofing the electronics capsule why not fill it with insulating oil so it has internal hydrostatic pressure to resist water ingress?

  • @Swiss_Person
    @Swiss_Person 2 หลายเดือนก่อน +1

    I too love nylon but I alos love this video
    Really really Awesome!
    Keep it up :D

  • @Ironarmgaming1
    @Ironarmgaming1 2 หลายเดือนก่อน +1

    0:32 I’m pretty sure your hull is more resistant than the real ocean gate one was

  • @user-pp5nf7bz8o
    @user-pp5nf7bz8o 2 หลายเดือนก่อน +1

    People take different roads seeking fulfilment and happiness. Just because theyre not on your road doesn't mean they've gotten lost.

  • @maximthemagnificent
    @maximthemagnificent 2 หลายเดือนก่อน +1

    Not that it matters, but if anyone's interested an abbreviation formed by first letters in a phrase that makes a pronounceable word is an acronym (e.g. RADAR), if it's not it's called an initialism (e.g. FYI).

  • @zdog90210
    @zdog90210 2 หลายเดือนก่อน

    I'm not sure if they have it in your country but for my 3D printed RC boats and submarines I use flex seal spray the clear kind it's like a rubberized spray

  • @julianpalmer4674
    @julianpalmer4674 2 หลายเดือนก่อน +1

    Rather than trying to make the electronics container conpletely water proof, have you considered using a high pressure gas supply (CO2) cartridge for example with a regulator to pressurise the inside of the container to maintain an acceptable pressure differential between the inside and outside? Using an automatic vent valve to perge the pressure as you then come back up. Your depth limit then is really the pressure of the gas in your pressuising 'air supply'. Look at how a diver in a dry suit stops getting pinched by his suit as he goes deeper, as well as controlling his bouyancy. Just a suggestion.

  • @KrazyNomadQc
    @KrazyNomadQc 2 หลายเดือนก่อน

    What 3d design software are you using?

  • @alskar0952
    @alskar0952 2 หลายเดือนก่อน

    What if you flood the inside where the coponits are with menrile oil than pressureris it

  • @khimbittle7705
    @khimbittle7705 2 หลายเดือนก่อน

    What type of filament were you using?

  • @bimodesign1815
    @bimodesign1815 2 หลายเดือนก่อน +1

    What if metal plating the submarine, I don't think iron man drinks water.😂

  • @benashbaugh5982
    @benashbaugh5982 2 หลายเดือนก่อน

    Why don't you spray the surface with something like the Flexseal? It's a rubber seal that work well enough.

  • @matthewsnyder4211
    @matthewsnyder4211 2 หลายเดือนก่อน

    If you use PLA try Methyl Acetate to waterproof. I've left a 2mm thick at 500psi for 30 minutes and there was no observable leakage

  • @user-dk3ih5ok6k
    @user-dk3ih5ok6k 2 หลายเดือนก่อน

    What about putting dictol in pressure chamber ,drop hulls in ,pressurize for a hour then dry and test???????

  • @ansiaaa
    @ansiaaa 2 หลายเดือนก่อน

    I might be missing something but couldn't you prime the model and use dielectric grease on the electronics?

  • @Denis_Stein
    @Denis_Stein 2 หลายเดือนก่อน

    What type of plastic did you use for FDM printing? This is a fundamentally important issue, since of all plastics, only PETG provides the best adhesion between layers.

  • @Chitose_
    @Chitose_ 2 หลายเดือนก่อน

    *HELL NAW THE THUMBNAIL*

  • @AlexvrbX
    @AlexvrbX 19 วันที่ผ่านมา

    if you're going to use an o-ring, use an actual o-ring and not a glued one... and make round indentations on both surfaces, tight fit (if you have to force the rubber in ever so slightly that's not necessarily a bad thing) that was the o-ring has more surface area to seal against and it's unable to shift around. A flat seal might be even better, but only if you can apply LOTS of pressure spread evenly across the entire perimeter. Speaking of which... more bolts = less (or more even) distortion = more sealing power.

  • @nkronert
    @nkronert 2 หลายเดือนก่อน +1

    Adding some bags of desiccant on the inside should resolve the moisture issue 😉

  • @matthewspurling-tf8kl
    @matthewspurling-tf8kl 2 หลายเดือนก่อน

    nah, the titan sub was crazy