Sir apka bahut bahut dhanyawad jo practical and actual field me use hone bala video dalte hain. But I think here A=R*T+2(T-F)^2*Tan@/2 hoga. Where @ =angle thita
Thank you very much for sharing this info. We found right info at right time. Very useful. We are searching a video for Argon consumption calculation in GMAW.
Sir please ek video bna de kaise report bnante hai field experience.. Excel sheet me Mujhe report bnani nhi aati hai .. Qc reports in excel sheel., fitup report, ndt inspection report. Welder test report, aur procedure.. Jb inspection check krwana hai.. .
Agar ap ispe ek video bna de to .excel sheet use krke please.. Bhut help ho jayegi apki sari video follow krta hu mai.. Maine NDT level 2 kiya hua hai
sir, this video mention the electrode consumption calculation for butt weld in plate but how to calculate for pipe butt weld (because, for length(L) we have to calculate circumference, what will be the radius, because OD and ID will be different), plz reply.
Sigle V and double V butt joint ka welding angle and thickness ka kya formula hai is par aap ek video banaya to apka bahut aabhari honge hum dhanyavaad 🙏🙏🙏🙏🙏🙏
Can you make a video on manpower estimation for piping spool fabrication work productivity in terms of inch dia and piping spool erection work in terms of inch metres
Dear Sir, For 18" Pipe required 10Kg max value to weld i check with formula it comes maximum 1Kg of electrode. Pipe Dia 18" Thickness 10mm R= 2 F= 3 Angle 60 Degree A= 0.48 cm2 Length = Pi x Dia 3.1416 x 18" x 25.4 = 1436mm =143 cm W= (0.48x 7.85x 143 )/0.55 W= 979 gm Reinforcement 20% Total Wt = 1.1 Kg and practically 10 Kg Can you explain Plz
You have taken the reinforcement factor , but what about the penetration factor ( because this will vary based on the parameters or gases used ) ? Plz support ..
How can we say that 20% consumption for reinforcement can you give me any reference or approximate calculations ??? 2. When you calculate for fillet weld please correlate with throat thickness for better understanding including it’s reinforcement also ????
With due respect, when I am calculating for route and hotpass of an 12" pipe ( thinkness taken for route and hotpass is 4.6) , the results comes out as around 3 filler wire. When in practical it is taking 6 filler wire. What must be the problem?
sir, this video mention the electrode consumption calculation for butt weld in plate but how to calculate for pipe butt weld (because, for length(L) we have to calculate circumference, what will be the radius, because OD and ID will be different), plz reply.
Sir apka bahut bahut dhanyawad jo practical and actual field me use hone bala video dalte hain.
But I think here A=R*T+2(T-F)^2*Tan@/2 hoga. Where @ =angle thita
correct for both it has to be multiplied into 2
Sir hindi me vedio banane ke liye thanks🙏🙇
Thank you sir..... For making such a video....
Thank you. Please join my channel to support my initiative. Joining link: th-cam.com/channels/H7nXSievFlbRKzKzEySbkw.htmljoin
Nice knowledge, thanks sir! And I hope to be worked together.
Thnaks again sir!
Very use information sir ... Thank you sir
Thank you. Please visit my website www.weldingandndt.com/
so thanks. dear very use full information. once again so thanks
Thank you. Please join my channel. Joining Link: th-cam.com/channels/H7nXSievFlbRKzKzEySbkw.htmljoin
Very much informative brooo...👍👍👍
Bahut badhia
Aise hi sir aap bhale hi english me likhe pr bola kriye hindi language me hi esse kafi logo ko faayda hoga.... Thank you
Great explanation my friend, all new estimators can learn from basics. Thanks a lot
Thank you. Please visit my website www.weldingandndt.com/
Osom video... Best one
Thank you. Please visit my website www.weldingandndt.com
Please make a video pipe consumable arc welding
Thank you very much for sharing this info. We found right info at right time. Very useful. We are searching a video for Argon consumption calculation in GMAW.
Thank you. If you want to financially support me, Please join my channel. Joining Link: th-cam.com/channels/H7nXSievFlbRKzKzEySbkw.htmljoin
Welding current requirements please upload
Many thanks saheb
Thank you. Please join my channel to support my initiative. Joining Link: th-cam.com/channels/H7nXSievFlbRKzKzEySbkw.htmljoin
No doubt your the best.
Thank you. Please visit my website for notes, videos and other important informations www.weldingandndt.com/
Great explanation, could you please explain the double bevel and fillet joint.
Thank you.sir.ur video always help full for us. How can I calculated for pipe
Nicely eleborated
Thank you. Please join my channel to support my initiative. Joining link:
th-cam.com/channels/H7nXSievFlbRKzKzEySbkw.htmljoin
Sir piping ko kaise calculate krte h plz .
Dear sir if I am welding or filling the material in hole that is to seal the hole at that time what LL you consider welding length ...pls reply
Thank you sir for your information and time.
Thanks a lot. Please visit my website www.weldingandndt.com/
plz explan fir fillet welding
Sir please ek video bna de kaise report bnante hai field experience.. Excel sheet me
Mujhe report bnani nhi aati hai .. Qc reports in excel sheel., fitup report, ndt inspection report. Welder test report, aur procedure.. Jb inspection check krwana hai.. .
Agar ap ispe ek video bna de to .excel sheet use krke please..
Bhut help ho jayegi apki sari video follow krta hu mai.. Maine NDT level 2 kiya hua hai
Zaberdust sir.
Thanks a lot. Please visit my website www.weldingandndt.com/
Nicely explained 👍🏻😊
Thank you. Please visit my website www.weldingandndt.com/
Superb video
Awesome sir
Thanks a lot. Please visit my website www.weldingandndt.com/
Sir, please make video on consumption of electrode or filler for excess root penetration it is main part in it if we talk about calculation.
Thank you. Please visit my website www.weldingandndt.com/
Sir plz video upload for mention pipe.
Great sir
Thank you. Please join my channel to watch all the videos. Joining link: th-cam.com/channels/H7nXSievFlbRKzKzEySbkw.htmljoin
J group joint Ka bhi video banaya ha kya?
Also thanks for the videos , you are doing a good job -
Kindky update: the density being used in the formula is of base metal or filler electrode ?
Filler. Mostly the filler and base are same material. Thank you. Please visit my website www.weldingandndt.com/
@@WeldingandNDT l
Thank a lot
Thank you. Please join my channel to watch all the videos. Joining link: th-cam.com/channels/H7nXSievFlbRKzKzEySbkw.htmljoin
Sir thoda bataie ki density kiska dalna hey formula mein base metal ki filler metal ?? Please sir batao
Appreciate
Thank you. Please visit my website www.weldingandndt.com/
Tube to tube welding joint me kitna lgega sir
How to choice Industrial welding machine .. PLZ sir ik video bnaye welding machine..pr
sir, this video mention the electrode consumption calculation for butt weld in plate but how to calculate for pipe butt weld (because, for length(L) we have to calculate circumference, what will be the radius, because OD and ID will be different), plz reply.
OD. Thank you. Please visit my website for notes, videos and other important informations www.weldingandndt.com/
Backchip welding Ka kaise hoga
Please It is beneficial to say a little if there are words in the code book.
Wating for your reply.
Can u pls tell in English it's useful to all
What about ESW and EWG.
Deposition rate. In case of autogenous welding how to consider deposition rate.
It was a good session.
Thank you. Please visit my website www.weldingandndt.com/
Sigle V and double V butt joint ka welding angle and thickness ka kya formula hai is par aap ek video banaya to apka bahut aabhari honge hum dhanyavaad 🙏🙏🙏🙏🙏🙏
Sir kindly share with me.... tolerance of undercut different plate.....
Pipe circumstances How to calculate
yes that was not cleared ..confused through ID or OD..
Thanks
Thank you. Please join my channel to watch all the videos. Joining Link: th-cam.com/channels/H7nXSievFlbRKzKzEySbkw.htmljoin
Can you make a video on manpower estimation for piping spool fabrication work productivity in terms of inch dia and piping spool erection work in terms of inch metres
Very good
Thank you. Please join my channel to support my initiative. Joining Link:th-cam.com/channels/H7nXSievFlbRKzKzEySbkw.htmljoin
Sir,
6010 aur 7010 alag alag kaise nikalenge?
very nyc
Thank you. Please visit my website for notes, videos and other important informations www.weldingandndt.com/
Sir .
how to calculate lenght of weld of different dia Pipe in single v butt joint ?
Thnx sir
Thank you. Please join my channel. Joining Link: th-cam.com/channels/H7nXSievFlbRKzKzEySbkw.htmljoin
Hello, could you plese explain how to calculate activity based welding cost
good
Thank you. Please visit my website for notes, videos and other important informations www.weldingandndt.com/
Nice sir
What about gtaw +smaw process include
Sir ji
I want to know the consumption of Gad during MIG welding
Why efficiency in. MIG welding is much higher then SMAW (electrode welding)? Is it due to flux weight or something else?
How do calculate deposition efficiency?
It is done practically in the lab. Thank you. Please visit my website www.weldingandndt.com/
Sir how to calculate gas consumption
Gas consumption during mig welding
20 Percentage of 680 is 136
एक फुल आर्गन सिलिंडर में कितना रनिंग मीटर वेल्डिंग होता है?
Ye formula kis book ya code me mention hai har koi different batata hai
Sir , from where I can do level 2 online course?
For level II Please contact Mr. Baldeo Patel: 9638053503
would you mine if let me tell you onething 100mm=10 cm
48.273mm=4.8cm is it ok sir
I am getting confused here while calculation
Sir, why did you devide by 100 to convert mm to cm it will be 10..am I correct?
It's mm^2 that's why
Dear Sir,
For 18" Pipe required 10Kg max value to weld i check with formula it comes maximum 1Kg of electrode.
Pipe Dia 18"
Thickness 10mm
R= 2
F= 3
Angle 60 Degree
A= 0.48 cm2
Length =
Pi x Dia
3.1416 x 18" x 25.4
= 1436mm
=143 cm
W= (0.48x 7.85x 143 )/0.55
W= 979 gm
Reinforcement 20%
Total Wt = 1.1 Kg and practically 10 Kg
Can you explain Plz
Tig me non consumable electrode use hota h master
You have taken the reinforcement factor , but what about the penetration factor ( because this will vary based on the parameters or gases used ) ? Plz support ..
Nice
Niceeee
Open table is quicker
How can we say that 20% consumption for reinforcement can you give me any reference or approximate calculations ???
2. When you calculate for fillet weld please correlate with throat thickness for better understanding including it’s reinforcement also ????
Why should we use inert gas while doing welding ????
Inert gases are non reactive that's y we used
Sir pls mujhe best book btaiye welding ke liye jo AWS Ko follow kare plz tell me , I am fabrication engineer
F value how
English please
th-cam.com/video/uKRHRR89eZs/w-d-xo.html
With due respect, when I am calculating for route and hotpass of an 12" pipe ( thinkness taken for route and hotpass is 4.6) , the results comes out as around 3 filler wire. When in practical it is taking 6 filler wire. What must be the problem?
Why r x t, perhaps it should be r x f
Whats F
sir, this video mention the electrode consumption calculation for butt weld in plate but how to calculate for pipe butt weld (because, for length(L) we have to calculate circumference, what will be the radius, because OD and ID will be different), plz reply.
L= 2pie r
Thanks so much for video.
Very nice sir