  • Taken from "How To Make A Clock In The Home Machine Shop - Part 9 - Etching, Waxing And Silvering A Chapter Ring" • Clockmaking - How To M...
    You can also help me make these videos by purchasing via the following Amazon Affiliate links:
    Cameras:
    Panasonic GH5 - amzn.to/2rEzhh2
    Panasonic X920 - amzn.to/2wzxxdT
    Books:
    "Solidworks 2013 Bible": amzn.to/2FObS1D
    "Machinery's handbook": amzn.to/2pi7XE5
    "Lathework: A Complete Course (Workshop Practice Series)" - amzn.to/3Zt1DJM
    "Drills, Taps and Dies", Tubal Cain: amzn.to/4c0e5H0
    "Hardening, Tempering & Heat Treatment", Tubal Cain: amzn.to/2IdTQLw
    Tools & Shop Products:
    Sherline Lathe: amzn.to/2pnXM19
    Sherline WW collets: amzn.to/2FYZ7F8
    Optivisor Headband Magnifier: amzn.to/2HFg1FU
    Norton 1-by-2-by-8-Inch Fine/Coarse India Combination Oilstone, Red: amzn.to/2tTEPb0
    Digital Caliper 6 inch/150 mm Electronic Vernier Calipers: amzn.to/48Ofcac
    Interapid Dial Test Indicator: amzn.to/2FPInwH
    Saint Gobain (Norton) - 4 Arkansas Stones + case: amzn.to/2HCOAMX
    Dormer A190202 Jobber Drill Set, 1.0 mm - 6.0 mm x 0.1 mm Size: amzn.to/2DR5fdb
    Dormer A190203 Jobber Drill Set, 6.0 mm - 10.0 mm x 0.1 mm Size: amzn.to/2ITfeTa
    Heavy Duty Arbor Press: - amzn.to/46HdTZV
    Geevorks Spotting Drill Bit, M42 HSS High Speed Steel Drill Bit Set,7PCS 90 Degree Drilling Chamfering Tool - 3 4 5 6 8 10 12mm: amzn.to/48KiTO5
    Magnetic Base Adjustable Metal Test Indicator Holder Digital Level 14" - Tool Stand: amzn.to/2PkyoTV
    Proxxon 37172 Micro Band Saw MBS/E: amzn.to/2ONORR1
    Anytime Tools Angle Block Set 1°, 2°, 3°, 4°, 5°, 10°, 15°, 20°, 25°, 30° Precision +/- 20 Seconds, Machinist Tool, 10 Piece Set: amzn.to/2QFqM2Y
    Consumables:
    Dykem 80300 Steel Blue Layout Fluid: amzn.to/3LvNAO8
    Bergeon Professional Cleaning Rodico: amzn.to/3LyKKb3
    Dialux Metal Polishing Compound White and Grey 4oz 1/4b: amzn.to/3vopCPo
    Blue Matador Abrasive Paper: amzn.to/3PRnQhJ
    Moebius Multi-Purpose Lubricating High Grade Swiss Oil: amzn.to/3PNNK5M
    General Purpose Latex Finger Cots: amzn.to/3ZsYrhi
    Proxxon 28174 Band saw blade for MBS/E Swedish steel, fine (24 TPI), Silver|Silver metallic: amzn.to/3RzIV1l
  • บันเทิง

ความคิดเห็น • 72

  • @protocol6
    @protocol6 ปีที่แล้ว +47

    Reminds me of the days before surface mount electronics when I'd make circuit boards at home.

    • @taitano12
      @taitano12 ปีที่แล้ว +3

      Eh. I still do this, even with SMDs... Or, at least I used to. SMD is a bit fiddly for my taste. Though, I do look to be getting back into electronics again.

    • @blahblahblahblah2933
      @blahblahblahblah2933 ปีที่แล้ว +1

      I prefer SMD parts when I make my own boards; fewer holes to drill.

    • @HSkraekelig
      @HSkraekelig ปีที่แล้ว +1

      Me, too, though after working with Ferric Chloride for a while I switched to Ammonium Persulfate. Much less stainy :) Letraset dry transfers and a resist pen. Those were the days :)

  • @taitano12
    @taitano12 ปีที่แล้ว +14

    I remember the main video series this came from. The whole thing is part of several projects on this and a few other channels that have really motivated me to get back into Making and Hacking. The finished clock is freaking gorgeous, and the shop is small enough that I can build something like it on a trailer. Chris definitely has given me some good inspiration.

  • @jakobhalskov
    @jakobhalskov ปีที่แล้ว +6

    Smiled when the iPhone timer from ancient times appeared :)

  • @doug8515
    @doug8515 ปีที่แล้ว +13

    A master talent at work. Incredible craftsmanhip.

  • @ironnerd8336
    @ironnerd8336 ปีที่แล้ว +1

    You have a way of making nerve-wracking things chill, and it never disappoints.

  • @Watchyn_Yarwood
    @Watchyn_Yarwood ปีที่แล้ว +1

    You never cease to amaze me!

  • @PhilWaud
    @PhilWaud ปีที่แล้ว +2

    Your silent instructional videos are so well made and informative! Thank you.

  • @dyamant78
    @dyamant78 ปีที่แล้ว

    Can’t wait for the next video of A. Mechanism series!! Thank you for sharing your awesome content!!

  • @needamuffin
    @needamuffin ปีที่แล้ว

    I love that it also alters the chemistry of the parts it does affect and bribs more of the copper to the surface so that the color changes.

    • @nerd1000ify
      @nerd1000ify ปีที่แล้ว

      It's dezincification of the brass. What's actually happening is the zinc dissolves first, leaving a porous layer of copper behind. A common problem for brass parts in chloride solutions, e.g. seawater.
      You can get dezincification resistant (DZR) brass, it has a small amount of arsenic added to the alloy.

  • @willembont4790
    @willembont4790 10 หลายเดือนก่อน +1

    Nice job. Looks beautiful.

  • @TheTarrMan
    @TheTarrMan ปีที่แล้ว

    Looks awesome.

  • @ServantOfBoron
    @ServantOfBoron ปีที่แล้ว

    Masterwork level of craftsmanship! When can we expect the next video about Antikythera mechanism?

  • @beez8888
    @beez8888 ปีที่แล้ว +1

    Gorgeous !!

  • @heighRick
    @heighRick ปีที่แล้ว

    Thanks for the video, helps a lot!

  • @nzs316
    @nzs316 11 หลายเดือนก่อน

    Fascinating!

  • @johnnycomelately6341
    @johnnycomelately6341 ปีที่แล้ว +1

    Brilliant

  • @apollorobb
    @apollorobb ปีที่แล้ว +1

    Same way i do circuit boards . Except i use a thermal printer transfer method a lot less steps . Never thought of doing it on brass

  • @matthasaname
    @matthasaname ปีที่แล้ว +8

    Oh to be able to just push around a broom in your shop.

    • @mpetersen6
      @mpetersen6 ปีที่แล้ว +8

      To judge by his shop tour video you could pretty much do it standing still.

    • @theselectiveluddite
      @theselectiveluddite ปีที่แล้ว

      @@mpetersen6 :D

  • @clintongryke6887
    @clintongryke6887 ปีที่แล้ว

    Lovely.

  • @soxxz2028
    @soxxz2028 ปีที่แล้ว +1

    wish i could get my pcbs this good

  • @Philtoid
    @Philtoid ปีที่แล้ว +1

    Phenomenal

  • @redfish6C
    @redfish6C ปีที่แล้ว

    Bravo !!!

  • @joesmith1574
    @joesmith1574 10 หลายเดือนก่อน

    Cool!

  • @stevearehart313
    @stevearehart313 ปีที่แล้ว

    I wish you lived in Nebraska, USA

  • @thoane1
    @thoane1 ปีที่แล้ว +1

    For beter application of the film, you can spray water on the brass plate befor application the film

  • @jigglemore
    @jigglemore ปีที่แล้ว

    Man that’s a cool retro phone you got there! How is that thing still alive?!

  • @ralhmcc47
    @ralhmcc47 ปีที่แล้ว +1

    In the event it has to be done vent that the finished dial is not up to your standards can the dial be salvaged or a new piece of brass and start over? Or flip it over and etch the other side?

  • @enricotosco
    @enricotosco ปีที่แล้ว

    Bellissimi lavori! Come agente corrosivo puoi anche usare, in bagni differenti, acqua ossigenata a 130volumi per ossidare e acido cloridrico concentrato per corrodere la parte ossidata.
    Intervallando con risciacqui con acqua corrente.

  • @IIGrayfoxII
    @IIGrayfoxII ปีที่แล้ว +1

    I have a large bottle of Ferric Chloride powder I have not used in ages.

  • @TrevorDyck
    @TrevorDyck ปีที่แล้ว +1

    So cool. I would *definitely* screw this up in at least ten ways!

  • @donaldasayers
    @donaldasayers ปีที่แล้ว

    Spent a good part of my teaching career, teaching electronics and using ferric chloride to etch circuits; I hate the stuff.

  • @stevearehart313
    @stevearehart313 ปีที่แล้ว

    Excellent video as usual. A bit of verbal explanation per process on this one would be nice.

    • @Bobs-Wrigles5555
      @Bobs-Wrigles5555 ปีที่แล้ว +1

      If you want the very detailed narrative go to the video link in the description, Chris has purposely changed the sound track to music for this "clips" channel

  • @butsukete1806
    @butsukete1806 ปีที่แล้ว +6

    That phone has to be at least a decade old, how does the battery still hold a charge?

    • @ClickspringClips
      @ClickspringClips  ปีที่แล้ว +12

      preview of iphone 20, they're going full retro :)

    • @cantisaniluthier
      @cantisaniluthier ปีที่แล้ว

      I still have an iphone 3gs that I use as an ipod. it have better battery than the iphone 5 I owned a few years ago 😅

  • @CorwynGC
    @CorwynGC ปีที่แล้ว

    I'm curious what washing with water does *after* cleaning with Acetone.

    • @highlorddarkstar
      @highlorddarkstar ปีที่แล้ว

      Given the acetone was to get rid of resist, probably to prevent damage to the resist you want to keep by washing off any remaining acetone.

  • @cycoholic
    @cycoholic ปีที่แล้ว +1

    Just thinking closed captions like Primitive Technology does on his videos would be good for these silent Clickspring videos.
    👍❤

    • @ClickspringClips
      @ClickspringClips  ปีที่แล้ว +2

      Refer to link in description for source video for more details - Cheers :)

    • @cycoholic
      @cycoholic ปีที่แล้ว +2

      Oh I know. It was just an idea. 😊

  • @olivierw7405
    @olivierw7405 หลายเดือนก่อน

    Hi dear Friend
    What is the temperature of the water you add to your sodium carbonate please ?
    I need to wait for a very long time to develop but i use it at ambiant temperature
    Thanks
    Olivier from France

  • @undersiege3402
    @undersiege3402 ปีที่แล้ว +1

    would be cool to plate the etched parts with silver or something

    • @DanielSMatthews
      @DanielSMatthews ปีที่แล้ว

      Before you remove the etch mask you could try electroplating if you want another metal in those etched details.

    • @theselectiveluddite
      @theselectiveluddite ปีที่แล้ว

      Click on the link in the description; he uses a method called 'Silvering'' to coat it in a layer of silver :) Cheers

  • @SeraphimKnight
    @SeraphimKnight ปีที่แล้ว

    An iphone 3G?! Hot damn, that's pretty ancient now

  • @sanudhara
    @sanudhara 10 หลายเดือนก่อน

    What was that black sticker? Is it regular sticker?

  • @randysarmiento8842
    @randysarmiento8842 9 หลายเดือนก่อน

    what is the last liquid you apply is it water or what?

  • @AdrajKSA
    @AdrajKSA 6 หลายเดือนก่อน

    What is the name of the material used to transfer the design to metal?

  • @sachinaudiolibrary3656
    @sachinaudiolibrary3656 6 หลายเดือนก่อน

    What is the chemical used to take a print on it To print a photo on it first put a sticker on it What is the chemical in it

  • @bulachesan
    @bulachesan 11 หลายเดือนก่อน

    Hello , what varnish are good with mirror finish brass ( keeping from darkening and oxidation in general)

    • @ClickspringClips
      @ClickspringClips  11 หลายเดือนก่อน

      A general PU coating works ok, I have used this: www.bunnings.com.au/white-knight-500ml-rust-guard-clear-quick-dry-topcoat-paint_p1564192 - Cheers :)

    • @bulachesan
      @bulachesan 11 หลายเดือนก่อน

      @@ClickspringClips thank you for our answer , help me a lot
      have to see if I find this in Europe
      Daniel

  • @raymondsanderson304
    @raymondsanderson304 ปีที่แล้ว

    Chris why IIII why not IV??

  • @zsomborhollay930
    @zsomborhollay930 ปีที่แล้ว

    What is the reason for using IIII instead of IV? It always bugged me as a child and I still don't know the answer.

    • @d00dEEE
      @d00dEEE ปีที่แล้ว +1

      That's the original additive notation that the Romans used (IIII VIIII and so on). The subtractive notation (IV and IX) was a later notation developed by the Germans.

    • @ZackC
      @ZackC ปีที่แล้ว

      There’s also the aesthetics of how IIII more neatly balances visually against VIII than IV would.

  • @ExcessiveModeration5
    @ExcessiveModeration5 ปีที่แล้ว

    Why is 4 represented as “IIII” not IV…I saw this on another clock once and thought it was a goof up

  • @TimoWestenfelder
    @TimoWestenfelder ปีที่แล้ว

    what kind of foil is that?

    • @Zetex2000
      @Zetex2000 ปีที่แล้ว

      photoresist dry film

    • @nalinux
      @nalinux ปีที่แล้ว

      Photosensitive Dry Film

    • @blahblahblahblah2933
      @blahblahblahblah2933 ปีที่แล้ว

      Riston is one brand (though there are several types).

  • @ianpendlebury3704
    @ianpendlebury3704 ปีที่แล้ว +1

    Be very careful with Ferric Chloride. My Dad was a circuit board builder in the 1980's and he had major problems with my otherwise easy-going Mother concerning 'degradation' of the so-called stainless steel kitchen sink. This stuff is relentless in its staining capabilities. Just a heads up.....

  • @nalinux
    @nalinux ปีที่แล้ว +2

    Citric acid works as well as vinegar to clean copper, and doesn't smell.
    It also taste better IMHO :)

    • @mpetersen6
      @mpetersen6 ปีที่แล้ว +2

      Vinegar works better on salads though.

  • @X3ST3RIN
    @X3ST3RIN ปีที่แล้ว

    3.32........