  • Here are the 6 different Hot Melt Glue Sticks I used in this video
    1. Easton Low Temp Hot Melt ► amzn.to/3pRrDyR
    2. Bohning 1308 Ferry-L-Tite Cool Flex ► amzn.to/3mrUNm8
    3. Black Hot Melt ► amzn.to/3pQyjgy
    4. Infinity Bond Tough Guy ► amzn.to/3EzzZzs
    5. Orange Hot Melt ► amzn.to/3EtilgA
    6. CDM Flitemate ► www.lancasterarchery.com/cdm-...
    TOP 2 Winners
    ►1st Place CDM Flitemate ► www.lancasterarchery.com/cdm-...
    ►2nd Place Easton Low Temp Hot Melt ► amzn.to/3pRrDyR
    MERCH & MORE ARCHERY! : shoreshotarchery.org/store/
    Subscribe & Like Here: ► / @shoreshotarchery
    My Camera Gear
    Main Camera ► Canon C200 amzn.to/2WneqPw
    Second Camera ► Canon C100 Mark II amzn.to/38UbrRs
    Travel Camera ► Canon G7 X Mark III amzn.to/33oplKa
    Slow Motion Camera ► GoPro Hero 8 Black amzn.to/2vrzMjP
    My Drone ► amzn.to/2x1CtsH
    My Smaller Drone ► amzn.to/39Yeh99
    Camera Bag ► amzn.to/2WlrYez
    Gnarly 28-70 Lens ► amzn.to/2QjzX7W
    DOPE B Roll Lens ► amzn.to/3d8gOQg
    3 Legged Thing Tripod ► amzn.to/3d9t8Q3
    Microphone ► Audio Technica AT875R amzn.to/2WkcM1i
    Rode Video Mic Pro Plus ► amzn.to/2Ur8VwT
    Think Tank Memory Card Organizers ► amzn.to/3d5EZyx
    Think Tank SD Organizers ► amzn.to/2TWEG1H
    Samsung T5 SSD Drive ► amzn.to/2WiVEJ0
    FOLLOW ME:
    Instagram ► anthonyarch...
    Facebook ► / shoreshotarchery1
    Website & Shop ► shoreshotarchery.org/
    Twitter ► / shoreshotarcher
    Affiliate links were used in this description.

ความคิดเห็น • 29

  • @shoreshotarchery
    @shoreshotarchery  2 ปีที่แล้ว +10

    The Blue Glue from Bohning is designed for all carbon arrows. It is NOT designed for carbon arrows with aluminum on the inside like the Easton X10. Yet archers around the world still use it on aluminum shafts and aluminum interior walled shafts.

    • @zacharyclark8905
      @zacharyclark8905 2 ปีที่แล้ว +4

      I was about to say the same thing

    • @garrettstraffon608
      @garrettstraffon608 ปีที่แล้ว +1

      I just ordered some hot melt and was going to start messing with it and I chose the blue glue and was kinda disappointed until I seen you said this. I’m using Easton axis so there not aluminum on the inside. But I do what to experiment and take them out anyways kinda why I’m messing with the hot melt. When it’s all said and done I’ll prob epoxy my final hunting arrow

    • @garrettstraffon608
      @garrettstraffon608 ปีที่แล้ว +1

      @@timberlandone4054 trust me I’ve made a bunch of arrows. And use hot melt if you want to tinker with weight. But if you are sure about the weight you want I would say epoxy your hunting arrows if you want.

    • @Australian_Made
      @Australian_Made 4 หลายเดือนก่อน

      😎

  • @InFerrumVeritas
    @InFerrumVeritas ปีที่แล้ว

    This is still maybe my favorite video from you.

  • @pequodexpress
    @pequodexpress ปีที่แล้ว

    Has anyone tested Stanley Dual Melt for securing arrow points?

  • @wangchili
    @wangchili ปีที่แล้ว +3

    Did not mention Bohning Yellow. Bohning Blue for carbon arrows therefore lower heat and probably lower strength. Bohning Yellow, for everything else and stronger. Would advise including Bohning Yellow and ditching one of the other off/non archery brands. I've got the sneaking suspicion that the Easton Yellow might be Bohning Yellow in disguise.

  • @YoureSoVane
    @YoureSoVane ปีที่แล้ว +1

    I should probably use a good hot melt, but instead I've been running an automotive impact resistance adhesive. Only thing that has come loose are Gold Tip points, and that's because GT is notorious for tolerances. They like really small internal components, creating way too big of a gap.

  • @swamprat9018
    @swamprat9018 4 หลายเดือนก่อน

    you really need to put some in the arrow. the tight tolerance between shaft of point pushes the glue out. learned that years ago when running a shop in the 80's the no. 4 was my guess as best glue.

  • @Australian_Made
    @Australian_Made 4 หลายเดือนก่อน

    · Ima gunna git me
    some o' that CDM low-melt stuff
    100% 👍👍
    THANK YOU for doing this so I don't ...

  • @loh3n785
    @loh3n785 2 ปีที่แล้ว +2

    I have been using Gorilla glue for years, no need to heat up and it's an armored collage that has never budged

    • @shoreshotarchery
      @shoreshotarchery  2 ปีที่แล้ว

      Your the 2nd person to tell me about this. What type of Gorilla Glue?

    • @garrettstraffon608
      @garrettstraffon608 ปีที่แล้ว +2

      The whole point of hot melt is to be able to take them out, but yes gorilla glue epoxy and they will never come out

  • @imper-usr
    @imper-usr 2 ปีที่แล้ว

    Thx for comparison! But plz - do something with video focus =(

    • @shoreshotarchery
      @shoreshotarchery  2 ปีที่แล้ว +3

      Best I can afford at the moment sorry😞 After 1k videos the camera is getting old

  • @thong0128
    @thong0128 ปีที่แล้ว +3

    Good information and decent test, but I think you should focus more on presentation like adding charts or graphs, it will be more helpful. Try to learn from channels like fam project, which have great presentation and straight forward. With it, i think you will have more subscribers, keep up the good work

  • @Australian_Made
    @Australian_Made 4 หลายเดือนก่อน

    😂 😜 😁

  • @davidbryan4978
    @davidbryan4978 2 ปีที่แล้ว +2

    Pardon the pun, what’s the point?
    Any glue only needs to be stronger then the friction generated by removing the arrow, for the point to remain in the shaft.
    an arrow maybe shoot into a target at 45 pounds, it’s not 45 lbs to removing the arrow.
    It’s friction on the point and arrow that a glue would have to over come.
    If it’s solely a test of the glue use a gauge and a winch to pull them apart and see where it fails.

    • @atxjaphotos4217
      @atxjaphotos4217 ปีที่แล้ว

      Adjusting an arrow for a new broadhead is important to people who don't want to buy brand new arrow shafts.

    • @davidbryan4978
      @davidbryan4978 ปีที่แล้ว

      @@atxjaphotos4217 yeah I know what the point of glue is... did you read the full comment?
      and most people I know that use broadheads use screw in points so they can change from a field point for practice and broadhead for hunting.

  • @Australian_Made
    @Australian_Made 4 หลายเดือนก่อน

    · I'm 100% SOLD on
    Bohning Blue low-melt glue for
    PIN NOCK ADAPTORS !!!!!! 👍👍

    • @Australian_Made
      @Australian_Made 4 หลายเดือนก่อน

      ... that is ... as a consequence
      of YOUR testing ! TY 😇👍

    • @Australian_Made
      @Australian_Made 4 หลายเดือนก่อน

      Especially since I already own
      the Bohning Ferr-L-Tite BLUE

  • @mariusdevalmont7432
    @mariusdevalmont7432 2 ปีที่แล้ว +3

    The Blue Bohning was STUPID to test on a X10...The Blue Bohning is SPECIFICALLY formulated for ALL CARBON shafts...and YOU stuck it IN an aluminum ID shaft.....

    • @shoreshotarchery
      @shoreshotarchery  2 ปีที่แล้ว +5

      I know of several top archers in the USA and internationally that use it for their Easton X10s.

  • @jeremyliem7879
    @jeremyliem7879 ปีที่แล้ว

    Dude, the constantly changing focus on the intro gave me a headache

  • @Why...So...Stupid...
    @Why...So...Stupid... 3 หลายเดือนก่อน

    The blue bohning is made for carbon shafts only.