    These soft lead stick ons take longer in this hot plate set-up because they are pure lead with the melting point of 621 degrees F. The clip on weights are an alloy of lead, Tin, and antimony. Tin lowers the melting point somewhat so they melt quicker.

  • @jamespollard1670
    @jamespollard1670 ปีที่แล้ว

    The ingot pans may have been teflon coated and caused the pitting on the ingots .

    • @ITZGR82BFREE
      @ITZGR82BFREE  ปีที่แล้ว

      No doubt... hopefully that will burn off and produce better looking ingots. Ugly still serves its purpose.

    • @jamespollard1670
      @jamespollard1670 ปีที่แล้ว

      @@ITZGR82BFREE I found some old solid aluminum muffin pans at a garage sale . The ingots fall right out and no worry about the ingot pan coming apart . The newer ones are crimped together and separate some times .

    • @ITZGR82BFREE
      @ITZGR82BFREE  ปีที่แล้ว

      @@jamespollard1670 Good point. Always looking to repurpose items to save money. Thanks