  • @edycoo3499
    @edycoo3499 ปีที่แล้ว +2

    Excellent video and sound quality.Very impressive product!!

  • @andrewwilliams7141
    @andrewwilliams7141 ปีที่แล้ว +3

    You've now got 3 whisks coated with gluey gunk. It's almost impossible to clean them. I use wood battens as mixing sticks which can simply be thrown away. Saves having a drill outside in the elements too.
    Thanks for the video though.

    • @bradley.h
      @bradley.h 8 หลายเดือนก่อน +1

      That's what I've always done and just normal black builders bucket with the litres on them, instead of those fancy ones

  • @digitaria
    @digitaria 3 หลายเดือนก่อน

    Don’t you need to put resin down on the primer surface before putting the mat down? I thought you put resin on the primer the two coats on the top of the matting.

  • @JohnDoepoops
    @JohnDoepoops 8 หลายเดือนก่อน

    is this better than felt ?

    • @bradley.h
      @bradley.h 8 หลายเดือนก่อน

      For an overlay system it is, but I would just strip it and just use their 10 10 products or Cure-It with new osb3 t&g

  • @thewoodmuncher8140
    @thewoodmuncher8140 ปีที่แล้ว +2

    Obviously don’t forget that not everything is obvious, obviously

    • @bradley.h
      @bradley.h 8 หลายเดือนก่อน

      He's most probably taking to people with previous experience with grp/liquid waterproofing

  • @BavaJee804
    @BavaJee804 10 หลายเดือนก่อน

    Can you put felth on a fibre glass ?

  • @stuw5910
    @stuw5910 6 วันที่ผ่านมา

    All those chemicals. All that mixing. Even some references to splashing yet . . . NO SAFETY GOGGLES!. Health and Safety at work! Obviously.

  • @robpower100
    @robpower100 5 หลายเดือนก่อน +1

    Obviously!! What ever you chose to do proper trades, strip and start again, secondly don't use a whisk with anything with a catalyst its a no no, it cooks too quickly. Don't be sold by the confusing buckets they are a complete waste of time and for marketing purposes only, it looks messy, amateurish and just another roofing gimmick.

  • @offshoretinker
    @offshoretinker 9 หลายเดือนก่อน +3

    NAH, rip it off and start again.

  • @Jim-s7l1s
    @Jim-s7l1s 10 หลายเดือนก่อน +1

    Load of crap. Just go over it again with sbs two layer felt

    • @bradley.h
      @bradley.h 8 หลายเดือนก่อน

      This is a quick overlay system. You can't beat classic grp though. Just stip the felt and overdeck with osb3 and fibreglass

    • @Jim-s7l1s
      @Jim-s7l1s 8 หลายเดือนก่อน +1

      @@bradley.h just about every fibreglass roof I’ve been on is leaking due to it cracking. Far too rigid.Only plus is that is looks well. I’ve recovered far too many grp roofs in my lifetime to reguard it as a good roof.

    • @bradley.h
      @bradley.h 8 หลายเดือนก่อน

      ​@@Jim-s7l1s Do you mean cracking of the topcoat or base layer. Fibreglass roofs do allow movement for expansion and contraction, however if expansion joints aren't installed or if the foundation is stable this will happen, expecially on warm roofs. It always comes down to the installer

    • @Jim-s7l1s
      @Jim-s7l1s 7 หลายเดือนก่อน

      @@bradley.h completely cracked enough for water penetration. Funny you say they allow for movement but I found this is not the case. The weather in uk and Ireland does not suit it. One day can be 3 degrees next day 20c

    • @bradley.h
      @bradley.h 7 หลายเดือนก่อน

      This is the fault of the installer. The topcoat is UV resistant and if the base layer cracked, they either haven't used suitable matting (600g) or the boarding is wrong. T&g sterling allows moving with spacing between the joins, also expansion joints are fitted at 50m2. I only do fibreglass roofs, and occasionally ponds, pools and wet rooms. If installed correctly, you cannot beat it. This shouldn't be an off-the-shelf product for anyone to buy