I can honestly say in my 40 years I've never ever seen inspection has bad as these guys, Finished weld only wire brush or a engineering file/chipping hammer Not a piece of angle iron which can add defect to the final weld the way he using it, Applicators am say no more how they used them,
I can honestly say in my 40 years I've never ever seen inspection has bad as these guys,
Finished weld only wire brush or a engineering file/chipping hammer
Not a piece of angle iron which can add defect to the final weld the way he using it,
Applicators am say no more how they used them,
Totally wrong 😮
Very bad
Wrong method
Wrong method