  • @MoeReefs
    @MoeReefs 11 ปีที่แล้ว +4

    Very informative video. Now I know all I need is to mix some baking soda in some water for flux and braze with a clothes hanger. THANKS

  • @441rider
    @441rider 13 ปีที่แล้ว

    Flows very well,

  • @cagrigurbuz
    @cagrigurbuz  17 ปีที่แล้ว

    Manufacturer is ForteBraze and the flux name is 040.
    Alloy composition used is ZnAl4 (Al: 4%, Zn: rest) wire.
    For contact details please refer to the explenation on the right of the video.

  • @demircivaz
    @demircivaz 16 ปีที่แล้ว

    Hocam eğitici bir video elinze sağlık

  • @azzaza12345
    @azzaza12345 14 ปีที่แล้ว

    The Oweld flame's temperature is about 3600 degrees. You don't melt the alluminum because you go more fast. Thanks to this temperature the alloy goes deeper and the joints are more stronger. Moreover with Oweld gas generators you don't spend costs of gas any more and you will have a safe workplace (without risks of explosion, monoxide of carbon...).

  • @ju87b1
    @ju87b1 13 ปีที่แล้ว

    How much pressure can the joint handle?
    Will it hold up to the new 410 pressures for air conditioners?

  • @cagrigurbuz
    @cagrigurbuz  17 ปีที่แล้ว

    Bu kalınlıktaki Aluminyum boruları birbirine veya Alumninyum - Bakır birleştirilmesinde, özellikle buzdolabı üretiminde bir sorun yaşanmadan rahatlıkla kullanılıyor. Başka Aluminyum birleştirmelerinde diğer sert-lehim metodları kullanılabilir.
    Burada kullanılan ZnAl4 alaşımı ile 450 °C'de işlem gerçekleşiyor, daha sık kullanılan AlSi12 alaşımıyla yapılan sert-lehim işlemi isie 560 °C'de.

  • @hoangdung8995
    @hoangdung8995 13 ปีที่แล้ว

    I want to ask compounds with aluminum brazing ???????

  • @danger52100
    @danger52100 14 ปีที่แล้ว

    tell me the flux mixture you used

  • @error204
    @error204 13 ปีที่แล้ว

    @OTOPUN ahi dice 040 mezclado con agua. supongo qe sera agua destilada.

  • @Realcreater12
    @Realcreater12 6 ปีที่แล้ว

    Sir what is White past

  • @JamesSmith-rl7nb
    @JamesSmith-rl7nb 2 ปีที่แล้ว

    #8staybrite works just as good.
    Clean piping with a brass brush/ never use sandcloth on aluminum

  • @danger52100
    @danger52100 14 ปีที่แล้ว

    What temperature you braze with, type of gas. type of flux I should have asked. would that hold up in refrigeration

  • @cagrigurbuz
    @cagrigurbuz  17 ปีที่แล้ว

    Forteflux 040 brazing flux is mixed with pure water. 20-25% pure water is added on a balance.

  • @error204
    @error204 13 ปีที่แล้ว

    @cagrigurbuz tap water?

  • @cagrigurbuz
    @cagrigurbuz  13 ปีที่แล้ว

    @error204 pure, distilled or demineralized water

  • @cagrigurbuz
    @cagrigurbuz  14 ปีที่แล้ว

    Oweld machines generates Hydrogen and Oxygen with electrolysis of water. Can be used, but due to Hydrogen flame has very high temperatures, there is a possibility to melt aluminium. Use of wide and soft flame is advised in this application, like propane.

  • @Dizaynspeed
    @Dizaynspeed 12 ปีที่แล้ว

    Nice Turks. keep it up :)

  • @kingofadana
    @kingofadana 17 ปีที่แล้ว

    Peki genel olarak soyle bir soru sorsam aliminyum parcaları birbirine lehim etmede en uygun yontem hangisi. Torch brazing mi yoksa baska bir metod mu? neden veya neden degil? tesekkurler. bu arada ben de cukurova makina muh. ogrencisi ya sen.

  • @zubeirrezaei4343
    @zubeirrezaei4343 3 ปีที่แล้ว

    پودر چیه ک با آب قاطی میکنه قبل جوشکاری ب لوله ها میزنه

  • @raskinozturk
    @raskinozturk 13 ปีที่แล้ว

    merhaba aluminyum kaynağı ile ilgili fikir alışverişinde bulunmak isterim

  • @cagrigurbuz
    @cagrigurbuz  14 ปีที่แล้ว

    flux is 040 mixed with water

  • @kingofadana
    @kingofadana 17 ปีที่แล้ว

    Beyler bari aliminyumun daha profesyonelce yapılan bir lehimini gosterseydiniz. Sizce aliminyumu lehim etmede en uygun yontem Torch brazing mi? Bence aliminyumun ic yapısı falan bayagı bozuluyor.

  • @z044017
    @z044017 13 ปีที่แล้ว

    what kind of flux are you using?

  • @AK-oy4ne
    @AK-oy4ne 4 ปีที่แล้ว

    Split AC के outdoor unit के aluminium condenser pipe और coper paip के जोड़ के लीकेज को ,बिना गैस निकाले और बिना bilding के, किस प्रकार जोड़े की , वहाँ पर का गैस लीकेज हमेशा के लिये बन्द हो जाये ।

  • @CoolasIce2
    @CoolasIce2 15 ปีที่แล้ว

    It looks like you are SOLDERING using the brazing flux.
    huh?

  • @1crazyfocker
    @1crazyfocker 13 ปีที่แล้ว +1

    thats not brazing..its just soldering..yes both are close to the same thing, but if you use solder then its soldering..lol still a good video but a little missleading. the two main differances between the twoo are 1. temp, (solder melts at a really low temp, almost like lead, in fact you can solder with lead as well) 2. when soldering all you have to do is touch one place on the pipe and it will flow all the way around the pipe "soldering it" with brazing you have to slowly work it around.

  • @cagrigurbuz
    @cagrigurbuz  14 ปีที่แล้ว

    oil should be cleaned before brazing.