Making an AMT Loudspeaker Membrane (practice)

แชร์
ฝัง

ความคิดเห็น •

  • @mariancol2428
    @mariancol2428 7 หลายเดือนก่อน +1

    Very detailed and explicit, a lot of movement with a lot of precision, that's why everything you do can be heard well!

    • @joppepeelen
      @joppepeelen  7 หลายเดือนก่อน

      thank you sir :) its fun to play around !

  • @emileburnabylautier9426
    @emileburnabylautier9426 4 ปีที่แล้ว +1

    this is genius Joppe my hat is off to you

  • @MechanicsDIY
    @MechanicsDIY 4 ปีที่แล้ว +3

    really good one . looks like the real deal . or close , it might be a good idea to use epoxy glue
    insted of hot glue for longer shelf life . (and pro standart resault )

    • @joppepeelen
      @joppepeelen  4 ปีที่แล้ว +2

      yeah downside is mixing and gettign right viscosity and waiting... i dont like waiting :) haha

    • @MechanicsDIY
      @MechanicsDIY 4 ปีที่แล้ว +2

      @@joppepeelen ya that's the way to go ... for a prototype . but you got somthing that can be more then that , once you get it right you might be able to make money selling some

  • @new-kids-on-the-block
    @new-kids-on-the-block 18 วันที่ผ่านมา +1

    thanks voor het door sturen van de info jij moet ok echt een vorm van ocd hebben wil je dit kunne en wille doen mooi project !! ok mooi de verkeerde kand folie zie je aleen maar als je het al gedaan hebt 🤣 woepsss

    • @joppepeelen
      @joppepeelen  18 วันที่ผ่านมา

      Nou ik kan redelijk rommelig zijn :) maar ik kan wel dingen 100 keer opnieuw proberen dat dan weer wel :)

  • @kuuhgle
    @kuuhgle ปีที่แล้ว

    Those metal plates of the jig...are they 1mm thickness too like the pleat spacing or less to make the fold better?

    • @joppepeelen
      @joppepeelen  ปีที่แล้ว +1

      its plastics, but if i remember correct they where 1mm. i did alter the combs to hold it before glueing , i made them thinner i believe to compensate for it bulging out a little and becoming wider then they should it has been a while since i made them. so cant say for sure. i do mention it i believe in the video what i did. changin the stack of plates is kind of allot of work so im sure i did not alter them haha i could have done, bit like the ADAM amt fold jig i believe

  • @leohobbleohobb3781
    @leohobbleohobb3781 4 ปีที่แล้ว

    A amt production i saw they put solder on each end with a strip when i was in the jig so it keep the shape.

    • @joppepeelen
      @joppepeelen  4 ปีที่แล้ว

      those amts have there connection point there. an extra strip above where the coil curves. to attach there wires :) but they did use a glue from a seringe before the soldering job :)

  • @rhalfik
    @rhalfik 2 ปีที่แล้ว +1

    Some Americans don't pronounce B in comb at all. They just say com with somewhat french accent.

  • @todayisgood7836
    @todayisgood7836 4 ปีที่แล้ว +1

    Прекрасно. Вы - мастер.

  • @leohobbleohobb3781
    @leohobbleohobb3781 4 ปีที่แล้ว

    you use hot glue where they solder when it is in the folding jig.aah the suspense..he he.

  • @黃千容-k9d
    @黃千容-k9d 2 ปีที่แล้ว

    Where did you get the tool?

  • @bunnythekid
    @bunnythekid 4 ปีที่แล้ว +1

    Would having the membrane in tension affect the sound negatively? You could add some more rods on your jig (at both ends), then glue tabs onto the membrane every time you fold it. That way you keep it together and you could tension it too. It would probably make it harder to pull the jig apart and get the membrane off after but it could be worth a try.
    If I’m not making what I mean very clear I’ll draw it up and send it to you Facebook.

    • @joppepeelen
      @joppepeelen  4 ปีที่แล้ว +1

      No the folds just look cleaner when on tension but resonance will increase to so :) not gone try :) saves us both some work to hehe

  • @joppepeelen
    @joppepeelen  4 ปีที่แล้ว

    sorry quality seems to be stuck at 360.... youtube is a bit slow

    • @Xumatro
      @Xumatro 4 ปีที่แล้ว +1

      I'm watching in 1080p rn so it's fixed

  • @camelazo
    @camelazo 4 ปีที่แล้ว

    That´s it!

  • @ABC-rh7zc
    @ABC-rh7zc 4 ปีที่แล้ว

    Do you sell any of your creations?

    • @joppepeelen
      @joppepeelen  4 ปีที่แล้ว +2

      Maybe , but for now I got nothing complete to sell haha. But in the end I wish to sell complete speakers as a brand. Incorporating my own creations

    • @sc0or
      @sc0or 3 ปีที่แล้ว

      joppe peelen You definitely could try selling tweeters. All they need is a finished front panel and some 3d printed case. And prices for good tweeters are quite high. Your ribbon ones that can play from below 2kHz, are quite unique. This way you might get funds for the loudspeakers production.

  • @lightbit553
    @lightbit553 4 ปีที่แล้ว

    Maybe you could use silicone instead of hot glue.

    • @ABC-rh7zc
      @ABC-rh7zc 4 ปีที่แล้ว

      or just super glue?

    • @camelazo
      @camelazo 4 ปีที่แล้ว

      Rigid epoxi (A-B) is the solution!! th-cam.com/video/J1-5IvkrNQc/w-d-xo.html, you need stiffness to avoid the damp of that gooey silicon, that´s obvious.

    • @joppepeelen
      @joppepeelen  4 ปีที่แล้ว

      Both take much to long :(