  • Use nails to fix the two types of floors on the ground, increase the high temperature to more than 40 degrees, and start the timer to 51 degrees, the PVC floor begins to deform, continue to increase the high temperature for testing, the SPC floor still does not lift for 10 minutes after the high temperature rises above 60 degrees After the PVC floor becomes very soft