Solvent Welding Acrylics

แชร์
ฝัง
  • เผยแพร่เมื่อ 14 ก.ย. 2020
  • Mike from Model Makers Inc demonstrates solvent welding acrylic sheets. This process allows us to create 3-dimensional shapes or build complex structures from flat acrylic sheets.
    Do you have any questions on plastic fabrication? Just let us know!

ความคิดเห็น • 123

  • @canuckle7shucks
    @canuckle7shucks 6 วันที่ผ่านมา

    Methylene Chloride, also known as Rez-n-bond. Used this for 37 plus years in the sign business. You can make a thick glue with this by adding scrap acrylic pieces to a gallon and letting it sit for a few weeks

  • @sudheergodgeri
    @sudheergodgeri 6 หลายเดือนก่อน +1

    Great info and technique - thanks I needed just this to make a small PC HDD cage using acrylic - without drilling/making holes

  • @reneephillips3020
    @reneephillips3020 ปีที่แล้ว +1

    Thank you for this tutorial. Would the same bonding technique be used for mirrored acrylic?

  • @les5074
    @les5074 2 ปีที่แล้ว +2

    Great video. I've been wanting to make my own display case for years " I'm a figure painter. " This was so helpful thanks....

  • @muthupanchu
    @muthupanchu 2 ปีที่แล้ว

    thank you sir.

  • @tazz347
    @tazz347 ปีที่แล้ว +6

    what happens if you get an accidental spill or a drop on the acrylic and how to clean it?

  • @wosang_pingf1238
    @wosang_pingf1238 ปีที่แล้ว +1

    thanks for your tutorial. Is there any reliable bond for very tiny piece acrylic to metal ? Any idea!

  • @noneofurbizness1271
    @noneofurbizness1271 2 ปีที่แล้ว +2

    Where can you buy this? and what exactly is the brand??

  • @davebarkerdesign
    @davebarkerdesign ปีที่แล้ว

    Do you quote prototypes? I need a plastic drawer roughly 28" x 28" x 7"

  • @gifted6305
    @gifted6305 2 ปีที่แล้ว

    Can I get the link to purchase it, I'm making a acrylic enclosure for my 3d printer and this would work great?

  • @WoodcraftBySuman
    @WoodcraftBySuman 3 ปีที่แล้ว +3

    Great video! I want to bond a large area of plexiglass. Roughly 9x14". Are the weld-on 3 an ideal solution for large surface like that?

    • @modelmakers33
      @modelmakers33  3 ปีที่แล้ว

      Yes, you can use this type of thin fast acting solvent to bond a large area, and it will be very strong, but it can be kind of patchy and not look good through the clear plexi. In order to achieve a thoroughly even, clear joint, you have to use a thicker and/or slower solvent.

  • @frankenstein3163
    @frankenstein3163 ปีที่แล้ว

    I wat to make double wall acrylic similar to double wall POLYCARBONATE sheets. Do you think the double wall acrylic with have a better insulation property's that the double wall polycarbonate ? I'm attempting to make a glass studio/office.

  • @michaelfenton5378
    @michaelfenton5378 2 ปีที่แล้ว

    We are building acrylic wine drawers, that will hold 4 wine bottles, should we use the methylene chloride solvent or should we use a stronger agent? We need to make sure the drawers do not come apart. Your guidance is much appreciated. Thank you!

    • @modelmakers33
      @modelmakers33  2 ปีที่แล้ว +2

      The methylene chloride bond is very strong as long as the mating surfaces have good contact. The solvent will not fill any voids.
      If you're not sure, you can put gussets on the inside corners - 1/8" X 1/8" or 1/4" X 1/4" square rod is commonly available. Cut the rod to the length of the seams, lay it in the corners, and bond to both the floor and the sides. That makes for a VERY strong joint!
      But again, this is not necessary if you have full contact between gluing edge and gluing surface. The solvent actually welds them into one piece where they touch.

  • @user-iq9mr5kb4c
    @user-iq9mr5kb4c 6 หลายเดือนก่อน

    염화메틸렌과 다른 첨가물을 혼합해서 쓰나요??
    접착면에 기포가 많이 생깁니다

  • @sachafourmann419
    @sachafourmann419 2 ปีที่แล้ว

    Puis je savoir quelle est la colle à utiliser pour un rendu extra solide svp ? merci

  • @nmc5h8MIZ
    @nmc5h8MIZ 4 หลายเดือนก่อน

    Is the bond improved if you can somehow apply pressure to the joint? I'm guessing since the liquid is so thin that an unsmooth surface can also mean a poor bond?

  • @voljoun5636
    @voljoun5636 ปีที่แล้ว +3

    hey ! nice video. if i want 2 acrylic parts to be strongly stuck together but keep it very transparent with no visible glue marks, what should i use?

  • @emildimofte6538
    @emildimofte6538 2 ปีที่แล้ว +2

    Bravoooo,model maker!!!excelent video lesson!!!!much obliged!!!!good luck to you master!!!👍👍👍👍👍👍👍👍👍👍👍👍👍👍👍👍👍🎯🎯🎯🎯🎯🎯🎯🎯🎯🎯🎯🎯🎯🎯⭐⭐⭐⭐⭐⭐⭐⭐⭐⭐⭐⭐⭐💎💎💎💎💎💎💎💎💎💎💎💎💎💯💯💯💯💯💯💯💯💯💯💯💯💯👏👏👏👏👏👏👏👏👏👏👏👏👏🎯🎯🎯🎯🎯🎯🎯🎯🎯🎯🎯🎯🎯💎💎💎💎💎💎💎💎💎💎💎💎💎⭐⭐⭐⭐⭐⭐⭐⭐⭐⭐⭐⭐⭐💯💯💯💯💯💯💯💯💯💯💯💯💯

  • @jakehealthx
    @jakehealthx ปีที่แล้ว

    does this process work the same for colored acrylic?

  • @nanda_pamungkas
    @nanda_pamungkas 2 ปีที่แล้ว

    Hello sir
    Im verry interest with acrylic, im planning to build acrylic bath for my pc to immersed with liquid oil for colling the gpu's, my question is is acrylic heat resisstant with temperature arround 40 to 90 degrees, if i want build my own bath gpu's / pc, i need that glue to combine anggle the acrylic, and is that glue heat ressistant and leak proffing for my liquid colling pc?
    For the answer im say thanks🙏🙏

  • @davidfreitas3992
    @davidfreitas3992 3 หลายเดือนก่อน

    Does this work on saw cut edges? I caught in the middle of the video on the manufacturer's website that they recommend ips weld on 16 acrylic cement instead if not a purely flat finish which your video seems to show?

  • @steputube
    @steputube 2 ปีที่แล้ว +1

    Thanks! What solvent would you recommend to glue a broken turntable cover - without a line?

    • @modelmakers33
      @modelmakers33  2 ปีที่แล้ว +1

      I assume the cover is clear plastic, and that it's cracked through. The type of solvent (not glue) to repair the crack would depend on the type of plastic its made of. I'm not sure what you mean by 'without a line' -
      If by that you mean 'without any visible seam' then it's probably not feasible If the cover material is clear.

  • @bdizzle1118
    @bdizzle1118 ปีที่แล้ว +1

    Great video! Is there a difference between welding two pieces of cast acrylic together and welding two pieces of extruded acrylic together?

    • @castorex
      @castorex 5 หลายเดือนก่อน

      Actually, it is - cast acrylic does not have any internal stress/tension and does not crack when in contact with solvent. Extruded acrylic have much more internal tension, which makes it crack (small but clearly visible cracks on the surface) when contacted with solvent.

  • @ThePoolSharkWizard
    @ThePoolSharkWizard ปีที่แล้ว

    What Welding Product are you using?

  • @Jack-ht5xk
    @Jack-ht5xk ปีที่แล้ว

    My acrylic is making tiny cracking fragments when bonding the acrylic together any ideas why

  • @postullio8775
    @postullio8775 6 หลายเดือนก่อน +2

    Where do you buy your methylene chloride?

  • @wareagleA5
    @wareagleA5 2 ปีที่แล้ว +1

    What about surface prep for solvent welding, do we have to router, or sand the edge ? I get great results on factory edges and terrible results on my saw cut edges, but I was told not to sand the edges because it would cause crazing. My blade is good enough to cut a rough edge with no breaking, but it doesn't leave as smooth an edge as your cutting demo. I'm trying to decide between getting a router table or a better circular saw blade.

    • @elfiurer
      @elfiurer ปีที่แล้ว +2

      The pieces must be perfectly cut, but that's very difficult to do, for if one's hand is not perfectly vertical when cutting the acrylic, the edge will not be square with the surface, I think.

    • @CountDoucheula
      @CountDoucheula ปีที่แล้ว +1

      Time to buy a CNC, my dude.

    • @elfiurer
      @elfiurer ปีที่แล้ว

      @@CountDoucheula Thanks.

  • @prakhyathshetty590
    @prakhyathshetty590 ปีที่แล้ว

    Plz recommend one best solvent sir, we from India

  • @thebrownlizard3988
    @thebrownlizard3988 ปีที่แล้ว

    amazing video i was trying it today and i was so confused why its evaporates !! i was woriied from the mess and it stickign to the floor? so it only bond acrylic plastic together? and wont bond any other surface to it ? like is some leaked it will evaporate or fgell on floor it wont glue it to the floor? also is that solvent toxic if inhaled ?

    • @DJ_Switzer
      @DJ_Switzer 6 หลายเดือนก่อน

      He keeps saying glue, but it's not an adhesive. It's a solvent. It dissolves the plastic and creates cohesion, and the plastic hardens again after the solvent evaporates. DCM is very volatile, like alcohol, it evaporates quickly, relative to water.

  • @burakuslu3661
    @burakuslu3661 3 หลายเดือนก่อน

    I am trying to make aquarium by plexiglass. Can i use that solvent? Is it waterproof?

  • @sum1sw
    @sum1sw ปีที่แล้ว

    How would you unweld something like this?

  • @elfiurer
    @elfiurer ปีที่แล้ว

    The pieces must be perfectly cut, but that's very difficult to do, for if one's hand is not perfectly vertical when cutting the acrylic, the edge will not be square with the surface, I think.

  • @scriptkidv1340
    @scriptkidv1340 ปีที่แล้ว

    very hepful

  • @icebmwpower
    @icebmwpower 2 ปีที่แล้ว

    Great video! 🥇🏆
    New subscriber here ... and I need you help pls.
    I would like to ask you, which is the best approach to weld the PMMA on edges (means stronger and will give me clear joints):
    *1) Methylene Chloride*
    *(also known as Dichloromethane)*
    or
    *2) Trichloromethane CHCl3*
    *(also known as Chloroform)*
    Why I’m asking you. My project is to build a custom taillights on my car), so I need new smoked clear lenses and since they are extremely curved in any direction (X, Y, Z) the thermoforming method doesn’t work for me. Next step in my plan is to cut the taillight lenses on segments (like 25x10, 25x14, 25x11mm and so on), to pre-heat and curve them and finally to try to weld them using one of the products above and hopefully it will be solid enough (and leakage free). So please let me know how to achieve the strongest pmma welding possible (and relatively invisible if possible). Thank you in advance.

    • @modelmakers33
      @modelmakers33  2 ปีที่แล้ว +2

      We don't use chloroform. Methylene chloride will give you a strong clear joint on PMMA (aka acrylic)

    • @icebmwpower
      @icebmwpower 2 ปีที่แล้ว

      @@modelmakers33 thank you for that input.

  • @user-ot3ht9er8h
    @user-ot3ht9er8h 3 หลายเดือนก่อน

    Does this solvent create a water tight seal?

  • @juliusganot1321
    @juliusganot1321 ปีที่แล้ว

    hello sir, if you don't mind can you give me the name of that adhesive...thank you very much

  • @lastcent5140
    @lastcent5140 5 หลายเดือนก่อน

    worth metioning dichloromethane is carcinogenic. Can also be found in paint stripper in australia. Thanks

  • @user001sg9
    @user001sg9 2 ปีที่แล้ว +2

    Nice video, but where to get the solvent from?
    So far as I have learned Methylene chloride is not available on the market for private users or hobby constructors. Is this understanding correct? If possible, could you kindly give the link where one could buy this from, please? Thanks

    • @modelmakers33
      @modelmakers33  2 ปีที่แล้ว +1

      I'm not sure where you're located, but plastic distributors are much more likely to have it than hobby/craft stores

    • @modelmakers33
      @modelmakers33  2 ปีที่แล้ว +3

      PS - An internet search for methylene chloride may point you to certain paint strippers - don't use that.
      Brand names for methylene chloride include: Rez N Bond, Weld-On, and EZFix(303) - use that, and always remember to be careful with this stuff. Its volatile and flammable. Don't breathe the vapors, don't get it on your skin, and don't use it near an open flame.

    • @user001sg9
      @user001sg9 2 ปีที่แล้ว

      @@modelmakers33 Many thanks for your reply and caution tips. Btw I am located in Germany and found Weld-On4 on the Internet.

    • @DJ_Switzer
      @DJ_Switzer 6 หลายเดือนก่อน

      @@user001sg9 Weld-On 3

  • @terrable_makes
    @terrable_makes หลายเดือนก่อน

    Thanks for the info! I am trying to use this technique but I am not seeing an instant bond, it is not "sticking" until it's sat there for a while. Any advice on why? they are laser cut pieces, so all I can think of is maybe i need to lightly sand the edges.

    • @iAnasazi
      @iAnasazi หลายเดือนก่อน

      Have you figured it out?

  • @jacobaguilar6756
    @jacobaguilar6756 ปีที่แล้ว

    What brand of solvent is that?

  • @-johnny-deep-
    @-johnny-deep- 3 ปีที่แล้ว

    Very cool. This strikes me as the absolute best way to bond acrylic to other acrylic. Better than any glue could ever be. Are there any drawbacks to this method? I guess pretty fast setting time might be one.

    • @modelmakers33
      @modelmakers33  3 ปีที่แล้ว +4

      I'm not sure if you would consider this a drawback, but the solvent won't fill gaps, and so the mating surfaces have to be in full contact. The resulting bond is extremely strong.
      Fast set time is usually considered a plus. Its not instant - you have a little time to adjust. But a better, cleaner joint will be achieved if the pieces are not moved at all once the solvent is applied. Best practice is to hold the parts together exactly where you want them when you apply the solvent. It will find its way into the tiniest crack via capillary action.

    • @-johnny-deep-
      @-johnny-deep- 3 ปีที่แล้ว +2

      @@modelmakers33 Thanks - makes sense. Yeah, the flatness of the joining surfaces is a must with this method. Another drawback I can see after some googling is that apparently this stuff is extremely toxic and evaporates like crazy!

    • @carmonaconsulting
      @carmonaconsulting 2 ปีที่แล้ว +1

      The solvent - methylene chloride - is pretty toxic, so you need to have adequate ventilation or a respirator with filters designed to counteract the solvent (not just any random mask, this is specific filter cartridges for specific chemicals). Same thing with Xylene and a bunch of other stuff - it's great to work with, but can royally screw up your body, especially the nervous system. Be careful and PLEASE read the warning labels!

  • @jaysoutdoors723
    @jaysoutdoors723 2 ปีที่แล้ว

    Hey I’m looking at making a livewell for my boat would that be strong enough to say hold the pressure of 15-20 gallons of water

    • @DJ_Switzer
      @DJ_Switzer 6 หลายเดือนก่อน

      Pressure of water depends upon it's height - 1/2lb per vertical foot.

  • @modelmakers33
    @modelmakers33  ปีที่แล้ว

    why not use double wall polycarbonate?

  • @rickgividen4318
    @rickgividen4318 2 ปีที่แล้ว +1

    If I add bits of acrylic to a little solvent, can I use it for filling in holes/cracks?

    • @modelmakers33
      @modelmakers33  2 ปีที่แล้ว +2

      Theoretically, yes, but in practice that's a technique that works much better with softer materials like ABS and polystyrene. If you do try it with acrylic, use acrylic sawdust, or very, very, VERY thin shavings. It will take forever to completely dissolve anything chunky. Keep the container sealed so the solvent doesn't all evaporate.
      Another technique you can try is puddling some solvent onto a flat piece of material and then scratching and scraping the surface with an exacto knife or screwdriver - any kind of small, stiff, thin metal paddle. You may get a bit of 'putty' like that. I wouldn't discourage you from giving that a try with acrylic, but again it's a technique better suited to softer plastic.

    • @rickgividen4318
      @rickgividen4318 2 ปีที่แล้ว

      @@modelmakers33 thank-you 😊

    • @modelmakers33
      @modelmakers33  2 ปีที่แล้ว +1

      @@rickgividen4318 No problem. BTW - Its not quite same thing as putty, but SciGrip 16 (aka Weld-on16) is a solvent with some 'body' that remains in the seam after the solvent has evaporated

    • @rickgividen4318
      @rickgividen4318 2 ปีที่แล้ว

      @@modelmakers33 Thanks

  • @asmafiver6422
    @asmafiver6422 2 ปีที่แล้ว

    Does this solvent liquid work w plexi glass? Would it be strong enough for a narrow a plexi glass A frame terrarium top for a old fish tank?

    • @modelmakers33
      @modelmakers33  2 ปีที่แล้ว +1

      Yes. Plexi glass is a brand name of acrylic

    • @asmafiver6422
      @asmafiver6422 2 ปีที่แล้ว

      thank you

  • @jerrycrafts5301
    @jerrycrafts5301 5 หลายเดือนก่อน

    Where can you buy methylene chloride you use in the video?

  • @blesskavala
    @blesskavala 2 ปีที่แล้ว

    I wanted to make acrylic podium , can I use this bond for 9mm acrylic

    • @modelmakers33
      @modelmakers33  2 ปีที่แล้ว +2

      Yes, methylene chloride (aka dichloromethane, or DCM) will bond acrylic together no matter how thick it is. The key to a good joint is contact between the mating surfaces, and penetration of solvent into the joint by capillary action. You can actually see the solvent going into the joint if your material is clear. The solvent won't fill gaps, and the parts won't bond together in any places where they don't touch.

    • @blesskavala
      @blesskavala 2 ปีที่แล้ว

      @@modelmakers33 thank you 👍

  • @dexterchewy
    @dexterchewy 2 ปีที่แล้ว

    Hmm how do i have it clear throughout. Does it cause blooming for this type of solvents?

    • @modelmakers33
      @modelmakers33  2 ปีที่แล้ว +2

      You may get a white spot or 'bloom' if you inadvertently get any solvent on the surface, but the joint will be clear wherever there is full contact between the mating parts.

    • @dexterchewy
      @dexterchewy 2 ปีที่แล้ว

      @@modelmakers33 ah i see so i really have to make the interface flat enough regardless. Does flame polishing the corners help prior to using the solvent. Say 3mm edge thickness acrylic (est contact area) for a box

    • @modelmakers33
      @modelmakers33  2 ปีที่แล้ว +2

      @@dexterchewy No don't polish first, that will round over the edge, and you don't want that. Don't soften any sharp corners prior to bonding in any way. Sharp corners facilitate the capillary action that draws the solvent into the joint. The edge must be flat and have good contact with the mating piece. The solvent will clarify the material wherever there is contact.

    • @dexterchewy
      @dexterchewy 2 ปีที่แล้ว

      @@modelmakers33 thanks a lot sir. Much appreciated for the advice. Got what you mean. Haha. Would be happy to visit your workshop in person but ive since left US after my studies. Really cool guy thanks for replying. Cheers.

  • @philkrueger5961
    @philkrueger5961 ปีที่แล้ว

    What is the brand name for Methylene Chloride, How expensive it it, and is it better than acetone, laquer thinner, or MEK (Methyl,Ethyl,Keton)?

  • @melissakasey1878
    @melissakasey1878 2 ปีที่แล้ว

    Is this waterproof afterword if you wanted to use for a vase?

    • @melissakasey1878
      @melissakasey1878 2 ปีที่แล้ว

      Afterward***

    • @modelmakers33
      @modelmakers33  2 ปีที่แล้ว +3

      If you get a good joint, yes, absolutely. The only way it would leak is if there was a hole or crack - but that does include any incomplete bonds in the seams. The key to a good solvent bonded joint (seam) is to have full contact between the mating surfaces. The solvent 'bonds' completely, but it will not 'fill' any voids. It just dissolves the surface of the mating pieces and then evaporates. There are products with some 'body' that remains in the seam after the solvent has evaporated (SciGrip 16, aka Weld-on16) and if you need waterproof, and you're not confident of full contact between the mating pieces, then this might be a better choice. Its messier to use, but it will both solvent bond and fill small voids.

    • @melissakasey1878
      @melissakasey1878 2 ปีที่แล้ว

      @@modelmakers33 I really can't thank you enough for the education on the matter and letting me know what products to use. Really appreciate your time & expertise!!!

    • @modelmakers33
      @modelmakers33  2 ปีที่แล้ว +1

      @@melissakasey1878 You're welcome! And thanks for the question. We're planning to do another video that addresses this subject in more detail

  • @DJ_Switzer
    @DJ_Switzer 6 หลายเดือนก่อน

    Would be nice if you mention your tools when you mention your materials.

  • @jkbarz841
    @jkbarz841 2 ปีที่แล้ว

    Can we use that for acquaruim?

    • @modelmakers33
      @modelmakers33  2 ปีที่แล้ว +1

      Yes. But you must have full contact between the mating surfaces for a waterproof seal. You can also use a solvent that has some 'body,' like Weldon16, that will remain to fill voids after the solvent evaporates. Check out our video 'Solvent bonding smooth vs. rough plastic surfaces' posted about a week ago.

  • @elsamendoza7664
    @elsamendoza7664 ปีที่แล้ว

    Can this fix a crack on plexiglass leaving no lines?

    • @modelmakers33
      @modelmakers33  ปีที่แล้ว +1

      No, you will still see a line

  • @MB4LDERRO
    @MB4LDERRO 2 ปีที่แล้ว

    Where can i buy the solvent?

  • @prasadnandvikar3149
    @prasadnandvikar3149 11 หลายเดือนก่อน

    Can we use for polycarbonate??

    • @DJ_Switzer
      @DJ_Switzer 6 หลายเดือนก่อน

      See Wikipedia page for Solvent Bonding. It lists plastics and compatible solvents.

  • @andrewluchsinger
    @andrewluchsinger 2 ปีที่แล้ว

    Where would a guy like me be able to purchase the solvent?

    • @modelmakers33
      @modelmakers33  2 ปีที่แล้ว +2

      I'm not sure where you're located, but a plastic distributor is probably more likely to have methylene chloride (aka dichloromethane, or DCM) than a hobby/craft store. Tell them what you want it for. Internet searches for methylene chloride may point you to paint strippers - don't try to use that.

    • @andrewluchsinger
      @andrewluchsinger 2 ปีที่แล้ว

      @@modelmakers33 I live in WI. I think I found a place. I am a member of a model railroad club and we use plexiglass for areas around the layout that we don't want hands to be in. Many of the areas are pretty long so we are looking for ways of gluing the plexiglass together without messy or bad looking joints. Just a few ounces is all we would need.

  • @bobylachanche
    @bobylachanche ปีที่แล้ว

    will works with polycarbonate ?

    • @modelmakers33
      @modelmakers33  ปีที่แล้ว +1

      Yes. Bonds polycarbonate. Also bonds ABS to polycarbonate

  • @flufycat2748
    @flufycat2748 ปีที่แล้ว

    Ok. The name of the solvent is ???

  • @moostakssayyed9624
    @moostakssayyed9624 3 ปีที่แล้ว

    What's name of this solvent

    • @illla
      @illla 3 ปีที่แล้ว +1

      1,2-Dichloroethane

    • @icebmwpower
      @icebmwpower 2 ปีที่แล้ว +1

      @@illla 1,2-Dichloroethane is C2H4Cl2 and the Model Makers talking about DichloroMethane (DMC) which is CH2Cl2. Greetings.

  • @annoorkhan4219
    @annoorkhan4219 2 ปีที่แล้ว

    Do you have any company or where is your location ?

    • @modelmakers33
      @modelmakers33  2 ปีที่แล้ว +1

      Yes. Modelmakers Inc, in Rockaway New Jersey, USA. We have website too: Modelmakersinc.com

  • @deny9540
    @deny9540 3 หลายเดือนก่อน

    Sir acrelic kar pientar

  • @christopherlynn8377
    @christopherlynn8377 2 ปีที่แล้ว

    Is there anyone whom I can pay, to make an acrylic shelf for me, approximately 14 inches wide, and maybe like 18 in tall, and 3 in deep, with four shelves

    • @modelmakers33
      @modelmakers33  2 ปีที่แล้ว +1

      You might be able to get something similar to those dimensions that is mass produced 'off the shelf.' You'd probably pay somewhere north of $100 for a stock item that size, which is less than you would pay for a custom piece. I'm not sure what your budget is, but to answer your question - Yes. There are plenty of businesses (including Modelmakers Inc) that can make something like that to your exact specifications.

  • @robjupp
    @robjupp 2 ปีที่แล้ว +1

    Not melting, dissolving.

    • @modelmakers33
      @modelmakers33  2 ปีที่แล้ว +1

      Yes. In common parlance chemical solvents (not to mention discouragement - or kindness...vulnerability...) can cause something to melt, but technically the term 'melt' is usually reserved for situations where heat is the agent of change!

  • @acrylicrizwan514
    @acrylicrizwan514 2 ปีที่แล้ว

    Hi my name rizwan
    Im acrylic working Acrylic fabricator

  • @moostakssayyed9624
    @moostakssayyed9624 3 ปีที่แล้ว

    Where I can buy in India

    • @modelmakers33
      @modelmakers33  3 ปีที่แล้ว +3

      The solvent used in this video is methylene chloride. Brand names include 'Rez-N-Bond' and 'EZ Fix 303.'
      Keep in mind that it can be used to weld some 'bondable' plastics together - acrylic, PS, PC, PETG, and ABS - but not others. For example, methylene chloride will not weld PE together, or vinyl, or PP. It won't interact at all with many plastics.
      One other thing to remember is that while acrylic can be welded to acrylic using this method, and PS to PS, PETG to PETG, etc., it is not the case that different kinds of 'bondable' plastics can be welded together. For example, If you try to weld acrylic to PS, the solvent will melt both, and they will 'stick' a little bit, but they will not bond together chemically to form a truly solid piece. This is a good rule of thumb, but there are exceptions: ABS can be completely welded to PC using methylene chloride.

  • @SumitThakur-hv5ne
    @SumitThakur-hv5ne 2 ปีที่แล้ว

    Glue name ?

    • @modelmakers33
      @modelmakers33  2 ปีที่แล้ว +2

      Methylene chloride. Its not exactly 'glue' - its a solvent, and like many solvents, it is a volatile organic compound (VOC) and should be used with care. Stay tuned, we're planning a few more videos on this subject in the near future.

    • @nanda_pamungkas
      @nanda_pamungkas 2 ปีที่แล้ว

      Is it heat ressistant?

    • @modelmakers33
      @modelmakers33  2 ปีที่แล้ว +1

      @@nanda_pamungkas As much as the material itself - the solvent itself does not persist, it merely acts as a catalyst to bond separate pieces of the material.