    NICKEL PLATING
    Nickel Plating is a process of depositing nickel onto a metal part. Parts to be plated must be clean and free of dirt, corrosion, and defects before plating can begin. To clean and protect the part during the plating process, a combination of heat treating, cleaning, masking, pickling, and etching may be used. Once the piece has been prepared it is immersed into an electrolyte solution and is used as the cathode. The nickel anode is dissolved into the electrolyte to form nickel ions. The ions travel through the solution and deposit on the cathode.
    PROCESS OF NICKEL PLATING 2 EURO COIN
    I used 12-percent vinegar and salt for a process, I mixed content and added cathode and anode of Nickel. On Stabilised Rectifier set on 4.5 V and started of process. A process was going on 20 seconds.
    THANK'S FOR WATCHING AND SUPPORTING ME! ♥️
    Please subscribe if you want to see more cool upcoming restoration projects. 👍 🛠 🔔 🎬 🔨 ⚙️ 🔩
    / @amazingworkshop
    Follow me on:
    Instagram _ / amazing.workshop
    My Facebook _ / amazing-workshop-10793...
    TikTok _ www.tiktok.com...
    And DON’T FORGET TO SEE, Large German KEROSENE Lamp - Restoration - Gottfried Puhlmann:
    • Large German OIL LAMP ...
    Thanks for watching my video, HOW TO MAKE THE NICKEL PLATING SOLUTION. ♥️
    Music: From TH-cam free audio library.
    Best regards, Martin
  • ภาพยนตร์และแอนิเมชัน

ความคิดเห็น • 96

  • @amazingworkshop
    @amazingworkshop  3 ปีที่แล้ว +2

    In this video I make the Nickel Plating Solution. Please leave your comment below and don’t forget to Subscribe @amazingworkshop! 🎬 🔔 👍
    th-cam.com/channels/TcxeBzkk-kZrsaLlyNGLMA.htmlvideos?sub_confirmation=1
    Thanks.

    • @khansharif5313
      @khansharif5313 2 ปีที่แล้ว +1

      Can u tell how make liquid to solid

  • @haja-sb6ur
    @haja-sb6ur ปีที่แล้ว

    Hello. Thank you for your kindness.

  • @mashmo123
    @mashmo123 2 ปีที่แล้ว +2

    keep up with the good work scientist!

  • @peterjordan5947
    @peterjordan5947 ปีที่แล้ว +1

    In the setup the negative was the red cable. Ut then you attached the coin to the black (positive) which wouldn't work?

    • @georgesquenot1404
      @georgesquenot1404 8 หลายเดือนก่อน +1

      I noticed that too. I think that the red crocodile should have been tagged with a plus (+) and the black one with a minus (-).

    • @goguyted
      @goguyted 8 หลายเดือนก่อน

      Not a helpful mistake in the video for us newbeez​@@georgesquenot1404

  • @rameshrsn3558
    @rameshrsn3558 3 หลายเดือนก่อน

    Very nice

  • @donaldspeck9212
    @donaldspeck9212 ปีที่แล้ว +1

    Can you do the same process with Nichrome?
    Thank you Sir 😊

  • @AritraDey2008
    @AritraDey2008 หลายเดือนก่อน +1

    Vote for Indian ten rupees coin.👍🏻

  • @shreesaralservice1435
    @shreesaralservice1435 2 ปีที่แล้ว +1

    Best

  • @faze_koki
    @faze_koki 2 ปีที่แล้ว +1

    Can u kindly prepare gold plating solution?

  • @kennethboydsr3966
    @kennethboydsr3966 ปีที่แล้ว

    Thanks !!!

  • @afiyagardenplanner3012
    @afiyagardenplanner3012 3 หลายเดือนก่อน

    plz tell me ratios of using chemical and nickel plat, thank you

  • @faustocapuciatti
    @faustocapuciatti ปีที่แล้ว

    excelente. gracias!

  • @llimo4382
    @llimo4382 2 ปีที่แล้ว +2

    Love the sound effects!!! Can this also be used for brush plating? thanks.

    • @amazingworkshop
      @amazingworkshop  2 ปีที่แล้ว

      Yes :)

    • @jayantaroy3033
      @jayantaroy3033 ปีที่แล้ว +1

      @@amazingworkshop amazing video, can u plz tell what is the material used as cathode and anode ?

    • @amazingworkshop
      @amazingworkshop  ปีที่แล้ว +1

      @@jayantaroy3033 anode and cathode is pure Nickel :)

  • @allinalladityan318
    @allinalladityan318 2 ปีที่แล้ว +2

    I used nickle strips (for connecting batteries) and tried to make the solution with vinegar and salt, but the solution didn't get green, but brownish color?

    • @alsemi-back-up579
      @alsemi-back-up579 2 ปีที่แล้ว +3

      Strips were nickel plated copper
      Same thing happened to me

    • @kchappelle
      @kchappelle 2 ปีที่แล้ว +1

      @@alsemi-back-up579 me too

    • @comi496
      @comi496 10 หลายเดือนก่อน

      nickel plated steel

  • @nu7480
    @nu7480 2 ปีที่แล้ว

    Hi I have already make after watching your video but the problem after making solution next day it get purple colour ? Why is wrong ? Also after making it won’t come nice green colour !

  • @taruntamrkartamrkar2374
    @taruntamrkartamrkar2374 ปีที่แล้ว

    Sar jo vedyo me bataya hi apne ouska kitan pirac hi our ap esko parsal kar sakte hi purane bath room nal par karna hi

  • @missmjvlog9087
    @missmjvlog9087 ปีที่แล้ว

    Is it possible to put stainless steel or whatever? Is that possible?

  • @helioturbo100
    @helioturbo100 2 ปีที่แล้ว +1

    Hello, good work, i would like to know where i buy niquel chrome, thankyou.

  • @eduardomalaquias297
    @eduardomalaquias297 ปีที่แล้ว

    How long did u leave the nickel plates in the vinegar for?

  • @stealhty1
    @stealhty1 2 ปีที่แล้ว

    Isn't suposed to put the part n the Positive ? since electricity flow from Negative

  • @ramsglobal5063
    @ramsglobal5063 4 หลายเดือนก่อน

    can we plate iron with this solution

  • @bujjyboddu6218
    @bujjyboddu6218 2 ปีที่แล้ว

    Good video sir, thank you, how to make tin sulphate, share vidio.

  • @arifmuhammad9268
    @arifmuhammad9268 ปีที่แล้ว

    Amazing

  • @punjabi_tutor
    @punjabi_tutor 6 หลายเดือนก่อน

    What is used as cathode?

  • @hassanhammami5452
    @hassanhammami5452 3 หลายเดือนก่อน

    The anode and cathode can be used again?

  • @devildeva-yt1594
    @devildeva-yt1594 ปีที่แล้ว

    Can i plating like zinc barrel for nickel plating ?

  • @maciejpiatek169
    @maciejpiatek169 8 หลายเดือนก่อน

    What vinegar did you use?

  • @newageautotechnology
    @newageautotechnology 5 หลายเดือนก่อน

    How much does it take to make a gallon ?

  • @apistosig4173
    @apistosig4173 2 ปีที่แล้ว +2

    In Australia - defacing a coin is a crime. Nice presentation.

  • @mehedihassan8944
    @mehedihassan8944 2 ปีที่แล้ว +1

    i cant find pure nickel near me, should i use nichrome wire?

    • @amazingworkshop
      @amazingworkshop  2 ปีที่แล้ว +1

      I haven't tried nichrome wire yet, I don't think it would work.

    • @guyteigh3375
      @guyteigh3375 ปีที่แล้ว

      Be etremely careful with nichrome - and Stainless steel. The chrome will come out and (IIRC) can present as hexavalent chromium which can be quite spectacularly toxic.
      A good place for nickel is ebay - look for "solar cell tabbing wire" or "battery nickel". Try to get from a seller with 99% feedback or better as you NEED solid nickel and not nickel plated steel :)
      i am a keen amateur chemist but i am cautious with some of the metal salts - they can be very useful but they can be quite toxic. I do not know wnough about chrome (and safe handling) so it is one of the metal I will not usually use.
      Same deal with cadmium. Arguably a good metal to plate with - BUT cadmium plating solutions are dangerously toxic.
      Just because you can use "household / safe" vinegar to make a plating solution, does not mean the solution is safe once you start reacting it with metals to make metal salts.
      Try or aliexpress for nickel strip, nickel tabbing, nickel anodes or nickel foil. You should strike lucky. Also pure anodes tend to give MUCH better results than "mixed metals".

  • @soulimanezaoui4700
    @soulimanezaoui4700 2 ปีที่แล้ว

    nice

  • @omarfrij3090
    @omarfrij3090 ปีที่แล้ว

    Can you use a nickel tube?

  • @TalkingGIJoe
    @TalkingGIJoe ปีที่แล้ว

    will epsom salts work for this?

  • @er.2357
    @er.2357 6 หลายเดือนก่อน

    GENERALLY NICKEL SULFATE SOLUTION USED AS AN ELECTROLYTE IN THE NICKEL PLATING... BUT IN THIS CASE WHERE IS SULPHATE ?

  • @gtmemories67
    @gtmemories67 2 ปีที่แล้ว +2

    How you made that stickers

  • @conancimmerian8348
    @conancimmerian8348 ปีที่แล้ว

    if this real and not a trick.......then it's amazing

  • @alexmcgrath7645
    @alexmcgrath7645 ปีที่แล้ว

    How to? What’s the ingredients?

  • @oliangomes6776
    @oliangomes6776 2 ปีที่แล้ว +1

    very good content! Happy birthday!
    I have a doubt can you use sulfuric acid to make the solution?

    • @amazingworkshop
      @amazingworkshop  2 ปีที่แล้ว +1

      Thank you! :)
      I haven't tried it yet, maybe in the next video

  • @troygaffer9913
    @troygaffer9913 8 หลายเดือนก่อน

    boss,pwede mgturo sayo kung ano ang kagamitan o pagproseso sa pag nickle pwede pkilista nlng boss salamat😊

  • @bhojraypatre
    @bhojraypatre ปีที่แล้ว

    सर ये जो मसीन है मुझे चाहिये कहा मिलेगा

  • @Juice556
    @Juice556 2 ปีที่แล้ว +1

    How durable is the plating?

    • @amazingworkshop
      @amazingworkshop  2 ปีที่แล้ว +1

      The longer it is in nickel, the more resistant it is to mechanical wear.

  • @kapiteinsjemanovzegtneeteg6166
    @kapiteinsjemanovzegtneeteg6166 2 ปีที่แล้ว

    is this also for gold?

  • @rakeshchavan509
    @rakeshchavan509 2 ปีที่แล้ว

    Is possible to silver

  • @طالبعباس-ق3ع
    @طالبعباس-ق3ع 2 ปีที่แล้ว

    ماهي المواد نيكل ناري اشتريها وامزجهن كل مراء

  • @MunishMunish-wl1tv
    @MunishMunish-wl1tv ปีที่แล้ว +1

    This solvent is only vinegar and salt that's all

    • @guyteigh3375
      @guyteigh3375 ปีที่แล้ว +2

      It's not really a "solvent" - nickel will not dissolve in it. Electricity is used to drive a reaction but it is not really "dissolving it". if it was a solvent in the true sense, you would have nickel dissolved in acetic acid - where if you boiled off the acetic acid/vinegar, you would have elemental nickel again - not Nickel Acetate.
      The electrolyte created is dilute nickel acetate and sodium chloride.

  • @Hamid-az
    @Hamid-az 4 หลายเดือนก่อน

    You said black crocodile is plus but after that you put it in minus part of power source 😂

  • @jakubthedanger8158
    @jakubthedanger8158 8 หลายเดือนก่อน

    I´m pretty sure you devalued those coins.

  • @abazarviolin-fans2185
    @abazarviolin-fans2185 หลายเดือนก่อน

    what thise Ni?

  • @ArnelGarnodo
    @ArnelGarnodo 25 วันที่ผ่านมา

    Bos Anong mga kagamitan Yan

  • @mohsin786aa
    @mohsin786aa 2 ปีที่แล้ว

    Can we do Nikel plating on plastic...?

  • @CristianoLini
    @CristianoLini 2 ปีที่แล้ว

    Finally a happy video..... I like crocodiles 😂

  • @rohit-eh8gb
    @rohit-eh8gb ปีที่แล้ว

    Water is hot ??

  • @annonymus4025
    @annonymus4025 ปีที่แล้ว

    Great and simple content.
    I trying this since a year and never reach constant results.
    The first test like coins are ok, but after when trying to plate parts (bike parts what I really want) soon I always get black lines and patches like oxide and a while it looks like its not even nikkel.
    The worst part, if I get decent finish on iron or steel it starts to rust in spots about 2 weeks.
    Any ideas?

    • @amazingworkshop
      @amazingworkshop  ปีที่แล้ว

      Thank you :)
      Black lines and patches usually occur if the part is not completely degreased. Try dipping in the activator first, then nickel plating.

    • @annonymus4025
      @annonymus4025 ปีที่แล้ว +1

      @@amazingworkshop I tried reversed electrolisis, acetone dipping, acid etching. Somehow always get the same black oxide. Only thing in my mind is maybe the 99% pure nickkel anode that I have from China is not that pure and have some residue.

    • @astrodax2753
      @astrodax2753 ปีที่แล้ว +1

      @@annonymus4025 have you been able to figure it out? I'm researching the subject too. I suggest you do multiple platings on top of each other. I found out that when they plate steel they start by plaiting it copper to prevent rust, they then plate it nickel then nickel chrome. Perhaps a couple of nickle coats would help. Keep me updated.

    • @donventura3844
      @donventura3844 ปีที่แล้ว +1

      Electrolytic nickel plating is hard for non simple shapes. Usually a copper wash/coating is necessary pre plating. Electroless will be a better option for corrosion resistance and it will coat sharp edges and blind holes better. They sel solutions for non electroless nickel plating

  • @dineshkumar-qp3th
    @dineshkumar-qp3th 2 ปีที่แล้ว

    Kharkdenge kaise

  • @Aldenbalubar
    @Aldenbalubar 9 หลายเดือนก่อน

    Magkano po pang nickel

  • @menashewalsh5128
    @menashewalsh5128 2 ปีที่แล้ว

    Chrome plating?

  • @me.samsulhaque2810
    @me.samsulhaque2810 ปีที่แล้ว

    আমি নিকেল কারখানা করতে চাই army nikal kar khana kurte

  • @VSbest18
    @VSbest18 2 ปีที่แล้ว

    Sloth

  • @MetalGearIV
    @MetalGearIV 2 ปีที่แล้ว

    😆

  • @mariyavoloven2529
    @mariyavoloven2529 ปีที่แล้ว

    minus red and plus black? you have no any knowledge of electronic.

  • @alsemi-back-up579
    @alsemi-back-up579 2 ปีที่แล้ว +1

    TALK MUCH!!!!!!!!!!!

  • @lesschattermoresplatter5769
    @lesschattermoresplatter5769 2 ปีที่แล้ว

    Congratulations! I wasn’t 0:30 into the video before I had to downvote.

  • @nu7480
    @nu7480 2 ปีที่แล้ว

    After setup 4v how long I have to keep the current on