Memperbaiki Belt Conveyor yang Rusak

แชร์
ฝัง

ความคิดเห็น • 6

  • @hejatexgmbh4753
    @hejatexgmbh4753 ปีที่แล้ว +2

    With the hybrid vulcanizing material Multiface 1.5 you will have the same result, maybe better. In fact it provides the same chemical crosslink like in the case of hot vulcanizing repair but without any solvents and already at room temperature and with no pressure. You can ever use it on an heat resistant belt made of EPDM for the transport of clinker in a cement plant. It can be used even on wide surfaces as there is almost no maximum over-coating time and in very wet conditions (fog, drizzle), which pose real problems to traditional hot splicing or cold gluing with a patch. After applying a first thin layer, you have to rub it with a round brush before filling the hole with Multiface 1.5. Half hour later the repair is ready to start at 23°C (60 min. at +5°). Of course, you accelerate the process with a hot gun or a vulcanizing press or a clamp press if you want to have the best result.
    If you really want to know if it is true you have to purchase some quantity and test it!

  • @WTFmoments99
    @WTFmoments99 2 หลายเดือนก่อน

    Itu disiram dengan cairan apa bang?

  • @adi17canel58
    @adi17canel58 ปีที่แล้ว

    bg bagaimana kalau koyak terbelah di tengah apakah bisa diperbaiki

    • @papanyaanak-anak5064
      @papanyaanak-anak5064  ปีที่แล้ว

      Bisa namun sifatnya temporary saja menggunakan flexco fasterner namun suaranya akan berisik karena bersentuhan dengan roller.

    • @alvinkho5575
      @alvinkho5575 ปีที่แล้ว

      @@papanyaanak-anak5064 om iti mata gerinda nya pakai mata apa ya?

    • @papanyaanak-anak5064
      @papanyaanak-anak5064  ปีที่แล้ว

      @@alvinkho5575 pakai rubber grinding pak