Voron 2.4r2: First mods, PETG Tune, and Troubleshooting

แชร์
ฝัง
  • เผยแพร่เมื่อ 24 ธ.ค. 2024

ความคิดเห็น • 5

  • @AetCount
    @AetCount ปีที่แล้ว +1

    *Adds all of those to my checklist*
    Those are all great specially how you diagnosed the failure with input shaping.
    Thanks!

    • @Driver732
      @Driver732  ปีที่แล้ว +1

      You're welcome! I didn't find much information on those input shaping errors online. Hopefully this will be improved in the future!

  • @deeply999
    @deeply999 ปีที่แล้ว +1

    Great info, Although the dessicant does not pull water out of filament, it needs to be dried first then kept in the storage for dryness.
    thanks for the info

    • @Driver732
      @Driver732  ปีที่แล้ว

      Thank you for the information on the dessicant, I learned something too.

  • @heheitme83
    @heheitme83 2 หลายเดือนก่อน

    How did you get your petg to stick to the smooth side of the build plate? I can only get my petg to stick to the textured side.