- Aluminum alloy surface treatment:
BC-22 Cyanide-free zinc precipitation water
Cu-231 Cyanide-free alkali copper
Cu-910 Acid Copper Brightener
Ni-301 Electroplating Nickel Brightener
Guangdong Bigely Technology Co.,Ltd
Degreasing agent, zinc plating, nickel plating, tin plating, copper plating, etc.
Address:Xiyanglin Industrial Zone,Jieyang City, Guangdong Province, China
Website: www.bigelaizin...
Alibaba: bigely.en.alib...
Tel: +86 0663 8670377
Fax: +86 0663 8291627
Mobile: +86-18026024810
Email: sale01@bigelaizincplating.com
He exposed whole industry
Not really.
Hi !thanks for the info ! One question : for the Ni Ca Sil cylinders plating what its the right sequence to be done ?And what materials to be use properly ?
This process does not required zincate layer onto aluminum, is that right
Amazing
Why he ain't got no gloves on?
👍👍👍👍👍
Por favor me pueden dar un curso y como puedo compryesos químicos
what cost for all
what were the chemicals in this process, i am looking to set up a plating business
add my wts:+86 18026024810
Que top o processo é o mesmo usando em cilindro cr125 2t ?
Where can I get this done?
Please contact me
Guangdong Bigely Technology Co.,Ltd
Degreasing agent, zinc plating, nickel plating, tin plating, copper plating, etc.
Address:Xiyanglin Industrial Zone,Jieyang City, Guangdong Province, China
Website: www.bigelaizincplating.com
Alibaba: bigely.en.alibaba.com
Tel: +86 0663 8670377
Fax: +86 0663 8291627
Mobile: +86-18026024810
Email: sale01@bigelaizincplating.com
how can i get the products?
Confusing. The captions are not coincide with video.
Can you send me how to prepare the solution, please?
add my whatsapp:+86 18026024810
Now watch it rust in a day, nickel is nice and all but doesn’t last long
Beri tau kami dong cara crom nya
add my wts:+86 18026024810
I want buy this camical
add my wts:+86 18026024810
Was it electroless after zincate
No, after Zinc precipitation. it's electroplating