I just used some new Klingsooor belts I has in stock. Every one of them snapped in 45 seconds to 3 minutes, just running with no load. The tape came loose. Never again.
The zig-zag of that joint allows for more surface area in the joint and hat makes it stronger. Also, it is less likely to catch on the sharp edge of a glass piece (compared to the No. 4 joint that has a larger flat area for the glass to catch). You can run the No. 3 joint in both directions, so you get more life out of such a belt than of the ones with the tape on the back.
I just used some new Klingsooor belts I has in stock. Every one of them snapped in 45 seconds to 3 minutes, just running with no load. The tape came loose. Never again.
very nice repersentation showed a lot of class glad to be a part of successful business
Thank you!
I'm running my on business
Would love to know the shelf life of butt jointed belts.how long can they be stored
Muito bom parabéns prá mim é a melhor fabricante de Abrasivos
i live in the UK and want to purchase a roll of no 4 high strength tape, can you help me with my search please
What is the shell life of tape joints?
Thanks! Great info. 👍
Good stuff, why the fancy joint for the glass industry?? thanks.
The zig-zag of that joint allows for more surface area in the joint and hat makes it stronger. Also, it is less likely to catch on the sharp edge of a glass piece (compared to the No. 4 joint that has a larger flat area for the glass to catch). You can run the No. 3 joint in both directions, so you get more life out of such a belt than of the ones with the tape on the back.
Tape chaheye
Which tape used for number 1 & number 4 butt splice method joint ??
It's a special industrial tape.
Name?
You Have stock lot abrasives material
Yes we do
Where are you located?
"Butt joint" - ha ha hee hee ! ! !
👍👍👍