1) SINK MARK
2) WELD LINES/KNIT LINES
3) WARPAGE/DEFORMATION
4) BURN MARK /DIESEL EFFECT
5) SCORING
6) HALF SHOTS/SHORT MOLD
7) FLASH .
8) VOID/BUBBLES/AIR POCKET/ BLISTER .
9) FLOW LINES
10) SILVER MARK/SILVER STREAKS
11) DELAMINATION
12) JETTING
#plasticdefect
#sinkmark
#automotivepartdefects
#InjectionMoldingDefects
#HowtoControlPlasticDefect
#PlasticDefectsIt'sSolution
#Plasticdefectsandremedie
#troubleshootingmoldingdefects
#whataredefectsinplastic
#automotivepartdefects
#howtoavoidSinkmark
#sinkmarkcutout
#plasticCoring
DEMO_Automotive Interior Exterior Trim Plastic Product Design & Development - using CATIA by Kiran Balaji Datal
on-app.in/app/oc/301801/zmkul?Dwhatsapp%26Dtutor-course-referral-wa%26Dcourse-overview-app
Thank you for information , simple and best explanation
VERY GOOD VIDEO SIR..........😊
zmkul.on-app.in/app/oc/310681/zmkul? For details
Specific identification and solutions for defects
Thank you
Very helpful sir thank you 🙏
Good work Kiren sir
Thank you bro.for you help I appreciate it..
zmkul.on-app.in/app/oc/310681/zmkul?Dcopy-link%26Dtutor-course-referral%26Dcourse-overview-app
Good work sir.. ❤️
Very nice 👍👍
Thankyou sir
Sir how can we find min and Max wall thickness for desired plastic is there any method or data sheet ? Please answer
Thank you
👌👌
Thanks sir.... 👏🏻
zmkul.on-app.in/app/oc/310681/zmkul?Dcopy-link%26Dtutor-course-referral%26Dcourse-overview-app
Nice explain
Thank you
Production se releted
Superb video
Thank you
zmkul.on-app.in/app/oc/301801/zmkul?Dcopy-link%26Dtutor-course-referral%26Dcourse-overview-app
How to design honey comb ribs