- Cause of Problem:
Bearding may be due to dryer configuration, use of wider spray angles and powder formulation, but mostly due to deficient nozzle design. This increases the cleaning up frequency, which delays production. Stopping production for cleaning and short run times play a big part to dryers’ low productivity
Solution: Flat Cap Profile
Click&Dry™ flat cap design provides a lower outer face profile greatly reducing bearding. This means less dryers shut down for clean up, and therefore, higher productivity. If we reduce build-up, we slow bearding process and therefore, nozzles can run longer. Click&Dry™ system offers longer run times!
By moving the o-rings into the wear part helps achieve this result.