What is the norm for this test? Usually this test is carried out at 23°C, but OK, infield can deviate. Moreover, usually, you pull max possible force to figure out the peel strength. The resolution is not good, but the applied force seems to be pretty low. This product can handle way more 😉
What is the norm for this test? Usually this test is carried out at 23°C, but OK, infield can deviate.
Moreover, usually, you pull max possible force to figure out the peel strength. The resolution is not good, but the applied force seems to be pretty low. This product can handle way more 😉
put some video peel test on overlap joint coating
There are a peel to 3LPE videos in this channel.
Please can you provide a list of all the instrument used for the peel test
Temperature gauge. Peel cutter/ knife, peel gauge with E clamp, timer/ watch,measuring tape & marker.
Sir agar 5 kag me crass kar deta to aur 5 kg pr adhesion nikal ke chala aata to failure hai???
Sir please tell me what is the acceptance criteria of peel test for htlp 80 and dirox sleeves as per temperature?
As per the ISO : 5 N/ mm @23+/- 2 def.c & 1 N/mm @ 60 +/-2deg.c.
As per EN: 3.5 N/mm @ 23 deg. C & 1 N/ mm 60 deg. C.
Sir
Please explain in simple way I don't understand this acceptance criteria very well.@@kesavakumarthecompletefami9610
Can we do peel test on both direx and normal sleeves and what is the temp and peel value range ?
Yes, we can conduct peel test between 23Deg.C to 60 Deg.C.
@@kesavakumarthecompletefami9610 can we do peel test below 23 deg please explain sir
@@rc7147 yes we can. We have to consider minimum peel values ( 23 Deg.c values).
Why we always close the seal at 10 or 2 o clock and what is the overlapping criteria
Test angle is wrong
It should be in 90 degrees angle.
Please list of instrumentation name.
Pesola you can use any other similar instrument.