Mr /Kumar. If steel is visible at damages, abrading with sand paper is enough or we can use bristle blaster to reinstate the profile? What does the Manufacturer recommend?
COULD YOU PLEASE CLARIFY : CAN WE USE LIQUID EPOXY INSTEAD OF EPOXY PRIMER IN REPAIR KIT? IF WE USE EPOXY IN REPAIR KIT WHAT MAX THICKNESS WE CAN APPLY.? AND THERE ARE S 1401 AND S 1301 EPOXIES, FOR HDD WHICH ONE TO BE USED?
You can use both epoxies on exposed steel portion. Epoxy is the main anti corrosive layer. Repair patch is only for mechanical protection. Filler mastic is to fill the gap ( deep damage of HDPE ) of 3LPE.
VERY USEFUL INFORMATION, SEVAKUMAR. EXCELLENT EXPLAINATION. PERFECT DEMO.!
Bahut bahut shukriya sir aap ne hame jankai Dene ke liye
Thank you
Mr /Kumar. If steel is visible at damages, abrading with sand paper is enough or we can use bristle blaster to reinstate the profile? What does the Manufacturer recommend?
60 mesh sand paper is more than enough.
You can find Repair patch adhesion video in my channel
th-cam.com/video/xE9h8sZJrMs/w-d-xo.html
Can we follow this process in online or line pack condition?
COULD YOU PLEASE CLARIFY : CAN WE USE LIQUID EPOXY INSTEAD OF EPOXY PRIMER IN REPAIR KIT? IF WE USE EPOXY IN REPAIR KIT WHAT MAX THICKNESS WE CAN APPLY.? AND THERE ARE S 1401 AND S 1301 EPOXIES, FOR HDD WHICH ONE TO BE USED?
You can use both epoxies on exposed steel portion. Epoxy is the main anti corrosive layer. Repair patch is only for mechanical protection. Filler mastic is to fill the gap ( deep damage of HDPE ) of 3LPE.
Where can i purchase perp 80 material?
You can send a mail to info@sealforlife.com