  • Machining test of 5051 aluminum alloy using the DLC coated 1-Cut Carbide End Mill.
    This cutter is specially sharpened for aluminum and the coating is the most advanced currently available for this application.
    We all know that alloy 5051 is the most difficult to machine in the cnc process as it is very soft and tends to stick to the cutter a lot, if the cutter is the wrong type it can happen within a few seconds of machining.
    We machine the material using compressed air, alcohol and soluble oil.
    In testing, it was seen that the cutter did very well, no significant difference was noticed using fluids, thus making it the best cutter option for those who cannot use fluids on their machines.
    DLC 1-cut cutters are available for purchase in our online store, visit: www.codigog.co...
    Remembering that Code G does not sell machines, we only sell the Mills.

ความคิดเห็น • 18

  • @marcomachado39
    @marcomachado39 2 ปีที่แล้ว +2

    Top 10, show esse video.

    • @CodigoG
      @CodigoG  2 ปีที่แล้ว

      Obrigado!!

  • @Corteex_Lab-Criativo
    @Corteex_Lab-Criativo 2 ปีที่แล้ว +3

    perfeito acabamento! Principalmente para o meu caso que não posso usar fluidos para refrigeração das minhas usinagens. A minha dúvida é: esse modelo de fresa exemplificado no vídeo serve para corte em outros metais NÃO ferrosos tipo latão, cobre e bronze? Ou somente em ligas de alumínio? Desde já agradeço a atenção e PARABÉNS pelos ótimos vídeos!

    • @CodigoG
      @CodigoG  2 ปีที่แล้ว +2

      Que bom que o vídeo ajudou! O caso do alumínio é que algumas ligas grudam na fresa e outras não, as ligas 6XXX e 7XXX são muito melhores pra usinar que as ligas 5XXX. Já no caso do latão e bronze, são infinitamente mais fáceis de usinar do que o alumínio, neste caso você pode continuar utilizando a fresa sem cobertura mesmo, ela já atende muito bem. De toda forma, eu faria o teste com uma fresa com cobertura DLC para tirar a duvida da vida útil, a tendência é você usinar mais tempo com essa cobertura antes que a ferramenta perca o corte.

  • @wellton22
    @wellton22 2 ปีที่แล้ว +1

    Vou testar ela no ACM também

    • @CodigoG
      @CodigoG  2 ปีที่แล้ว +1

      Se o alumínio do ACM não gruda na fresa sem cobertura, talvez essa com cobertura não seja necessário, porem, de toda forma eu recomendo o teste para ver a questão da durabilidade, essa com cobertura pode durar mais tempo que a sem cobertura.

    • @wellton22
      @wellton22 2 ปีที่แล้ว +1

      @@CodigoG quero testar justamente isso: a durabilidade

    • @CodigoG
      @CodigoG  2 ปีที่แล้ว

      @@wellton22 Por favor, quando testar, nos retorne com o feedback! Abraço!

  • @playboyxbox
    @playboyxbox 2 ปีที่แล้ว

    Qual fresa vc recomenda para magnesio de 4mm? Preciso gravar cliches com alta precisao

  • @exactpoint6738
    @exactpoint6738 2 ปีที่แล้ว +1

    Perfeito, preciso dessas fresas. Na usinagem das paletas vi que o movimento é diferente do que utilizo, sendo que esse do vídeo é bem interessante, não sei se é do pós-processador ou é recurso de um programa específico, eu geralmente uso o Aspire para gerar o gcode, então para as paletas, no Aspire seria percurso de desbaste, que é muito chato. Qual o nome de tipo de percurso?

    • @CodigoG
      @CodigoG  2 ปีที่แล้ว +1

      Olá, que bom que gostou do vídeo e abriu margem pra gente ajudar! O percurso é chamado de trocoidal, o aspire e artcam não faz. Nesse projeto usamos o Fusion360 (muito recomendado) ele tem estratégias de usinagem muito superior ao aspire e artcam, não tem comparação. No fusion360 esse percurso é chamado de desbaste adaptativo, é bastante eficiente, vale muito a pena aprender a usar esse programa, você pode fazer a peça e a usinagem no mesmo programa, ele exporta pro mach3. Esse programa é praticamente o SolidWorks, só que mais barato. Abraço!

    • @exactpoint6738
      @exactpoint6738 2 ปีที่แล้ว +1

      @@CodigoG Maravilha, eu tenho o fusion360 versão estudante, mais ainda não consegui acertar um percurso, sempre dá posicionamento errado no material. Bom saber que esse recurso é dele, já vi essa palavra nele, mais não sabia que era assim, vou estudar mais o fusion360. Obrigado 👍

    • @CodigoG
      @CodigoG  2 ปีที่แล้ว +1

      @@exactpoint6738 O Fusion é muito confuso pra quem veio do artcam e aspire, mas quando você pegar a manha dele, não vai mais conseguir usar o artcam e aspire, vale muito a pena o estudo!

  • @worlordes
    @worlordes 2 ปีที่แล้ว

    bom dia quantos psi ou bar usam de pressao para soprar os detritos?

    • @CodigoG
      @CodigoG  2 ปีที่แล้ว

      Olá! Esse é o nebulizador V da tapmatic, funciona de 0,5 a 4,0 bar

  • @americanpier04
    @americanpier04 2 ปีที่แล้ว

    Essa fresa posso usar em um pantógrafo cortesa para fazer usinagem em perfis de alumínio?

    • @CodigoG
      @CodigoG  2 ปีที่แล้ว

      Desculpe a demora na resposta, a notificação da mensagem não apareceu. Não conheço esse pantógrafo, mas se for aqueles manuais, não recomendo fresas de metal duro, elas são sensíveis demais e qualquer deslize elas quebram

  • @_west94
    @_west94 2 ปีที่แล้ว +1

    You are enjoying drill