I have to say that is one of the coolest processes i have ever seen!! I cant imagine the trial and error that went into getting that 'bubble' to end up like that!!
Thank you!! Definitely a lot of trial and error went into this job, however we enjoyed it and accomplished the task for the customer!
Another quality custom job from Bo-Mer Plastics in Auburn, NY! Thanks for showing us these processes TJ!
Thank you and you are very welcome! More to come!
How much acriylic mm ?
Starting gauge is .220"
My greetingsgood jobWhat is the appropriate temperature for forming sheets of polycarbonate in this way
The forming temperature depends on the starting gauge of the material as well as the process used to form the part.
I have to say that is one of the coolest processes i have ever seen!! I cant imagine the trial and error that went into getting that 'bubble' to end up like that!!
Thank you!! Definitely a lot of trial and error went into this job, however we enjoyed it and accomplished the task for the customer!
Another quality custom job from Bo-Mer Plastics in Auburn, NY! Thanks for showing us these processes TJ!
Thank you and you are very welcome! More to come!
How much acriylic mm ?
Starting gauge is .220"
My greetings
good job
What is the appropriate temperature for forming sheets of polycarbonate in this way
The forming temperature depends on the starting gauge of the material as well as the process used to form the part.