tarrace Waterproofing IPS flooring
ฝัง
- เผยแพร่เมื่อ 16 ต.ค. 2024
- Construction Process of IPS flooring
clean floor by water wash and application of brush
after cleaning, level mark are done by spirit leveling at 2-3 meter interval on surrounding wall
after proper level setting, concrete dummy dote are constructed at a 2 to 3 square meter area.
now concrete in specified mixed should be pour in panel.
after pouring of concrete, surface to be leveled with A straight edge and surface with wooden float or trowel.
cement punning 2 to 3 mm thicker is spread over IPS flooring to archive glossy look of floor.
curing period of minimum 15 day is required after construction.
other fiber may be use to prevent cracks.
sometime vacuum dewatering machine also use to get very hard surface of concrete floor.
AdPushupReport this ad
1 Share
nikeetasharma Guru
Added an answer on December 3, 2020 at 1:48 pm
IPS flooring generally stands for Indian Patent Stone which is also considered as a cheap flooring. The constituent of this type of flooring is cement, admixture, down 10mm coloured/white chips mixed with required water of around 35-50 mm thick on rcc/pcc surface. It is done through panel system making by glass trip/aluminium strip. Flotter can be used to surface smooth.
IPS floor can be used for all types of floors.
1 Share
Dhanya Beginner
Added an answer on August 2, 2020 at 9:02 am
Indian Patent Flooring (IPS) is a normal type of concrete flooring.
Construction procedure:
Make reference level on the wall. It is transferred across all the floor area.
Flooring thickness to be marked and also dummy level dots should be provided in every 1 to 2m
After proper setting, concrete of desired mix should be poured in panels to minimize shrinkage cracks.
After pouring level the surface with trowel.
Allow it to harden for about 36 hours
For gloosy and smooth IPS flooring, neat cement pinning, 2 to 3 mm thick is spread over the concrete surface and allowed to soak.
For curing of IPS flooring surface pond or wet Hessian cloths are spread over the surface for 15 days.
0 Share
You must log in to add an answer.
Join for free or log in to continue reading...
AdPushupReport this ad
Continue with Facebook
Continue with Google
or use
Username or email*
Password*
Captcha*
Remember Me!Forgot Password?
Need An Account, Join Here
Sidebar
Popular Articles
Gopal Mishra
Types of Foundation for Buildings and their Uses [PDF]
Gopal Mishra
Compressive Strength of Concrete -Cube Test [PDF], Procedure, Results
Sadanandam Anupoju
16 Types of Heavy Equipment Used in Construction
Padmanabhan G
Methods of Rainwater Harvesting [PDF]: Components, Transport, and Storage
Gopal Mishra
Calculate Quantities of Materials for Concrete -Cement, Sand, Aggregates
Recent Articles
Neenu S K
How to Choose Tiles for Construction of Pools?
Madeh Izat Hamakareem
What is Relative Humidity of Concrete?
Neenu S K
How to Deal with Leaking Ceilings?
Madeh Izat Hamakareem
Effects of Unrepaired Early-age Cracking in Concrete Structures
Madeh Izat Hamakareem
What is Internal Curing of Concrete?
Recent Questions
jkshah
Which is the code used for the design of the RCC Bridge?
1 Answer
AKM59
What is the tolerance for compression test results of concrete, according to the standards?
1 Answer
Gopal Mishra
What must be the maximum dry density of Granular Sub Base & Wet Mix Macadam used ...
1 Answer
Gopal Mishra
What is the Safe Bearing Capacity values for Different Soils?
1 Answer
Gopal Mishra
What are the different types of handrails used in bridges?
1 Answer
Footer
Home
About Us
Contact Us
Privacy Policy
Terms & Conditions
Ask Questions
Write for us
Popular Questions
Facebook
Inst